Wilson® RH2150 Rockwell Hardness Tester

RH2150 Rockwell Hardness Tester
RH2150 Series prioritizes flexibility, ergonomic testing, and swift data output
Wilson Rockwell RH2150 Benefits
- Leveraging the concept of the Wilson RB2000, the RH2150 advances Rockwell testing with modern features tailored for quality control and research demands. Introducing a revamped user interface for streamlined testing, or seamlessly integrate with an optional DiaMet software package.
- With high demand for tighter manufacturing tolerances and advanced processes, the RH2150 excels in required reliability. This machine, characterized by a sheet metal casting and load cell protection, ensures resilient performance. Options like a secure clamping device and an innovative external foot switch facilitate fast and robust operations.
- The Wilson RH2150 seamlessly transitions from the production floor to the R&D lab. Innovative adapters and anvils optimize facility utilization across various applications. Its accessories accommodate diverse parts and components, enhancing its versatility. Balanced with its easy-to-use interface, the RH2150 features the flexibility required to meet industry’s escalating demands.
Diamet® Hardness Testing Software

Automated
By prioritizing swift and simple operation for all users, DiaMet software can utilize high automation, ensuring flexibility for the future.

Fast
Achieving auto-focus and auto-measurement in 5 seconds or less, deliver the fastest test cycle for precise and efficient results.

Safe
Emphasize machine safety with collision-resistant indenters and objectives, ensuring safety meets flexibility.

Versatile
Optimized for Vickers, Knoop, Rockwell, Superficial Rockwell, Brinell, and K1c fracture as per ISO and ASTM standards.
Ordering
| Wilson Rockwell Rh2150 Ordering | ||
|---|---|---|
| Part Number | Description | Request a Quote |
| W2101R | Size 1 - 10in [254mm] - with regular Rockwell scales, 10-187.5 kgf | Request a Quote |
| W2102R | Size 2 - 14in [356mm] - with regular Rockwell scales, 10-187.5 kgf | Request a Quote |
| W2101T | Size 1 - 10in [254mm] - with regular and superficial Rockwell scales, 1-187.5 kgf | Request a Quote |
| W2102T | Size 2 - 14in [356mm] - with regular and superficial Rockwell scales, 1-187.5 kgf | Request a Quote |
| Every tester includes a 63mm flat anvil, as well as a 1/16” ball indenter | ||
Specifications
| Test Load range | 1-187.5 kgf (9,81 - 1838,7 N) |
| Test load type | Closed loop |
| Indenter holder | Snap grip |
| Available indenters |
Rockwell: Rockwell diamond cone 120°, 1/16”, 1/8”, ¼”, ½” carbide ball indenters Brinell: 1mm, 2.5mm, 5mm and 10mm ball indenters |
| Rockwell test procedures ISO 6508-1, ASTM E18 | A, B, C, D, E, F, G, H, K, L, M, P, R, S, V, 15N, 30N, 45N, 15T, 30T, 45T, 15W, 30W, 45W, 15X, 30X, 45X, 15Y, 30Y, 45Y |
| Plastic testing Ball indentation ISO 2039-1 | HB5: 49N, 132N, 358N, 961N |
| Plastic testing Ball indentation ISO 2039-2 | HRR, HRL, HRM, HRE |
| Rockwell carbon testing Ball indentation DIN 51917 | HR5: 7, 20, 40, 60, 100, 150 HR10: 20, 40, 60, 100, 150 |
| Brinell depth testing (non-standardized) HBW-T | HBW-T2.5: 31.25, 62.5, 187.5 HBW-T5: 25, 62.5, 125 HBW-T10: 100 |
| Machine control | 7” User Interface for data tracking, statistics, indirect verification, data export via USB or ethernet, physical start and stop buttons |
| Z Axis | Automatic Z axis drive, physical up and down movement buttons |
| Clamping device (optional) | Unique clamping hat to hold samples in place before and during testing, clamping force 55 kgf (121lbs) |
| Workspace illumination | White LED for proper indent positioning |
| Maximum Specimen Height | 254 mm [10 in]; 356 mm [14 in] |
| Maximum Specimen Weight | 50 kg (centered on anvil) |
| Depth from Center line | 200mm |
| Anvil | 63mm flat anvil with 19mm pin, more anvils optional as well as T-slot table |
| Operating Temperature Range | 10° to 38°C [50° to 100°F] |
| Humidity | 10% - 80% non-condensing |
| Machine Dimensions (D × W × H) | 600mm [28in] × 350mm [21in] × 1260mm [39.2in] (size 1) or 1360mm [41.2in] (size 2) |
| Accessory (optional) | Flat anvils, V anvils, Jack rest, indenter extensions 2”, 4” and 6” (only with clamping device) |
| Machine Net Weight | 125 kg (275lbs) |
| Power Supply | 110 - 240V / 50 - 60Hz |
Consumables and Accessories
Related Products
Product Literature
Videos
Find Your Solutions
Full Lab
Metallography Solutions
Do you want to improve your process? Reach out for one-on-one help from our applications experts.
Quick Links

View all Products in the Buehler Product Catalog

Select a method by material

Search Buehler's Safety Data Sheets

Browse and search Buehler's product literature