Hardness Capabilities:
|
Regular & Twin
|
Hardness Scales:
|
A, B, C, D, E, F, G, H, K, L, M, P, R, S, V
|
Preliminary Load:
|
10kg [98.07N]
|
Test Loads:
|
60, 100, 150 kg [588.4, 980.7, 1471 N]
|
Dwell Time: Major Dwell Time:
|
1.0 - 50.0 seconds (more details in PDF)
|
Vertical Testing Capacity:
|
11.43in [289mm] accessories may decrease available capacity
|
Test Cycle:
|
Motorized (Manual preload, auto trip, auto brake)
|
Specimen Illumination:
|
Adjustable LED
|
Standards Compliance:
|
ASTM E18, ASTM D785, ASTM B294, ISO 6508, JIS Z2245, GB/T 230
|
Conversion:
|
ASTM E140, ISO 18265, DIN 50150, GB T1172 Convert up to 4 scales simultaneously
|
Statistics:
|
No. of Tests, Mean, St. Deviation, Min., Max., Range, CP, CPk, individual readings list
|
Languages:
|
English, German, Spanish, French, Italian, Chinese (Simplifed)
|
Data Memory:
|
999 per each hardness scale
|
Data Output:
|
USB and RS-232
|
Resolution:
|
0.1 or .01 HR (adjustable)
|
Throat Depth:
|
6.93in [176 mm] at the top, 6.13 in [155mm] at the bottom
|
Maximum Specimen Weight:
|
220 lbs [100kg]
|
Maximum Specimen Height:
|
165 lbs [75kg]
|
Applications:
|
Steels, Coppers, Cast Irons, Thin Materials, Shallow and Deep Case Hardened Materials
|