Do you dress well?

Diamond wafering blades used on Precision Cutting machines, such as the Isomet High Speed, are an excellent way to make extremely low damage sections in your metallographic samples. But do you know how to look after your blades? After a number of uses a diamond blade may start to cut less efficiently. Cut quality decreases […]
Accurate Porosity Measurement in Thermal Spray Coatings

Coatings manufactured via thermal spray typically have porosity in them. One of the most common processes for characterizing a spray coating is metallographic preparation. However, it’s long been established that there can be problems in both finding a correct approach to preparation, and to reproducing this approach over time. A good method is only part […]
Sample mounting – when method selection really matters!

Mounting presses are an excellent way to mount many specimens, and can be the most efficient and economical choice for many samples. However, the heat and pressure can cause significant damage to many samples – especially soft, porous or friable materials and coatings. In these cases, castable mounting systems must be used. Castable epoxy systems […]
Sectioning of Electronic Components

Introduction Sectioning of electronic components for quality control or failure analysis can be challenging as care must be taken to ensure the true structure is revealed, free from preparation-induced artifacts. Historically, sectioning processes that were highly damaging to the sample were used, which could induce artifacts that could easily be misinterpreted as manufacturing defects or […]
Metallographic Preparation of Medical Implants – Stents, Orthopedics…

Medical implants are increasingly used today, stemming from newer alloy developments and manufacturing techniques, such as additive manufacturing, necessitating a closer outlook at their microstructure usually with good mechanical strength, wear and corrosion resistant properties. Metallographic preparation of these components allows thorough inspection of microstructures, coatings (mainly hydroxyapatite) and potential imperfections from new manufacturing techniques. […]
EcoMet 30 – Semi-Automatic and Manual Grinder Polishers

Introduced by Buehler at Heat Treat 2017 Grinding and Polishing of Samples Simplified Lake Bluff, IL, Buehler, a global industrial manufacturer of value added consumables and testing equipment is introducing the EcoMet 30 Semi-Automatic and Manual Grinder Polisher for use in heat treat, automotive, aerospace, and electronic laboratory environments where fast reliable results are required in production environments. […]