title: AbrasiMet L Pro Automatic Abrasive Cutting Saw
url: https://www.buehler.com/uk/products/sectioning/abrasive-cutters/abrasimet-l-pro-automatic-abrasive-sectioning-saw/
date: 2023-08-29T20:43:39+00:00
modified: 2025-07-09T21:37:21+00:00
lang: en_GB
---

# AbrasiMet® L Pro Automatic Abrasive Cutting Saw

[![AbrasiMet L Pro Automatic Abrasive Cutter](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMet-L-Pro.png)AbrasiMet L Pro Automatic Abrasive Cutter](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMet-L-Pro.png)

[![AbrasiMet L Pro Automatic Abrasive Cutter](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMet-L-Pro-3qtrs.png)AbrasiMet L Pro Automatic Abrasive Cutter](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMet-L-Pro-3qtrs.png)

[![AbrasiMet L Pro Automatic Abrasive Cutter Large Chamber](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMet-L-Pro-Large-Chamber.jpg)Large Chamber](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMet-L-Pro-Large-Chamber.jpg)

[![AbrasiMet L Pro Automatic Abrasive Cutter High Visibility](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMet-L-Pro-High-Visibility.jpg)High Visibility](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMet-L-Pro-High-Visibility.jpg)

[![AbrasiMet L Pro Automatic Abrasive Cutter Dynamic Vising Table](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMet-L-Pro-Dynamic-Vising-Table.jpg)Dynamic Vising Table](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMet-L-Pro-Dynamic-Vising-Table.jpg)

## AbrasiMet L Pro

### Automatic Abrasive Sectioning Machine

The AbrasiMet L Pro automatic abrasive cutter is a high performance 14″ cut off saw, designed to be intuitive, advanced, and reliable. Available as either a benchtop or floor standing cutter, we have the right solution for your needs. Combine with Buehler’s abrassive wheels for a complete cutting solution providing optimal sample quality and reduced processing time.

#### AbrasiMet L Pro Benefits

Improve Sample Quality

- Variable SmartCut feature to deliver great quality while reducing cut time
- 6 coolant nozzles on the blade and cut sample
- Stored methods for consistent sample quality

Easy to Use, Easy to Setup

- Intutive touchscreen
- 4 cutting types for flexibility in cutting-Chop (Z cut), Y-feed (linear), Planar (sawing motion) and Manual
- Laser alignment, bright lights, and large viewing windows
- Program serial cut mode for multiple automatic cuts
- Quick locking nut to change blades without tools

Reliable and Easy to Maintain

- Automatic full chamber cleaning
- Filtering recirculation system to decrease cleaning time

Ordering

| AbrasiMet L Pro |  |  |
| --- | --- | --- |
| Part Number | Voltage | Request a Quote |
| 10-2830-200 | 200-240VAC Benchtop Machine | [Request a Quote](https://www.buehler.com/uk/buehler-request-a-quote-uk.php?pn=10-2830-200) |
| 10-2870-200 | 200-240VAC Floor Standing Machine | [Request a Quote](https://www.buehler.com/uk/buehler-request-a-quote-uk.php?pn=10-2870-200) |
| 10-2830-400 | 380-460VAC Benchtop Machine | [Request a Quote](https://www.buehler.com/uk/buehler-request-a-quote-uk.php?pn=10-2830-400) |
| 10-2870-400 | 380-460VAC Floor Standing Machine | [Request a Quote](https://www.buehler.com/uk/buehler-request-a-quote-uk.php?pn=10-2870-400) |

Specifications

| AbrasiMet L Pro |  |  |  |
| --- | --- | --- | --- |
| Operation |  |  |  |
| Cut Operation | Automatic and Manual Control with Variable SmartCut Mode |  |  |
| Units | English and Metric |  |  |
| Vertical (Z) movement (blade) | 8.75in \[220mm\] |  |  |
| Front-Back (Y) movement (table) | 9.8in \[250mm\] |  |  |
| Horizontal (X) movement (blade) | 11.8in \[300mm\] |  |  |
| Cut Type | Chop (vertical), Y-feed, Planar (Saw), Standard Manual, Smart Manual |  |  |
| Display | 10.5in \[267mm\] LCD Display with LED Back lighting |  |  |
| Controls | Touch Screen; Joystick Controller |  |  |
| Lighting | 2 LED Strip, Adjustable brightness |  |  |
| Programming | Retains last Settings, Serial Sectioning, Saved Custom Programs |  |  |
| Laser | Green Laser (520mm Class 2) |  |  |
| Dimensions |  |  |  |
| Maximum Sample Width | Up to 26in \[660mm\] |  |  |
| Cut Length Increment | 0.04in \[1mm\] |  |  |
| Recirculation/Filtration Tank Capacity | 35gal \[130L\] |  |  |
| T-Slot Table Dimensions | 18.9in x 11.8in \[480mm x 300mm\] |  |  |
| Bench-top Machine Dimensions & Weight | Width: 42.9in \[1090mm\] Depth: 37.8in \[960mm\]\* Height: 42.1in \[1070mm\] Weight: 948lbs \[430kg\] | Floor standing Machine Dimensions | Width: 42.9in \[1090mm\] Depth: 37.8in \[960mm\] Height: 77.2in \[1960mm\] Weight: 1422lbs \[645kg\] |
| Blade Size | 10in \[254mm\] | 12in \[305mm\] | 14in \[356mm\] |
| Cut Capacity | 3.4in \[87mm\] | 4.4in \[112mm\] | 5.4in \[135mm\] |
| Blade Speed | 3000rpm | 2600rpm | 2100rpm |
| \* For install, depth is 32.7in \[830mm\] before control panel is installed |  |  |  |
| Electrical |  |  |  |
| Motor Power | 5.5Hp \[4kW\] |  |  |
| Main Power Max Current | 200-240VAC, 3 Phase, 50/60Hz 26amp | 380-460VAC, 3 Phase, 50/60Hz 18amp |  |
| Safety Features | Interlock Door Switch, Emergency Stop, 2 Hand Operations for Blade Movement (Open Door), Variable SmartCut |  |  |
| Compliance | CE Directives |  |  |

##### Consumables and Accessories

[![Abrasive Vising for Sectioning](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/vising-main-image.png)](https://www.buehler.com/uk/products/sectioning/accessories-consumables/abrasive-vises-for-sectioning/)

[Abrasive Vising](https://www.buehler.com/uk/products/sectioning/accessories-consumables/abrasive-vises-for-sectioning/)

Vising for Abrasive Saws and Cutters

[![Premium Abrasive Blades for Sectioning](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/Premium-Abrasive-Blade_16in.png)](https://www.buehler.com/uk/products/sectioning/accessories-consumables/abrasive-blades-for-sectioning/)

[Abrasive Blades](https://www.buehler.com/uk/products/sectioning/accessories-consumables/abrasive-blades-for-sectioning/)

Abrasive Blades for Abrasive Saws

[![Cool 3 Coolants for Sectioning](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/Cool-3-Group-Photo.png)](https://www.buehler.com/uk/products/sectioning/accessories-consumables/coolants-for-sectioning/)

[Cool 3](https://www.buehler.com/uk/products/sectioning/accessories-consumables/coolants-for-sectioning/)

Coolants for Sectioning Machines

![AbrasiMet L Pro Mist Extractor](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMet-L-Pro-Mist-Extractor.png)

Mist Extractor

For AbrasiMet L Pro

###### Related Products

[![AbrasiMet XL Pro Automatic Abrasive Cutter](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMet-XL-Pro-Front.png)](https://www.buehler.com/uk/products/sectioning/abrasive-cutters/abrasimet-xl-pro-automatic-abrasive-cutter/)

[AbrasiMet® XL Pro](https://www.buehler.com/uk/products/sectioning/abrasive-cutters/abrasimet-xl-pro-automatic-abrasive-cutter/)

18in \[457mm\] Automatic Abrasive Saw

[![AbrasiMatic 300 Abrasive Cutter](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMatic-300_600x600.jpg)](https://www.buehler.com/uk/products/sectioning/abrasive-cutters/abrasimatic-300-automatic-manual-abrasive-cutter/)

[AbrasiMatic® 300](https://www.buehler.com/uk/products/sectioning/abrasive-cutters/abrasimatic-300-automatic-manual-abrasive-cutter/)

12in \[305mm\] Automatic Abrasive Saw

[![AbrasiMet M Manual Abrasive Cutter](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMet-M-3qtrs-open.png)](https://www.buehler.com/uk/products/sectioning/abrasive-cutters/abrasimet-m-manual-abrasive-cutter/)

[AbrasiMet® M](https://www.buehler.com/uk/products/sectioning/abrasive-cutters/abrasimet-m-manual-abrasive-cutter/)

12in \[305mm\] Manual Abrasive Saw

[![IsoMet High Speed Pro 112800](https://www.buehler.com/uk/wp-content/uploads/sites/4/2025/05/IsoMet-High-Speed-Pro_112800.jpg)](https://www.buehler.com/uk/products/sectioning/precision-cutters/isomet-high-speed-high-speed-pro/)

[IsoMet® High Speed Pro](https://www.buehler.com/uk/products/sectioning/precision-cutters/isomet-high-speed-high-speed-pro/)

8in \[203mm\] Automatic Precision Saw

Product Literature

[![AbrasiMet L Pro Sell Sheet](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMet-L-Pro-Sell-Sheet.jpg)](https://www.buehler.com/assets/Brochures/English/Sectioning/AbrasiMet-L_Sell_Sheet_08-24-2023.pdf)

[AbrasiMet L Pro Sell Sheet](https://www.buehler.com/assets/Brochures/English/Sectioning/AbrasiMet-L_Sell_Sheet_08-24-2023.pdf)

[![AbrasiMet L Pro Brochure](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/AbrasiMet-L-Pro-Brochure.jpg)](https://www.buehler.com/assets/Brochures/English/Sectioning/AbrasiMet-L_Brochure_08-24-2023.pdf)

[AbrasiMet L Pro Brochure](https://www.buehler.com/assets/Brochures/English/Sectioning/AbrasiMet-L_Brochure_08-24-2023.pdf)

[![Buehler Product Catalog](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/Buehler-Product-Catalog_default_600x782.jpg)](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

[Buehler Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

Videos

![Full Lab Metallography Solutions](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Dr-Mike-Keeble.jpg)

Find Your Solutions

###### Full Lab Metallography Solutions

Looking for more information from us? Browse through our Solutions section to view technical articles, find recommended processing methods, look at industry solutions, and more.

[Solutions by Industry](https://www.buehler.com/uk/solutions/buehler-solutions/solutions-by-industry/)

[Solutions by Material](https://www.buehler.com/uk/solutions/buehler-solutions/methods-by-material/)

Need Additional Help?

Do you want to improve your process? Reach out for one-on-one help from our applications experts.

![Contact Buehler Lab Team](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Lab-Icon.png)

Contact Lab Team

[Contact Lab](https://www.buehler.com/uk/contact-lab-uk.php)

![Contact Buehler](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Contact-Buehler.png)

Contact Customer Care

[Contact Us](https://www.buehler.com/uk/contact-us-uk.php)

###### Quick Links

Quickly access important info or visit our [E-Shop](https://www.metallography.biz/)

![Product Catalog](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Literature-Icon.png)

Product Catalog

View all Products in the Buehler Product Catalog

[Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

![Methods by Material](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/methods-by-material.png)

Methods by Material

Select a method by material

[Buehler Methods](https://www.buehler.com/uk/solutions/buehler-solutions/solutions-by-material/)

![Safety Data Sheets](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/SDS-Search.png)

SDS

Search Buehler's Safety Data Sheets

[Safety Data Sheets](https://www.buehler.com/uk/solutions/buehler-literature/safety-data-sheets/)

![Buehler Product Literature](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Buehler-Literature-Icon.png)

Product Literature

Browse and search Buehler's product literature

[Product Literature](https://www.buehler.com/uk/solutions/buehler-literature/product-literature/)