Coolants for Sectioning and Cutting help dissipate heat and remove swarf from the cutting point. Choose Buehler’s premium coolants to maintain high quality cutting surface, good blade life, and achieve consistent cutting results.Coolants for Your Cutters
Cool 3 Fluid
Water miscible fluid concentrate for abrasive and precision cutting. Dilute coolant to 1:25 to 2:25, with water.
IsoCut® Fluid
Oil based coolant only for use with the IsoMetTM Low Speed saw or any saw with a maximum speed of 500 rpm.
Ordering
| IsoCut Fluid | |
|---|---|
| Oil based coolant only for use with the IsoMet Low Speed Saw or any saw with a maximum speed of 500rpm. | |
| Part Number | Description |
| 11-1193-032 | 1qt [0.95L] |
| 11-1193-128 | 1gal [3.8L] |
Frequently Asked Questions
Would you have any recommendations for maintenance of Cool 3?
When an abrasive cutter machine is at rest, check that the coolant tank of the recirculating system is filled with coolant to the level recommended, typically about 4” to 6” from the top of the tank. This will allow the pump to effectively deliver coolant to the cut-off wheel and without drawing air intermittently from the coolant tank.
Check the coolant level daily. Replace coolant that has evaporated from the coolant tank with fresh coolant pre-mixed with water at the recommended ratio.
Would you have any recommendations for disposal of Cool 3?
Cool 3 is not considered hazardous for sanitary sewers per RCRA regulations, however local regulations must also be consulted in conjunction with the Cool 3 SDS.
Accessories
Related Consumables
Product Literature
Find Your Solutions
Full Lab
Metallography Solutions
Do you want to improve your process? Reach out for one-on-one help from our applications experts.

View all Products in the Buehler Product Catalog

Select a method by material

Search Buehler's Safety Data Sheets

Browse and search Buehler's product literature
Europe | EN