title: Wilson VH3300 Vickers and Knoop Hardness Tester
url: https://www.buehler.com/uk/products/hardness-testing/vickers-knoop-hardness-testers/wilson-vh3300-vickers-and-knoop-hardness-tester/
date: 2021-10-18T20:56:07+00:00
modified: 2025-07-10T13:07:28+00:00
lang: en_GB
---

# Wilson® VH3300 Vickers and Knoop Hardness Tester

[![Wilson® VH3300 Automatic Hardness Tester](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/10/VH3300_front-view_no-monitor.png)Wilson VH3300](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/10/VH3300_front-view_no-monitor.png)

[![Wilson® VH3300 Automatic Hardness Tester with Monitor](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/10/VH3300-with-monitor.png)Wilson VH3300](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/10/VH3300-with-monitor.png)

## Wilson VH3300

### Automated Hardness Testing System

The Wilson VH3300 offers an advanced, fully automated hardness tester for fulfilling both Vickers and Knoop hardness testing requirements. Designed for all users from novice to expert, it utilizes quick and straightforward operation without compromising the flexibility required for advanced applications. The VH3300 is not only a solution for your current needs, but also a reliable choice for future applications.

#### Wilson VH3300 Benefits

Ease of Use

- Ease of operation is facilitated by both the intelligently designed machine and the user-friendly DiaMet software

Flexible

- 6 position star turret to achieve up to a load range from 10gf to 50kgf when configured
- Illuminated and calibrated optional overview optics
- Designed for testing to Vickers, Knoop, and Brinell standards
- Select from a wide range of objectives and their fields of view

Increased Up-time

- Collision Resistant System preventing indenter or objective damage
- Built-in overshoot protection
- All components and software designed, manufactured, and integrated by Buehler

### Diamet® Hardness Testing Software

Enhance sample throughput while ensuring consistency with minimal complexity through our DiaMet 2.0 software system.

![DiaMet Computer Monitor](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/03/DiaMet-Computer-Monitor-1024x442.png)

![DiaMet - Automated](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/03/DiaMet-Automated.png)

Automated

By prioritizing swift and simple operation for all users, DiaMet software can utilize high automation, ensuring flexibility for the future.

![DiaMet - Fast](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/03/DiaMet-Fast.png)

Fast

Achieving auto-focus and auto-measurement in 5 seconds or less, deliver the fastest test cycle for precise and efficient results.

![DiaMet - Safe](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/03/DiaMet-Safe.png)

Safe

Emphasize machine safety with collision-resistant indenters and objectives, ensuring safety meets flexibility.

![DiaMet - Versatile](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/03/DiaMet-Versatile.png)

Versatile

Optimized for Vickers, Knoop, Rockwell, Superficial Rockwell, Brinell, and K1c fracture as per ISO and ASTM standards.

[Learn More About DiaMet](https://www.buehler.com/uk/products/hardness-testing/automation-software/diamet-hardness-testing-software/)

#### Ordering

| Wilson VH3300 |  |
| --- | --- |
| Configure your VH3000 Series Vickers-Knoop Hardness Tester and select from motorized stage sizes, vertical test capacity, optics, and load cell selections. |  |
| [Request a Quote](https://www.buehler.com/uk/buehler-request-a-quote-uk.php) |  |
| Part # | Description |
| Main Unit |  |
| W3210 | 3 objectives + 3 load cells, 0.010 - 50kgf load range\*, Includes DiaMet workstation and 24" monitor |
| Software Options |  |
| W3100A03 | DiaMet Full-Automatic software package |
| W3100A15 | DiaMet Enterprise software package |
| Motorized Stages |  |
| W3000SS | Standard Size (180 x 180mm) |
| W3000SL | Large Size (300 x 180mm) |
| Vertical Test Capacity |  |
| W3200D01 | Height - 105mm |
| W3200D02 | Height - 155mm |
| Load Cell |  |
| W3210E01 | 10N loadcell |
| W3200E02 | 100N loadcell |
| W3200E04 | 500N loadcell |
| Overview Camera |  |
| W3200F01 | Turret integrated camera for VH3300 - Includes Scan & Stitch function in the DiaMet software |
| Additional Accessories |  |
| W3100G01 | Indenter Holder (Standard) |
| W3100G02 | SnapGrip Holder |
| W9100687 | Vickers Indenter (Vickers Indenter, ISO & ASTM Certified) |

| Objectives |  |  |
| --- | --- | --- |
| Part Number | Negative Mag. | Max. Field of View |
| W5XLWDO | 5x | 3600μm |
| W10XLWD | 10x | 1800μm |
| W20XLWD | 20x | 900μm |
| W40XLWD | 40x | 450μm |
| W50XLWD | 50x | 360μm |
| W100XLWD | 100x | 180μm |
| \*depending on configuration |  |  |

#### Specifications

|  | Wilson VH3300 |
| --- | --- |
| Scales | HV, HK |
| Turret | Automatic 6 position incl. overview |
| Indenter positions | Up to 3 (select) |
| Test Load (select) | Small loadcell (10N) 10gf - 1kgf Medium loadcell (100N) 50gf - 10kgf Large loadcell (500N) 0,5kgf - 50kgf |
| Test Load Accuracy | ±1.5% 200g |
| Force Application | Load Cell |
| Dwell Time | 1 - 999 seconds |
| Standard Compliance | ASTM E384, E92; ISO 6507, 9385, 4545 |
| Magnification Range | 30X - 2000X with digital zooming |
| Overview Camera (optional) | 0.25 x 0.25in \[6 x 6 mm\] |
| Light Source | LED |

#### Consumables and Accessories

[![Rockwell Hardness Test Blocks](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/03/Hardness-Test-Blocks.png)](https://www.buehler.com/uk/products/hardness-testing/hardness-testing-blocks/)

[Test Blocks](https://www.buehler.com/uk/products/hardness-testing/hardness-testing-blocks/)

Available in a wide range that set the standard for industry

[![Hardness Testing Indenters](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/03/0012356_carbide-ball-116in-for-uh250-iso.png)](https://www.buehler.com/uk/products/hardness-testing/hardness-testing-indenters/)

[Indenters](https://www.buehler.com/uk/products/hardness-testing/hardness-testing-indenters/)

Browse our selection of ISO & ASTM Certified Indenters

[![Self Leveling Vise](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/03/0013215_6x-self-leveling-vise-for-round-samples-wo-insert.png)](https://www.buehler.com/uk/products/hardness-testing/hardness-testing-sample-holders-and-anvils/)

[Sample Holders](https://www.buehler.com/uk/products/hardness-testing/hardness-testing-sample-holders-and-anvils/)

Find sample support that’s right for your application

[![GP-HDT Sample Fixture](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/03/GP-HDT-Sample-Fixture.png)](https://www.buehler.com/uk/products/hardness-testing/gp-hdt-sample-fixture/)

[GP-HDT Sample Fixture](https://www.buehler.com/uk/products/hardness-testing/gp-hdt-sample-fixture/)

Move directly from grinding and polishing to hardness testing

[![Anti Vibration Table](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/03/anti-vibration-table.png)](https://www.metallography.biz/hardness-testing.php)

[Vickers-Knoop Vibration Isolation Systems](https://www.metallography.biz/hardness-testing.php)

Limit outside vibrations and ensure your specimen remains motionless during testing

#### Related Products

[![Wilson VH3000 All in One](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/03/VH3000-All-in-one.png)](https://www.buehler.com/uk/products/hardness-testing/vickers-knoop-hardness-testers/wilson-vh3100-and-vh3300-all-in-one-hardness-testers/)

[Wilson® VH3000 Series All-in-One Hardness Testers](https://www.buehler.com/uk/products/hardness-testing/vickers-knoop-hardness-testers/wilson-vh3100-and-vh3300-all-in-one-hardness-testers/)

Remove complexity with pre-configured machine setups and effortlessly conduct Vickers and Knoop hardness tests.

[![Wilson® VH3100 Vickers & Knoop Hardness Testers](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/10/VH3100.png)](https://www.buehler.com/uk/products/hardness-testing/vickers-knoop-hardness-testers/wilson-vh3100-vickers-and-knoop-hardness-testers/)

[Wilson® VH3100 Hardness Tester](https://www.buehler.com/uk/products/hardness-testing/vickers-knoop-hardness-testers/wilson-vh3100-vickers-and-knoop-hardness-testers/)

The workhorse of the VH3000 series. Featuring a 3-position virtual turret with one indenter and two measurement objectives.

[![Wilson® VH1102 & 1202 Micro Hardness Testers](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/10/VH1102-1202.png)](https://www.buehler.com/uk/products/hardness-testing/vickers-knoop-hardness-testers/wilson-vh1102-and-1202-micro-hardness-testers/)

[Wilson® VH1102 & VH1202 Hardness Testers](https://www.buehler.com/uk/products/hardness-testing/vickers-knoop-hardness-testers/wilson-vh1102-and-1202-micro-hardness-testers/)

Versatile and reliable solutions for accurate micro-hardness testing with optional DiaMet software.

#### Product Literature

[![Wilson VH3100 VH3300 Brochure English](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/10/Wilson-VH3100-VH3300-Brochure_English.jpg)](https://www.buehler.com/assets/Brochures/English/Hardness/Wilson_VH3300_low.pdf)

[VH3000 Series Brochure](https://www.buehler.com/assets/Brochures/English/Hardness/Wilson_VH3300_low.pdf)

[![DiaMet Software Brochure English](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/10/DiaMet-Brochure_English.jpg)](https://www.buehler.com/assets/Brochures/English/Hardness/DiaMet-Brochure-Update-09-12-2023.pdf)

[DiaMet brochure](https://www.buehler.com/assets/Brochures/English/Hardness/DiaMet-Brochure-Update-09-12-2023.pdf)

[![Buehler Product Catalog](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/Buehler-Product-Catalog_default_600x782.jpg)](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

[Buehler Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

##### Videos

![Full Lab Metallography Solutions](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Dr-Mike-Keeble.jpg)

Find Your Solutions

###### Full Lab Metallography Solutions

Looking for more information from us? Browse through our Solutions section to view technical articles, find recommended processing methods, look at industry solutions, and more.

[Solutions by Industry](https://www.buehler.com/uk/solutions/buehler-solutions/solutions-by-industry/)

[Solutions by Material](https://www.buehler.com/uk/solutions/buehler-solutions/methods-by-material/)

Need Additional Help?

Do you want to improve your process? Reach out for one-on-one help from our applications experts.

![Contact Buehler Lab Team](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Lab-Icon.png)

Contact Lab Team

[Contact Lab](https://www.buehler.com/uk/contact-lab-uk.php)

![Contact Buehler](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Contact-Buehler.png)

Contact Customer Care

[Contact Us](https://www.buehler.com/uk/contact-us-uk.php)

###### Quick Links

Quickly access important info or visit our [E-Shop](https://www.metallography.biz/)

![Product Catalog](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Literature-Icon.png)

Product Catalog

View all Products in the Buehler Product Catalog

[Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

![Methods by Material](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/methods-by-material.png)

Methods by Material

Select a method by material

[Buehler Methods](https://www.buehler.com/uk/solutions/buehler-solutions/solutions-by-material/)

![Safety Data Sheets](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/SDS-Search.png)

SDS

Search Buehler's Safety Data Sheets

[Safety Data Sheets](https://www.buehler.com/uk/solutions/buehler-literature/safety-data-sheets/)

![Buehler Product Literature](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Buehler-Literature-Icon.png)

Product Literature

Browse and search Buehler's product literature

[Product Literature](https://www.buehler.com/uk/solutions/buehler-literature/product-literature/)