Silicon Carbide Grinding Papers


EASY TO USE GRINDING PAPERS FOR YOUR NEEDS
CarbiMet®
Silicon Carbide Grinding Papers
Buehler’s CarbiMet® & MicroCut® Silicon Carbide grinding papers are the premier line of silicon carbide grinding papers offering efficient material removal and minimal surface damage. Our griding papers come in various grit sizes, micron sizes and diameters.
High Material Removal with Superior Surface Finish
CarbiMet grinding papers offer quick grinding times with minimal surface damage during the grinding process. Since there is less damage to remove, the amount of subsequent processing may possibly be reduced, saving valuable time in the preparation process.
Tightly controlled particle sizes ensures consistent scratch depths and patterns to prevent sample damage and rework.
Delicate Preparation
MicroCut grinding papers provide gentle material removal and superior surface finish when processing delicate or sensitive materials.
Quick Change-Overs
Apex® S backing allows for fast changeovers between grinding paper steps. Simply remove the previous paper and apply the next one without needing to remove any backings or liners.
Ordering
| PSA Backed | ||||
|---|---|---|---|---|
| CarbiMet | ||||
| Pressure sensitive adhesive (PSA) backing for easy application directly to platen. Qty 100 | ||||
| Grit Size | Approx. Micron Size | 8"[203mm] | 10"[254mm] | 12"[305mm] |
| 60 [P60] | 260 | 36-08-0060* | 36-10-0060* | 36-12-0060* |
| 80 [P80] | 188 | 36-08-0080 | 36-10-0080 | 36-12-0080 |
| 120 [P120] | 127 | 36-08-0120 | 36-10-0120 | 36-12-0120 |
| 180 [P180] | 78 | 36-08-0180 | 36-10-0180 | 36-12-0180 |
| 220 [P240] | 58 | 36-08-0220 | 36-10-0220 | 36-12-0220 |
| 240 [P280] | 52 | 36-08-0240 | 36-10-0240 | 36-12-0240 |
| 280 [P320] | 46 | 36-08-0280 | 36-10-0280 | 36-12-0280 |
| 320 [P400] | 35 | 36-08-0320 | 36-10-0320 | 36-12-0320 |
| 360 [P600] | 26 | 36-08-0360 | 36-10-0360 | 36-12-0360 |
| 400 [P800] | 22 | 36-08-0400 | 36-10-0400 | 36-12-0400 |
| 500 [P1000] | 18 | 36-08-0500 | 36-10-0500 | 36-12-0500 |
| 600 [P1200] | 15 | 36-08-0600 | 36-10-0600 | 36-12-0600 |
| 1000 [P2500] | 8.4 | 36-08-1000 | 36-10-1000 | 36-12-1000 |
| MicroCut | ||||
| Grit Size | Approx. Micron Size | 8"[203mm] | 10"[254mm] | 12"[305mm] |
| 800 [P1500] | 13 | 36-08-0800 | 36-10-0800 | 36-12-0800 |
| 1200 [P2500] | 8 | 36-08-1200 | 36-10-1200 | 36-12-1200 |
| P4000 | 5 | 36-08-4000 | 36-10-4000 | 36-12-4000 |
| * Contains 50 pcs | ||||
| Plain Backed | ||||
|---|---|---|---|---|
| CarbiMet | ||||
| Plain backing requires the use of an adhesive liner or holding band. Qty 100 | ||||
| Grit Size | Approx. Micron Size | 8"[200mm] | 10"[250mm] | 12"[300mm] |
| 60 [P60] | 260 | 30-08-0060* | 30-10-0060* | 30-12-0060* |
| 80 [P80] | 188 | 30-08-0080 | 30-10-0080 | 30-12-0080 |
| 120 [P120] | 127 | 30-08-0120 | 30-10-0120 | 30-12-0120 |
| 180 [P180] | 78 | 30-08-0180 | 30-10-0180 | 30-12-0180 |
| 220 [P240] | 58 | 30-08-0220 | 30-10-0220 | 30-12-0220 |
| 240 [P280] | 52 | 30-08-0240 | 30-10-0240 | 30-12-0240 |
| 280 [P320] | 46 | 30-08-0280 | 30-10-0280 | 30-12-0280 |
| 320 [P400] | 35 | 30-08-0320 | 30-10-0320 | 30-12-0320 |
| 360 [P600] | 26 | 30-08-0360 | 30-10-0360 | 30-12-0360 |
| 400 [P800] | 22 | 30-08-0400 | 30-10-0400 | 30-12-0400 |
| 500 [P1000] | 18 | 30-08-0500 | 30-10-0500 | 30-12-0500 |
| 600 [P1200] | 15 | 30-08-0600 | 30-10-0600 | 30-12-0600 |
| 1000 [P2500] | 8.4 | 30-08-1000 | 30-10-1000 | 30-12-1000 |
| MicroCut | ||||
| Grit Size | Approx. Micron Size | 8"[200mm] | 10"[250mm] | 12"[300mm] |
| 800 [P1500] | 13 | 30-08-0800 | 30-10-0800 | 30-12-0800 |
| 1200 [P2500] | 8 | 30-08-1200 | 30-10-1200 | 30-12-1200 |
| P4000 | 5 | 30-08-4000 | 30-10-4000 | 30-12-4000 |
| * Contains 50 pcs | ||||
| Apex® S Backed | ||||
|---|---|---|---|---|
| CarbiMet S | ||||
| High friction backing allows for easy & fast changeovers between grinding steps. Use with Apex S carrier film.Qty 100 | ||||
| Grit Size | Approx. Micron Size | 8"[203mm] | 10"[254mm] | 12"[305mm] |
| 60 [P60] | 260 | 16-08-0060* | 16-10-0060* | 16-12-0060* |
| 80 [P80] | 188 | 16-08-0080 | 16-10-0080 | 16-12-0080 |
| 120 [P120] | 127 | 16-08-0120 | 16-10-0120 | 16-12-0120 |
| 180 [P180] | 78 | 16-08-0180 | 16-10-0180 | 16-12-0180 |
| 220 [P240] | 58 | 16-08-0220 | 16-10-0220 | 16-12-0220 |
| 240 [P280] | 52 | 16-08-0240 | 16-10-0240 | 16-12-0240 |
| 280 [P320] | 46 | 16-08-0280 | 16-10-0280 | 16-12-0280 |
| 320 [P400] | 35 | 16-08-0320 | 16-10-0320 | 16-12-0320 |
| 360 [P600] | 26 | 16-08-0360 | 16-10-0360 | 16-12-0360 |
| 400 [P800] | 22 | 16-08-0400 | 16-10-0400 | 16-12-0400 |
| 500 [P1000] | 18 | 16-08-0500 | 16-10-0500 | 16-12-0500 |
| 600 [P1200] | 15 | 16-08-0600 | 16-10-0600 | 16-12-0600 |
| 1000 [P2500] | 8.4 | 16-08-1000 | 16-10-1000 | 16-12-1000 |
| MicroCut S | ||||
| Grit Size | Approx. Micron Size | 8"[203mm] | 10"[254mm] | 12"[305mm] |
| 800 [P1500] | 13 | 16-08-0800 | 16-10-0800 | 16-12-0800 |
| 1200 [P2500] | 8 | 16-08-1200 | 16-10-1200 | 16-12-1200 |
| P4000 | 5 | 16-08-4000 | 16-10-4000 | 16-12-4000 |
| * Contains 50 pcs | ||||
| PSA Backed for MiniMet® 1000 | ||||
|---|---|---|---|---|
| CarbiMet | ||||
| Grit Size | Micron Size | Part Number | ||
| 120 [P120] | 127 | 36-02-0120 | ||
| 180 [P180] | 78 | 36-02-0180 | ||
| 240 [P280] | 52 | 36-02-0240 | ||
| 320 [P400] | 35 | 36-02-0320 | ||
| 400 [P800] | 22 | 36-02-0400 | ||
| 600 [P1200] | 15 | 36-02-0600 | ||
| MicroCut | ||||
| Grit Size | Micron Size | Part Number | ||
| 800 [P1500] | 13 | 36-02-0800 | ||
| 1200 [P2500] | 8 | 36-02-1200 | ||
| SiC Paper PSA Backed, 2.875in [73mm] Qty 100 | ||||
Accessories
Related Consumables
Product Literature
Frequently Asked Questions
Why are there two numbers for the grit size?
Both the ANSI grit standard in the US and the FEPA grit standard in Europe relate to an average particle size, but use slightly different measurement methods. The ANSI size is succeeded by the term “grit” while he FEPA number is identified by a preceding “P”. A comparison chart is available at buehler.com.
How long should I use the paper for?
Why is my PSA backed paper difficult to remove from the platen?
How do I refresh my Apex S surface?
How do I avoid air entrapment when applying CarbiMet S or CarbiMet PSA paper?
How can I prevent embedding of SiC particles in very soft materials?
Videos
Find Your Solutions
Full Lab
Metallography Solutions
Do you want to improve your process? Reach out for one-on-one help from our applications experts.

View all Products in the Buehler Product Catalog

Select a method by material

Search Buehler's Safety Data Sheets

Browse and search Buehler's product literature
Europe | EN