title: Specialty Grinding and Polishing
url: https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/specialty-grinding-and-polishing/
date: 2021-10-11T16:15:46+00:00
modified: 2024-12-09T20:36:02+00:00
lang: en_GB
---

# Specialty Grinding and Polishing

# Specialty Grinding and Polishing

![FibrMet Discs Specialty Grinding and Polishing](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/10/69-3100_fibrmet-discs-4-in-psa-12-mic.jpg)

*FibrMet Discs*

![UltraPrep Lapping Films](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/0011495_ultra-prep8-1-mic-plain.png)

*UltraPrep Lapping Films*

## Specialty Solutions

### Specialty Grinding and Polishing

Some applications can benefit from a specialty product or solution. A variety of diamond lapping films, abrasive discs and powders are here to meet your application specific needs.

[Shop Now](https://www.metallography.biz/grinding-polishing.php)

### Coarse Polishing

Coarse polishing is the first polishing step after grinding and is typically done using diamond abrasive.

#### UltraPrep® Diamond Lapping Films

![UltraPrep Lapping Films](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/0011495_ultra-prep8-1-mic-plain.png)

UltraPrep diamond lapping films are designed for applications where surface flatness and minimal deformation is critical. These lapping films are available in a wide range of sizes from 0.1µm to 30µm. Applications include microelectronic devices, wafers, ceramics, optical fibers, petrographic, and more.

#### FibrMet® Abrasive Discs

![FibrMet Discs Specialty Grinding and Polishing](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/10/69-3100_fibrmet-discs-4-in-psa-12-mic.jpg)

FibrMet abrasive discs are coated with an aluminum oxide abrasive. These discs can be used wet or dry and are ideal for fine grindinging and polishing applications, such as optical fiber and microelectronics where surface flatness is essential. These abrasive discs are available in a wide range of sizes from 0.3µm to 12µm.

#### Abrasive® Powders

![Abrasive Powders](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/0013738_aluminum-oxide-powder-3m-5lb.png)

Abrasive powders are for fine grinding of cast iron and tin materials. Mixing is required with distilled water to achieve desired consistency.

##### Ordering

| UltraPrep Diamond Lapping Films (Qty 5) |  |  |
| --- | --- | --- |
| UltraPrep Diamond Lapping Films are designed for various material applications including microelectronic devices, wafers, ceramics, optical fibers, petrographic, and other metallographic materials. Ideal for preparation applica- tions where surface flatness and minimal deformation are critical. |  |  |
| Micron | 8in \[203mm\] PSA Backed | 8in \[203mm\] Plain Backed |
| 0.1µm | [15-6791](https://www.metallography.biz/product-information.php?pid=156791) | [15-6792](https://www.metallography.biz/product-information.php?pid=156792) |
| 0.5µm | [15-6795](https://www.metallography.biz/product-information.php?pid=156795) | [15-6796](https://www.metallography.biz/product-information.php?pid=156796) |
| 1µm | [15-6801](https://www.metallography.biz/product-information.php?pid=156801) | [15-6802](https://www.metallography.biz/product-information.php?pid=156802) |
| 3µm | [15-6803](https://www.metallography.biz/product-information.php?pid=156803) | [15-6804](https://www.metallography.biz/product-information.php?pid=156804) |
| 6µm | [15-6806](https://www.metallography.biz/product-information.php?pid=156806) | [15-6807](https://www.metallography.biz/product-information.php?pid=156807) |
| 9µm | [15-6809](https://www.metallography.biz/product-information.php?pid=156809) | [15-6810](https://www.metallography.biz/product-information.php?pid=156810) |
| 15µm | [15-6815](https://www.metallography.biz/product-information.php?pid=156815) | [15-6816](https://www.metallography.biz/product-information.php?pid=156816) |
| 30µm | [15-6830](https://www.metallography.biz/product-information.php?pid=156830) | [15-6831](https://www.metallography.biz/product-information.php?pid=156831) |

| FibrMet Abrasive Discs (Qty 50) |  |  |  |
| --- | --- | --- | --- |
| FibrMet Abrasive Disc are PSA (polyester backed) films, approx. 0.1 mm thick, coated with an aluminum oxide abrasive. These discs can be used wet or dry and are most suitable for fine grinding and polishing application, such as optical fiber and microelectronics where resultant surface flatness is essential. |  |  |  |
| Micron | 4in \[102mm\] | 8in \[203mm\] | 12in \[305mm\] |
| 0.3μm | [69-3104](https://www.metallography.biz/product-information.php?pid=693104) | [69-3174](https://www.metallography.biz/product-information.php?pid=693174) | [69-3124](https://www.metallography.biz/product-information.php?pid=693124) |
| 1μm | [69-3103](https://www.metallography.biz/product-information.php?pid=693103) | [69-3173](https://www.metallography.biz/product-information.php?pid=693173) | [69-3123](https://www.metallography.biz/product-information.php?pid=693123) |
| 3μm | [69-3102](https://www.metallography.biz/product-information.php?pid=693102) | [69-3172](https://www.metallography.biz/product-information.php?pid=693172) | [69-3122](https://www.metallography.biz/product-information.php?pid=693122) |
| 9μm | [69-3101](https://www.metallography.biz/product-information.php?pid=693101) | [69-3171](https://www.metallography.biz/product-information.php?pid=693171) | [69-3121](https://www.metallography.biz/product-information.php?pid=693121) |
| 12μm | [69-3100](https://www.metallography.biz/product-information.php?pid=693100) | [69-3170](https://www.metallography.biz/product-information.php?pid=693170) |  |

| Aluminum Oxide Powder |  |
| --- | --- |
| Aluminum Oxide Powder is used for fine grinding on cast iron, tin, or cloth-covered platens. They are mixed with distilled water to the desired consistency. |  |
| Part Number | Description |
| [406603030080](https://www.buehler.com/uk/buehler-request-a-quote-uk.php) | 3µm 5lb \[2.3kg\] |
| [406605050080](https://www.buehler.com/uk/buehler-request-a-quote-uk.php) | 5µm 5lb \[2.3kg\] |

##### Related Consumables

[![CarbiMet Silicon Carbide Papers](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/CarbiMet.png)](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/silicon-carbide-grinding-papers/)

[Silicon Carbide Grinding Papers](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/silicon-carbide-grinding-papers/)

[![0011394_apex-dgd-green-240-u-8_600.png](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/0011394_apex-dgd-green-240-u-8_600.png)](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/diamond-grinding-discs/)

[Diamond Grinding Discs](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/diamond-grinding-discs/)

[![MetaDi Diamond Suspension and Paste](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/MetaDi-Diamond-Suspension-and-Paste.png)](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/diamond-suspensions-and-paste/)

[Diamond Suspensions and Paste](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/diamond-suspensions-and-paste/)

[![Premium Polishing Cloths](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Premium-Polishing-Cloths_updated.png)](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/polishing-cloths/)

[Final Polishing Suspension](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/polishing-cloths/)

[![Final Polishing Suspension and Powders](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Final-Polishing-Suspension.png)](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/final-polishing-suspensions/)

[Final Polishing Suspension](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/final-polishing-suspensions/)

##### Product Literature

[![Polishing Guide English](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/10/Polishing-Guide_English.jpg)](https://www.buehler.com/assets/Brochures/English/Consumables/FN01465_0216_Polishing_Application_Guide_WEB.pdf)

[Polishing Guide](https://www.buehler.com/assets/Brochures/English/Consumables/FN01465_0216_Polishing_Application_Guide_WEB.pdf)

[![Buehler Product Catalog](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/Buehler-Product-Catalog_default_600x782.jpg)](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

[Buehler Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

[![Magnetic Backed Polishing Cloth English](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/10/Magnetic-Backed-Polishing-Cloths_English.jpg)](https://www.buehler.com/assets/Brochures/English/Consumables/Magnetic-Polishing-Cloth-Sell-sheet.pdf)

[Magnetic Backed Polishing Cloths](https://www.buehler.com/assets/Brochures/English/Consumables/Magnetic-Polishing-Cloth-Sell-sheet.pdf)

![Full Lab Metallography Solutions](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Dr-Mike-Keeble.jpg)

Find Your Solutions

###### Full Lab Metallography Solutions

Looking for more information from us? Browse through our Solutions section to view technical articles, find recommended processing methods, look at industry solutions, and more.

[Solutions by Industry](https://www.buehler.com/uk/solutions/buehler-solutions/solutions-by-industry/)

[Solutions by Material](https://www.buehler.com/uk/solutions/buehler-solutions/methods-by-material/)

Need Additional Help?

Do you want to improve your process? Reach out for one-on-one help from our applications experts.

![Contact Buehler Lab Team](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Lab-Icon.png)

Contact Lab Team

[Contact Lab](https://www.buehler.com/uk/contact-lab-uk.php)

![Contact Buehler](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Contact-Buehler.png)

Contact Customer Care

[Contact Us](https://www.buehler.com/uk/contact-us-uk.php)

###### Quick Links

Quickly access important info or visit our [E-Shop](https://www.metallography.biz/)

![Product Catalog](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Literature-Icon.png)

Product Catalog

View all Products in the Buehler Product Catalog

[Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

![Methods by Material](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/methods-by-material.png)

Methods by Material

Select a method by material

[Buehler Methods](https://www.buehler.com/uk/solutions/buehler-solutions/solutions-by-material/)

![Safety Data Sheets](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/SDS-Search.png)

SDS

Search Buehler's Safety Data Sheets

[Safety Data Sheets](https://www.buehler.com/uk/solutions/buehler-literature/safety-data-sheets/)

![Buehler Product Literature](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Buehler-Literature-Icon.png)

Product Literature

Browse and search Buehler's product literature

[Product Literature](https://www.buehler.com/uk/solutions/buehler-literature/product-literature/)