Polishing Cloths

HIGH PERFORMACE POLISHING CLOTHS FOR YOUR NEEDS
Premium Polishing Cloths
Buehler’s premium polishing cloths help you achieve high quality polish in most efficient time.
They are engineered to offer superior surface finish and flatness in your polishing process.
A Cloth for Every Application
With a variety of fabrics, weaves and naps, Buehler has a cloth to fit every application need you may have.
Delicate Preparation
MicroCut grinding papers provide gentle material removal and superior surface finish when processing delicate or sensitive materials.
Reliable Preparation Results
Our premium polishing cloths used with MetaDi® Supreme Diamond Suspension and Pastes offer a complete solution in your labs.
Coarse Polishing
Coarse polishing is the first polishing step after grinding and is typically done using diamond abrasive.
UltraPad®
Our most commonly used coarse polishing cloth, UltraPad is a polyester surface very much like sail cloth with an interrupted surface pattern that enhances material removal.
It is most commonly used for engineering materials including ferrous metal alloys, refractory alloys and ceramic.
UltraPol®
UltraPol is a silk cloth. Softer than UltraPad, UltraPol is great in preparation of mineral samples where it provides excellent flatness, retention of phases and high-quality surface finish.
Nylon
Intermediate Polishing
Intermediate polishing is the transition from harder cloths of coarse polishing to somewhat softer cloths that further improve surface finish.
TexMet® C
TexMet is a highly versatile choice for intermediate polishing of many materials. It is a woven, pressed and buffed cloth. It is particularly suited for polishing softer materials such as low-melting point alloys, polymers, precious metals and pure metals.
It is also the most commonly used cloth for manual polishing over a range of polishing steps including coarse, intermediate and fine.
Trident®
A synthetic woven cloth, Trident is an excellent cloth for intermediate polishing of engineering alloys (ferrous and refractory alloys).
VerduTex®
VerduTex is particularly suited to intermediate polishing of large or unmounted samples.
It is also preferred when working with highly abrasion-resistant materials such as ceramic and carbides.
WhiteFelt®
White Felt is a thick, soft cloth that can be used for a variety of ferrous and nonferrous metals.
PoliCloth®
PoliCloth is a medium hard cloth that suited the best for cast iron, copper and aluminum alloys.
Fine Polishing
Fine polishing is the last stage of polishing using the softest cloths and finest abrasives (0.05µm to 1µm) to achieve the highest quality surface finish.
MicroCloth®
Our best selling cloth. A synthetic rayon napped cloth with fibers bonded to a cotton backing, our MicroCloth is the most common, all-purpose fine polishing cloth in the market.
MicroCloth is most often used for polishing ferrous metals, copper alloys, polymers and minerals.
MasterTex®
MasterTex is best suited to non-homogenous materials where preferential polishing is of great concern. An example would be micro-electronics materials where different materials are present in the same sample, or coatings that differ in abrasion-resistance from the substrate.
MicroFloc®
MicroFloc is particularly suited for polishing very soft materials such as low-melting point alloys and precious metals.
ChemoMet®
A polyurethane cloth with a fine, porous surface, ChemoMet is best used for polishing aluminum, refractory metals, silicon and ceramic.
Polishing Cloth Selection Guide
Buehler’s premium performance cloths are for all material applications and are engineered for long life & superior surface finish.
| Polishing Cloth Selection Guide | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Type | Cloth | Backing | Quantity | 8in [203mm] | 10in [254mm] | 12in [305mm] | Description | Recommended Micron Size | Abrasive Type | Applications |
| Coarse | UltraPad® |
PSA Magnetic |
10 5 |
40-7118
42-3008 |
40-7120
42-3010 |
40-7122
42-3012 |
Hard woven, no nap | 6μm & Up | Diamond | Ferrous materials and thermal spray coatings |
| UltraPol® | PSA | 10 | 40-7448 | 40-7450 | 40-7452 | Hard woven, non-aggressive silk | 6μm & Up | Diamond | Minerals, coals, ceramics, inclusion retention in steels, and refractory metals | |
| TextMet® P | PSA | 5 | 40-7638 | 40-7640 | 40-7642 | Hard non-woven, perforated | 6μm & Up | Diamond | Electronics, ceramics, carbides, petrographic, hard metals, glass, and metal matrix composites | |
| Intermediate | Nylon |
PSA Magnetic |
10 5 |
40-7068
42-3108 |
40-7070
42-3110 |
40-7072
42-3112 |
Medium hard woven, oil resistant, no nap | 6μm & Up | Diamond | Ferrous materials, sintered carbides and cast irons |
| TexMet® C |
PSA Magnetic |
10 5 |
40-1108
42-3208 |
40-1110
42-3210 |
40-1112
42-3212 |
Non-woven, pressed | 15 - 0.02μm | Diamond, AI2O3, SiO2 | Ferrous and nonferrous metals, ceramics, electronics, PCB’s, thermal spray coatings, cast irons, cermets, minerals, composites, plastics | |
| TriDent® |
PSA Magnetic |
10 5 |
40-7518
42-3308 |
40-7520
42-3310 |
40-7522
42-3312 |
Soft woven synthetic, no nap | 15 - 0.02μm | Diamond, AI2O3 | Ferrous and nonferrous metals, microelectronics, polymer matrix composites, coatings | |
| VerduTex® |
PSA Magnetic |
10 5 |
40-8018
42-3408 |
40-8020
42-3410 |
40-8022
42-3412 |
Medium hard, synthetic silk | 9 - 1μm | Diamond | Ferrous and nonferrous metals, microelectronics, coatings | |
| VelTex® |
PSA Magnetic |
10 5 |
40-8218
42-3508 |
40-8220
42-3510 |
40-8222
42-3512 |
Short nap, synthetic velvet | 9 - 1μm | Diamond | Soft metals | |
| WhiteFelt® | PSA | 5 | 16-2002 | 16-2502 | 16-3002 | Soft, durable, matted wool | 6 - 0.02μm | Diamond, AI2O3, SiO2 | Ferrous and nonferrous metals | |
| PoliCloth® |
PSA Magnetic |
10 5 |
40-8418
42-3608 |
40-8420
42-3610 |
40-8422
42-3612 |
Medium hard, woven wool | 9 - 1μm | Diamond | Soft metals | |
| Fine | MicroCloth® |
PSA Magnetic |
10 5 |
40-7218
42-3708 |
40-7220
42-3710 |
40-7222
42-3712 |
Soft synthetic rayon, long nap | 5 - 0.02μm | Diamond, AI2O3, SiO2 | Ferrous and nonferrous metals, ceramics, composites, PCBs, cast irons, cements, plastics, electronics |
| MicroFloc® |
PSA Magnetic |
10 5 |
40-8318
42-3808 |
40-8320
42-3810 |
40-8322
42-3812 |
Soft, long nap | 3 - 0.02μm | Diamond, AI2O3, SiO2 | Ferrous and nonferrous materials | |
| MasterTex® |
PSA Magnetic |
10 5 |
40-7738
42-3908 |
40-7740
42-3910 |
40-7742
42-3912 |
Soft synthetic velvet, low nap | 1 - 0.05μm | AI2O3, SiO2 | Soft nonferrous and microelectronics | |
| ChemoMet® |
PSA Magnetic |
10 5 |
40-7918
42-4008 |
40-7920
42-4010 |
40-7922
42-4012 |
Soft synthetic, porous, chemically resistant | 1 - 0.02μm | AI2O3, SiO2 | Titanium, stainless steel, lead/tin, solders, electronics, soft nonferrous metals, plastics | |
Apex® Hercules
Apex Hercules is a unique offering from Buehler. Magnetic backed resin surface provides long life and excellent flatness. It’s ideal to use it with diamond suspensions and pastes such as our MetaDi® Supreme products.
Apex Hercules H
Fine grinding disc ideal for grinding hard ferrous and non-ferrous materials (>HRC 20/HV 236).
Apex Hercules S
Fine grinding disc ideal for griding soft ferrous and non-ferrous materials (>HRC 20/HV 236).
Polishing Cloth Selection Guide
Magnetic backed resin surface that provides excellent flatness and edge retention. Use with MetaDi® Diamond Suspension.
| Apex Hercules | |||
|---|---|---|---|
| Type | 8in [203mm] | 10in [254mm] | 12in [305mm] |
|
Apex Hercules H
Fine grinding disc for hard ferrous and non-ferrous material (> HRC 20/HV 236)
|
41-2740-308-001 | 41-2740-310-001 | 41-2740-312-001 |
|
Apex Hercules S
Fine Grinding Disc for soft ferrous and non-ferrous material (< HRC 20/HV 236)
|
41-2740-408-001 | 41-2740-410-001 | 41-2740-412-001 |
Frequently Asked Questions
How long will my cloths last?
Often, a cloth may get contaminated from improper care or gouged before showing significant signs of wear. End of life for a cloth is typically indicated by unusually high polish time or a drastically different texture than when new.
How can I extend the life of polishing cloths?
Proper storage and maintenance will enhance cloth life. Rinsing will also extend cloth life, but requires extra abrasive to recharge. Chamfering the edges of your mount will reduce the likelihood of damaging your cloth with a sharp edge.
Do I have to use a different cloth for each polishing step?
To avoid cross contamination, each polishing cloth should only be used with one abrasive size. Applying multiple abrasive sizes to a single cloth can create scratches on the specimen during polishing.
My PSA backed cloths are hard to remove. How can I get them off more easily?
Use magnetic back cloths, which eliminate cloth removal time, or MagnoPad, a Teflon coated carrier plate.
Product Literature
Accessories
Related Consumables
Find Your Solutions
Full Lab
Metallography Solutions
Do you want to improve your process? Reach out for one-on-one help from our applications experts.

View all Products in the Buehler Product Catalog

Select a method by material