title: AbrasiMet M Manual Abrasive Cutter
url: https://www.buehler.com/uk/products/sectioning/abrasive-cutters/abrasimet-m-manual-abrasive-cutter/
date: 2021-08-24T16:51:05+00:00
modified: 2025-07-09T21:35:09+00:00
lang: en_GB
---

# AbrasiMet® M Manual Abrasive Cutter

[![AbrasiMet® M Manual Abrasive Cutter](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/08/AbrasiMet-M-Front-Open-1.png)AbrasiMet® M Manual Abrasive Cutter](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/08/AbrasiMet-M-Front-Open-1.png)

[![AbrasiMet® M Manual Abrasive Cutter](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/08/AbrasiMet-M-3qtrs-open.png)AbrasiMet® M](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/08/AbrasiMet-M-3qtrs-open.png)

[![AbrasiMet® M Manual Abrasive Cutter](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/08/AbrasiMet-M_Front.png)AbrasiMet® M](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/08/AbrasiMet-M_Front.png)

[![Advanced Recirculation System for AbrasiMet M](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/08/Recirc-Tank-3Qtrs.jpg)Advanced Recirculation System for AbrasiMet M](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/08/Recirc-Tank-3Qtrs.jpg)

[![Advanced Recirculation System for AbrasiMet M](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/08/Recirc-Tank-Front.jpg)Advanced Recirculation System for AbrasiMet M](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/08/Recirc-Tank-Front.jpg)

## AbrasiMet M

### Manual Abrasive Sectioning Machine

The AbrasiMet M manual abrasive cutter is a benchtop cutter and the ultimate 12″ manual abrasive sectiojning machine, designed to be easy to use, durable, and versatile for your cutting needs. This cut off saw is ideal for easy sectioning in high-paced environments. Combine with Buehler’s abrasive blades for a complete sectioning solution providing optimal sample quality and fast cutting time.

#### AbrasiMet M benefits

Fast and Easy Cutting

- Large motor for cutting through any sample
- Bright chamber lights and large window
- Quick locking nut for tool-less blade change
- Dual cut accessory for acheiving 2 cuts at once
- Various vise table positions for compatibility with any 12mm vise
- Adjustable cutting handle for best ergonomics

Achieve Great Sample Quality

- 6 coolant nozzles for fast cooling
- Motor speed variation based on blade size for optimal rotation speed
- High cutting handle feedback allows users to quickly adjust cut force

Easy to Maintain

- Enclosed Motor to keep coolant and debris out
- Filtering recirculation system to decrease cleaning time
- High flow manual cleaning nozzle

Ordering

| AbrasiMet M - Ordering |  |  |
| --- | --- | --- |
| Part Number | Voltage | Request a Quote |
| 10-10107-200 | 200 - 240VAC, 50-60Hz | [Request a Quote](https://www.buehler.com/uk/buehler-request-a-quote-uk.php?pn=10-10107-200) |
| 10-10107-400 | 380 - 460VAC, 50-60Hz | [Request a Quote](https://www.buehler.com/uk/buehler-request-a-quote-uk.php?pn=10-10107-400) |
| 10-10107-200 | CSA 200-240VAC, 50-60Hz | [Request a Quote](https://www.buehler.com/uk/buehler-request-a-quote-uk.php?pn=10-10107-200) |

Specifications

| AbrasiMet M |  |
| --- | --- |
| Motor Power at 220VAC | 5.5hp\[4kW\] |
| Main Power | 200-240VAC or 380-460VAC 3 Phase, 50/60Hz |
| Blade Movement Axis | Z-Axis |
| Max Sample Width | 25in\[635mm\] |
| Blade Sizes | 10in\[254mm\] \| 12in\[304mm\] |
| Blade Table Clearance | 6.8in\[172mm\] \| 5.8in\[147mm\] |
| Cut Capacity | 4.3in\[109mm\] |
| Blade Speed | 3000rpm \| 2600rpm |
| Lighting | 2 LED strips |
| Dual Blade Cutting Width | 0.06in-1in\[1.52mm-25.4mm\] @.6in increments |
| Machine Dimensions | Width: 31.1in\[791mm\] Depth: 27.3in\[694mm\] Height: 25.7in\[653mm\] hood closed Height: 36.2in\[919mm\] hood open |
| T-Slot Table Dimensions | 9.8in x 7.1in\[250mm x 180mm\](L) 9.8in x 4.5in\[250mm x 115mm\](R) |
| Safety Features | Interlock Hood Switch, Emergency Stop |
| Compliance | CE Directives |

##### Consumables and Accessories

[![Abrasive Vising for Sectioning](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/vising-main-image.png)](https://www.buehler.com/uk/products/sectioning/accessories-consumables/abrasive-vises-for-sectioning/)

[Abrasive Vising](https://www.buehler.com/uk/products/sectioning/accessories-consumables/abrasive-vises-for-sectioning/)

Vising for Abrasive Saws and Cutters

[![Premium Abrasive Blades for Sectioning](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/Premium-Abrasive-Blade_16in.png)](https://www.buehler.com/uk/products/sectioning/accessories-consumables/abrasive-blades-for-sectioning/)

[Abrasive Blades](https://www.buehler.com/uk/products/sectioning/accessories-consumables/abrasive-blades-for-sectioning/)

Abrasive Blades for Abrasive Saws

[![Cool 3 Coolants for Sectioning](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/Cool-3-Group-Photo.png)](https://www.buehler.com/uk/products/sectioning/accessories-consumables/coolants-for-sectioning/)

[Cool 3](https://www.buehler.com/uk/products/sectioning/accessories-consumables/coolants-for-sectioning/)

Coolants for Sectioning Machines

[![Advanced Recirculation System for AbrasiMet M](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/08/Recirc-Tank-Front.jpg)](https://www.metallography.biz/product-list.php?pid=9)

[Recirculation Tank](https://www.metallography.biz/product-list.php?pid=9)

Advanced Recirculation Tank for AbrasiMet M

###### Related Products

[![AbrasiMet L Pro Automatic Abrasive Cutter](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMet-L-Pro-3qtrs.png)](https://www.buehler.com/uk/products/sectioning/abrasive-cutters/abrasimet-l-pro-automatic-abrasive-sectioning-saw/)

[AbrasiMet® L Pro](https://www.buehler.com/uk/products/sectioning/abrasive-cutters/abrasimet-l-pro-automatic-abrasive-sectioning-saw/)

14in \[356mm\] Automatic Abrasive Saw

[![AbrasiMet XL Pro Automatic Abrasive Cutter](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMet-XL-Pro-Front.png)](https://www.buehler.com/uk/products/sectioning/abrasive-cutters/abrasimet-xl-pro-automatic-abrasive-cutter/)

[AbrasiMet® XL Pro](https://www.buehler.com/uk/products/sectioning/abrasive-cutters/abrasimet-xl-pro-automatic-abrasive-cutter/)

18in \[457mm\] Automatic Abrasive Saw

[![AbrasiMatic 300 Abrasive Cutter](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMatic-300_600x600.jpg)](https://www.buehler.com/uk/products/sectioning/abrasive-cutters/abrasimatic-300-automatic-manual-abrasive-cutter/)

[AbrasiMatic® 300](https://www.buehler.com/uk/products/sectioning/abrasive-cutters/abrasimatic-300-automatic-manual-abrasive-cutter/)

12in \[305mm\] Automatic Abrasive Saw

[![IsoMet High Speed Pro 112800](https://www.buehler.com/uk/wp-content/uploads/sites/4/2025/05/IsoMet-High-Speed-Pro_112800.jpg)](https://www.buehler.com/uk/products/sectioning/precision-cutters/isomet-high-speed-high-speed-pro/)

[IsoMet® High Speed Pro](https://www.buehler.com/uk/products/sectioning/precision-cutters/isomet-high-speed-high-speed-pro/)

8in \[203mm\] Automatic Precision Saw

Product Literature

[![AbrasiMet M Manual Abrasive Cutter Sell Sheet](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/08/English-AbrasiMet-M-Sell-Sheet_06-28-2021.jpg)](https://www.buehler.com/assets/Brochures/English/Sectioning/AbrasiMet-M_Sell_Sheet_EN.pdf)

[AbrasiMet M Sell Sheet](https://www.buehler.com/assets/Brochures/English/Sectioning/AbrasiMet-M_Sell_Sheet_EN.pdf)

[![AbrasiMet M Manual Abrasive Cutter Brochure](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/08/English-AbrasiMet-M_06-28-2021.jpg)](https://www.buehler.com/assets/Brochures/English/Sectioning/AbrasiMet-M_Brochure_07-21.pdf)

[AbrasiMet M Brochure](https://www.buehler.com/assets/Brochures/English/Sectioning/AbrasiMet-M_Brochure_07-21.pdf)

[![Buehler Product Catalog](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/Buehler-Product-Catalog_default_600x782.jpg)](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

[Buehler Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

Videos

![Full Lab Metallography Solutions](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Dr-Mike-Keeble.jpg)

Find Your Solutions

###### Full Lab Metallography Solutions

Looking for more information from us? Browse through our Solutions section to view technical articles, find recommended processing methods, look at industry solutions, and more.

[Solutions by Industry](https://www.buehler.com/uk/solutions/buehler-solutions/solutions-by-industry/)

[Solutions by Material](https://www.buehler.com/uk/solutions/buehler-solutions/methods-by-material/)

Need Additional Help?

Do you want to improve your process? Reach out for one-on-one help from our applications experts.

![Contact Buehler Lab Team](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Lab-Icon.png)

Contact Lab Team

[Contact Lab](https://www.buehler.com/uk/contact-lab-uk.php)

![Contact Buehler](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Contact-Buehler.png)

Contact Customer Care

[Contact Us](https://www.buehler.com/uk/contact-us-uk.php)

###### Quick Links

Quickly access important info or visit our [E-Shop](https://www.metallography.biz/)

![Product Catalog](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Literature-Icon.png)

Product Catalog

View all Products in the Buehler Product Catalog

[Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

![Methods by Material](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/methods-by-material.png)

Methods by Material

Select a method by material

[Buehler Methods](https://www.buehler.com/uk/solutions/buehler-solutions/solutions-by-material/)

![Safety Data Sheets](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/SDS-Search.png)

SDS

Search Buehler's Safety Data Sheets

[Safety Data Sheets](https://www.buehler.com/uk/solutions/buehler-literature/safety-data-sheets/)

![Buehler Product Literature](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Buehler-Literature-Icon.png)

Product Literature

Browse and search Buehler's product literature

[Product Literature](https://www.buehler.com/uk/solutions/buehler-literature/product-literature/)