Wilson® Rockwell® 574 Hardness Tester
Rockwell 574 Hardness Tester
Industry Leading Gauge Repeatability and Reproducibility (GR&R)
The Wilson Rockwell 574 Hardness Tester Series stands out for its quality, durability, and leading Gauge Repeatability and Reproducibility (GR&R) in hardness testing instruments. Offering regular scale or twin (regular and superficial scale) models, these testers conform to ASTM E18 and ISO 6508 standards, catering to various needs.
Wilson Rockwell 574 Benefits
- Experience unparalleled GR&R performance with the Rockwell 574. Its high-precision depth measurement ensures utmost accuracy for consistently repeatable testing.
- Built to endure high-volume production environments, witness demonstrated robust design with stainless steel internal components. Elevate your testing capabilities with a diverse range of dynamic accessories and anvil options, setting the standard for strength.
- Powerful yet uncomplicated, this straightforward machine boasts an auto-braking system on preload for seamless operation. With a built-in USB port enabling rapid data transfer to Microsoft Excel or other applications, experience effortless usability and efficiency in one package.
Ordering
Wilson Rockwell 574 Ordering | ||
---|---|---|
Part Number | Description | Request a Quote |
WH574R | 574R – for all Regular test scales | Request a Quote |
WH574T | 574T – for all Regular and Superficial test scales | Request a Quote |
Specifications
Wilson Rockwell 574R Regular |
Wilson Rockwell 574T Twin |
|
---|---|---|
Pre-load | 10kgf (98.07N) | 3, 10kgf (29.42, 98.07N) |
Main-load | 60, 100, 150kgf (588.39, 980.67, 1471N) | 15, 30, 45, 60, 100, 150kgf (147.1, 294.19, 441,29, 588.39, 980.67, 1471N) |
Hardness Scales | HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRP, HRR, HRS, HRV | HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRP, HRR, HRS, HRV, 15N, 30N, 45N, 15T, 30T, 45T, 15W, 30W, 45W, 15X, 30X, 45X, 15Y, 30Y, 45Y |
Test load type | Calibrated Spring (Minor Load), Dead weight stack (Major load) | |
Test cycle type | Motorized with automatic pre-load brake | |
Vertical test capacity | 11.43in [289mm] accessories may decrease available capacity | |
Horizontal test capacity | 6.93in [175mm] at the top, 6.13in [155mm] at the bottom | |
Indenters (optional) | 120º Diamond cone, 1/16in, 1/8in, 1/4in, 1/2in Ball | |
Data-out | USB and RS232 | |
Standards Compliant | ASTM E18, ASTM D785, ASTM B294, ISO 6508, JIS Z 2245, GB/T 230 | |
Power | 100 - 240VAC, 60/50Hz |
Consumables and Accessories
Related Products
Maximize productivity with the versatile Wilson RH2150 series. Offering a broad testing range and user-friendly interface for efficient and flexible operations.
Product Literature
Videos
Buehler Latest

Archaeometallurgy can teach us a lot about the actions, knowledge, skills and beliefs of our ancestors. Metals can help tell the story of thousands of years of human development. This webinar takes snapshots of items stretching over nearly 4000 years, and discusses the metallurgical principles behind their creation, as well as the practical matter of how to prepare and etch the samples.

The National Aerospace and Defense Contractors Accreditation Program (NADCAP) is a global cooperative accreditation program for aerospace, defense and related industries. The program develops industry-wide manufacturing processes that are applied by aerospace accredited manufacturers and suppliers. These processes can be found in different areas of material-recovery, such as coating, heat treatment and welding processes as well as inspection methods, such as hardness testing and microstructural analysis.

Buehler is a division of Illinois Tool Works (ITW) and is based in Lake Bluff, Illinois. Our company’s legacy comprises groundbreaking designs including the first commercially available mounting press, the first Rockwell hardness tester and we were the first to automate polishing. This same forward-looking spirit, combined with a strong understanding of lab priorities, continues to inform how we serve our customers world-wide.

Protect your investment with Buehler’s Service Plans. Keep your lab up and running with access to wear part kits and your machine being services by one of our highly trained Service Technicians.
Properly maintaining your equipment will ensure consistent performance , minimize downtime and reduce the likelihood of costly repairs.

Visit our literature section

View our tools and training

Contact Buehler Service

Visit our E-Shop