Time Study Case Hardness Testing of Automotive Crank Pins and Journals

A study shows an operator time savings of 86% for making and measuring indents in three locations of crank pins and journals when using automation compared to manual testing. There was less part manipulation, fewer errors in data transcription and lower variability between operators performing tests.  Click here to view the full article.

Leave a Reply

Your email address will not be published. Required fields are marked *

This site uses Akismet to reduce spam. Learn how your comment data is processed.

Quick Links

Quickly access important info or visit our E-Shop

Buehler Literature
Product Catalog

View all Products in the Buehler Product Catalog

Methods by Material

Select a method by material

SDS

Search Buehler's Safety Data Sheets

Buehler Literature Search
Product Literature

Browse and search Buehler's product literature

Optimize Your Sectioning
Optimize Your Sectioning
Optimize Your Sectioning
Buehler an ITW Company
Buehler Products