Wilson® VH3300 Vickers and Knoop Hardness Tester
Wilson VH3300
Automated Hardness Testing System
Wilson VH3300 Benefits
- Ease of operation is facilitated by both the intelligently designed machine and the user-friendly DiaMet software
- 6 position star turret to achieve up to a load range from 10gf to 50kgf when configured
- Illuminated and calibrated optional overview optics
- Designed for testing to Vickers, Knoop, and Brinell standards
- Select from a wide range of objectives and their fields of view
- Collision Resistant System preventing indenter or objective damage
- Built-in overshoot protection
- All components and software designed, manufactured, and integrated by Buehler
Diamet® Hardness Testing Software


Automated
By prioritizing swift and simple operation for all users, DiaMet software can utilize high automation, ensuring flexibility for the future.

Fast
Achieving auto-focus and auto-measurement in 5 seconds or less, deliver the fastest test cycle for precise and efficient results.

Safe
Emphasize machine safety with collision-resistant indenters and objectives, ensuring safety meets flexibility.

Versatile
Optimized for Vickers, Knoop, Rockwell, Superficial Rockwell, Brinell, and K1c fracture as per ISO and ASTM standards.
Ordering
Wilson VH3300 | |||
---|---|---|---|
Configure your VH3000 Series Vickers-Knoop Hardness Tester and select from motorized stage sizes, vertical test capacity, optics, and load cell selections. | |||
Request a Quote | |||
Part # | Description | ||
Main Unit | |||
W3210 | 3 objectives + 3 load cells, 0.010 - 50kgf load range*, Includes DiaMet workstation and 24" monitor | ||
Software Options | |||
W3100A03 | DiaMet Full-Automatic software package | ||
W3100A15 | DiaMet Enterprise software package | ||
Motorized Stages | |||
W3000SS | Standard Size (180 x 180mm) | ||
W3000SL | Large Size (300 x 180mm) | ||
Vertical Test Capacity | |||
W3200D01 | Height - 105mm | ||
W3200D02 | Height - 155mm | ||
Load Cell | |||
W3210E01 | 10N loadcell | ||
W3200E02 | 100N loadcell | ||
W3200E04 | 500N loadcell | ||
Overview Camera | |||
W3200F01 | Turret integrated camera for VH3300 - Includes Scan & Stitch function in the DiaMet software | ||
Additional Accessories | |||
W3100G01 | Indenter Holder (Standard) | ||
W3100G02 | SnapGrip Holder | ||
W9100687 |
Vickers Indenter (Vickers Indenter, ISO & ASTM Certified) |
Objectives | ||
---|---|---|
Part Number | Negative Mag. | Max. Field of View |
W5XLWDO | 5x | 3600μm |
W10XLWD | 10x | 1800μm |
W20XLWD | 20x | 900μm |
W40XLWD | 40x | 450μm |
W50XLWD | 50x | 360μm |
W100XLWD | 100x | 180μm |
*depending on configuration |
Specifications
Wilson VH3300 | |
---|---|
Scales | HV, HK |
Turret | Automatic 6 position incl. overview |
Indenter positions | Up to 3 (select) |
Test Load (select) |
Small loadcell (10N) 10gf - 1kgf Medium loadcell (100N) 50gf - 10kgf Large loadcell (500N) 0,5kgf - 50kgf |
Test Load Accuracy | ±1.5% < 200g, ±1% > 200g |
Force Application | Load Cell |
Dwell Time | 1 - 999 seconds |
Standard Compliance | ASTM E384, E92; ISO 6507, 9385, 4545 |
Magnification Range | 30X - 2000X with digital zooming |
Overview Camera (optional) | 0.25 x 0.25in [6 x 6 mm] |
Light Source | LED |
Consumables and Accessories
Related Products
The workhorse of the VH3000 series. Featuring a 3-position virtual turret with one indenter and two measurement objectives.
Versatile and reliable solutions for accurate micro-hardness testing with optional DiaMet software.
Product Literature
Videos
Buehler Latest

Archaeometallurgy can teach us a lot about the actions, knowledge, skills and beliefs of our ancestors. Metals can help tell the story of thousands of years of human development. This webinar takes snapshots of items stretching over nearly 4000 years, and discusses the metallurgical principles behind their creation, as well as the practical matter of how to prepare and etch the samples.

The National Aerospace and Defense Contractors Accreditation Program (NADCAP) is a global cooperative accreditation program for aerospace, defense and related industries. The program develops industry-wide manufacturing processes that are applied by aerospace accredited manufacturers and suppliers. These processes can be found in different areas of material-recovery, such as coating, heat treatment and welding processes as well as inspection methods, such as hardness testing and microstructural analysis.

Buehler is a division of Illinois Tool Works (ITW) and is based in Lake Bluff, Illinois. Our company’s legacy comprises groundbreaking designs including the first commercially available mounting press, the first Rockwell hardness tester and we were the first to automate polishing. This same forward-looking spirit, combined with a strong understanding of lab priorities, continues to inform how we serve our customers world-wide.

Protect your investment with Buehler’s Service Plans. Keep your lab up and running with access to wear part kits and your machine being services by one of our highly trained Service Technicians.
Properly maintaining your equipment will ensure consistent performance , minimize downtime and reduce the likelihood of costly repairs.

Visit our literature section

View our tools and training

Contact Buehler Service

Visit our E-Shop