Sectioning of Electronic Components

Introduction Sectioning of electronic components for quality control or failure analysis can be challenging as care must be taken to ensure the true structure is revealed, free from preparation-induced artifacts. Historically, sectioning processes that were highly damaging to the sample were used, which could induce artifacts that could easily be misinterpreted as manufacturing defects or […]