Coolants for Sectioning and Cutting

Proper Cooling for your Sectioning Needs

Coolants for Sectioning

Cool 3

Effectively cool your sample to prevent heat damage with our water miscible and oil based coolants and lubricants.

Cooling for High Quality Cutting

Coolants for Sectioning and Cutting help dissipate heat and remove swarf from the cutting point. Choose Buehler’s premium coolants to maintain high quality cutting surface, good blade life, and achieve consistent cutting results.

Coolants for Your Cutters

Cool 3 Fluid

Coolant 3
Water miscible fluid concentrate for abrasive and precision cutting. Dilute coolant to 1:25 to 2:25, with water.

IsoCut® Fluid

IsoCut Fluid
Oil based coolant only for use with the IsoMetTM Low Speed saw or any saw with a maximum speed of 500 rpm.
Ordering
Frequently Asked Questions
Would you have any recommendations for maintenance of Cool 3?

When an abrasive cutter machine is at rest, check that the coolant tank of the recirculating system is filled with coolant to the level recommended, typically about 4” to 6” from the top of the tank. This will allow the pump to effectively deliver coolant to the cut-off wheel and without drawing air intermittently from the coolant tank.

Check the coolant level daily. Replace coolant that has evaporated from the coolant tank with fresh coolant pre-mixed with water at the recommended ratio.

Cool 3 is not considered hazardous for sanitary sewers per RCRA regulations, however local regulations must also be consulted in conjunction with the Cool 3 SDS.

Consumables and Accessories
Related Consumables
Product Literature
Full Lab Metallography Solutions

Find Your Solutions

Full Lab
Metallography Solutions
Looking for more information from us? Browse through our Solutions section to view technical articles, find recommended processing methods, look at industry solutions, and more.
Need Additional Help?

Do you want to improve your process? Reach out for one-on-one help from our applications experts.

Contact Buehler Lab Team

Contact Lab Team

Contact Buehler

Contact Customer Care

Quick Links
Quickly access important info or visit our E-Shop
Product Catalog
Product Catalog

View all Products in the Buehler Product Catalog

Methods by Material
Methods by Material

Select a method by material

Safety Data Sheets
SDS

Search Buehler's Safety Data Sheets

Buehler Product Literature
Product Literature

Browse and search Buehler's product literature

Buehler an ITW Company
Buehler Products