---
title: Polishing Cloths
url: https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/polishing-cloths/
date: 2021-10-11T16:14:26+00:00
modified: 2026-05-12T14:42:21+00:00
lang: en_GB
---

# Polishing Cloths

[![Premium Polishing Cloths](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Premium-Polishing-Cloths_updated.png)Premium Polishing Cloths](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Premium-Polishing-Cloths_updated.png)

## HIGH PERFORMACE POLISHING CLOTHS FOR YOUR NEEDS

### Premium Polishing Cloths

Buehler’s premium polishing cloths help you achieve high quality polish in most efficient time.

They are engineered to offer superior surface finish and flatness in your polishing process.

##### A Cloth for Every Application

With a variety of fabrics, weaves and naps, Buehler has a cloth to fit every application need you may have.

##### Delicate Preparation

MicroCut grinding papers provide gentle material removal and superior surface finish when processing delicate or sensitive materials.

##### Reliable Preparation Results

Our premium polishing cloths used with MetaDi® Supreme Diamond Suspension and Pastes offer a complete solution in your labs.

[Shop Now](https://www.metallography.biz/grinding-polishing.php)

### Coarse Polishing

Coarse polishing is the first polishing step after grinding and is typically done using diamond abrasive.

#### UltraPad®

![UltraPad](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/UltraPad.png)

Our most commonly used coarse polishing cloth, UltraPad is a polyester surface very much like sail cloth with an interrupted surface pattern that enhances material removal.

It is most commonly used for engineering materials including ferrous metal alloys, refractory alloys and ceramic.

[Shop UltraPad](https://www.metallography.biz/grinding-polishing.php)

#### UltraPol®

![UltraPol](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/UltraPol.png)

UltraPol is a silk cloth. Softer than UltraPad, UltraPol is great in preparation of mineral samples where it provides excellent flatness, retention of phases and high-quality surface finish.

[Shop UltraPol](https://www.metallography.biz/grinding-polishing.php)

#### Nylon

![Nylon](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Nylon.png)

Nylon cloth is an excellent all-purpose coarse polishing cloth. It is highly suited to polishing soft materials (low-melting point alloys, polymers, and precious metals) and is the most durable cloth choice when working with oil suspensions.

[Shop Nylon](https://www.metallography.biz/grinding-polishing.php)

### Intermediate Polishing

Intermediate polishing is the transition from harder cloths of coarse polishing to somewhat softer cloths that further improve surface finish.

#### TexMet® C

![0011166_texmet-c-2-78inch73mm-20pk.png](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/0011166_texmet-c-2-78inch73mm-20pk.png)

TexMet is a highly versatile choice for intermediate polishing of many materials. It is a non-woven, pressed cloth. It is particularly suited for polishing softer materials such as low-melting point alloys, polymers, precious metals and pure metals.

It is also the most commonly used cloth for manual polishing over a range of polishing steps including coarse, intermediate and fine.

[Shop TexMet C](https://www.metallography.biz/grinding-polishing.php)

#### Trident®

![Trident](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Trident.png)

A synthetic woven cloth, Trident is an excellent cloth for intermediate polishing of engineering alloys (ferrous and refractory alloys).

[Shop Trident](https://www.metallography.biz/grinding-polishing.php)

#### VerduTex®

![Verdutex](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Verdutex.png)

VerduTex is particularly suited to intermediate polishing of large or unmounted samples.

It is also preferred when working with highly abrasion-resistant materials such as ceramic and carbides.

[Shop VerduTex](https://www.metallography.biz/grinding-polishing.php)

#### WhiteFelt®

![WhiteFelt](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/WhiteFelt.png)

White Felt is a thick, soft cloth that can be used for a variety of ferrous and nonferrous metals.

[Shop WhiteFelt](https://www.metallography.biz/grinding-polishing.php)

#### PoliCloth®

![PoliCloth](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/PoliCloth.png)

PoliCloth is a medium hard cloth that suited the best for cast iron, copper and aluminum alloys.

[Shop PoliCloth](https://www.metallography.biz/grinding-polishing.php)

### Fine Polishing

Fine polishing is the last stage of polishing using the softest cloths and finest abrasives (0.05µm to 1µm) to achieve the highest quality surface finish.

#### MicroCloth®

![MicroCloth](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/MicroCloth.png)

Our best selling cloth. A synthetic rayon napped cloth with fibers bonded to a cotton backing, our MicroCloth is the most common, all-purpose fine polishing cloth in the market.

MicroCloth is most often used for polishing ferrous metals, copper alloys, polymers and minerals.

[Shop MicroCloth](https://www.metallography.biz/grinding-polishing.php)

#### MicroFloc®

![MicroFloc](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/MicroFloc.png)

MicroFloc is particularly suited for polishing very soft materials such as low-melting point alloys and precious metals.

[Shop MicroFloc](https://www.metallography.biz/grinding-polishing.php)

#### MasterTex®

![MasterTex](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/MasterTex.png)

MasterTex is best suited to non-homogenous materials where preferential polishing is of great concern. An example would be micro-electronics materials where different materials are present in the same sample, or coatings that differ in abrasion-resistance from the substrate.

[Shop MasterTex](https://www.metallography.biz/grinding-polishing.php)

#### ChemoMet®

![ChemoMet](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/ChemoMet.png)

A polyurethane cloth with a fine, porous surface, ChemoMet is best used for polishing aluminum, refractory metals, silicon and ceramic.

[Shop ChemoMet](https://www.metallography.biz/grinding-polishing.php)

### Polishing Cloth Selection Guide

Buehler’s premium performance cloths are for all material applications and are engineered for long life & superior surface finish.

| Polishing Cloth Selection Guide |  |  |  |  |  |  |  |  |  |  |
| --- | --- | --- | --- | --- | --- | --- | --- | --- | --- | --- |
| Type | Cloth | Backing | Quantity | 8in \[203mm\] | 10in \[254mm\] | 12in \[305mm\] | Description | Recommended Micron Size | Abrasive Type | Applications |
| Coarse | UltraPad® | PSA Magnetic | 10 5 | [40-7118](https://www.metallography.biz/product-information.php?pid=407118) [42-3008](https://www.metallography.biz/product-information.php?pid=423008) | [40-7120](https://www.metallography.biz/product-information.php?pid=407120) [42-3010](https://www.metallography.biz/product-information.php?pid=423010) | [40-7122](https://www.metallography.biz/product-information.php?pid=407122) [42-3012](https://www.metallography.biz/product-information.php?pid=423012) | Hard woven, no nap | 6μm & Up | Diamond | Ferrous materials and thermal spray coatings |
| UltraPol® | PSA | 10 | [40-7448](https://www.metallography.biz/product-information.php?pid=407448) | [40-7450](https://www.metallography.biz/product-information.php?pid=407450) | [40-7452](https://www.metallography.biz/product-information.php?pid=407452) | Hard woven, non-aggressive silk | 6μm & Up | Diamond | Minerals, coals, ceramics, inclusion retention in steels, and refractory metals |  |
| TextMet® P | PSA | 5 | [40-7638](https://www.metallography.biz/product-information.php?pid=407638) | [40-7640](https://www.metallography.biz/product-information.php?pid=407640) | [40-7642](https://www.metallography.biz/product-information.php?pid=407642) | Hard non-woven, perforated | 6μm & Up | Diamond | Electronics, ceramics, carbides, petrographic, hard metals, glass, and metal matrix composites |  |
| Intermediate | Nylon | PSA Magnetic | 10 5 | [40-7068](https://www.metallography.biz/product-information.php?pid=407068) [42-3108](https://www.metallography.biz/product-information.php?pid=423108) | [40-7070](https://www.metallography.biz/product-information.php?pid=407070) [42-3110](https://www.metallography.biz/product-information.php?pid=423110) | [40-7072](https://www.metallography.biz/product-information.php?pid=407072) [42-3112](https://www.metallography.biz/product-information.php?pid=423112) | Medium hard woven, oil resistant, no nap | 6μm & Up | Diamond | Ferrous materials, sintered carbides and cast irons |
| TexMet® C | PSA Magnetic | 10 5 | [40-1108](https://www.metallography.biz/product-information.php?pid=401108) [42-3208](https://www.metallography.biz/product-information.php?pid=423208) | [40-1110](https://www.metallography.biz/product-information.php?pid=401110) [42-3210](https://www.metallography.biz/product-information.php?pid=423210) | [40-1112](https://www.metallography.biz/product-information.php?pid=401112) [42-3212](https://www.metallography.biz/product-information.php?pid=423212) | Non-woven, pressed | 15 - 0.02μm | Diamond, AI2O3, SiO2 | Ferrous and nonferrous metals, ceramics, electronics, PCB’s, thermal spray coatings, cast irons, cermets, minerals, composites, plastics |  |
| TriDent® | PSA Magnetic | 10 5 | [40-7518](https://www.metallography.biz/product-information.php?pid=407518) [42-3308](https://www.metallography.biz/product-information.php?pid=423308) | [40-7520](https://www.metallography.biz/product-information.php?pid=407520) [42-3310](https://www.metallography.biz/product-information.php?pid=423310) | [40-7522](https://www.metallography.biz/product-information.php?pid=407522) [42-3312](https://www.metallography.biz/product-information.php?pid=423312) | Soft woven synthetic, no nap | 15 - 0.02μm | Diamond, AI2O3 | Ferrous and nonferrous metals, microelectronics, polymer matrix composites, coatings |  |
| VerduTex® | PSA Magnetic | 10 5 | [40-8018](https://www.metallography.biz/product-information.php?pid=408018) [42-3408](https://www.metallography.biz/product-information.php?pid=423408) | [40-8020](https://www.metallography.biz/product-information.php?pid=408020) [42-3410](https://www.metallography.biz/product-information.php?pid=423410) | [40-8022](https://www.metallography.biz/product-information.php?pid=408022) [42-3412](https://www.metallography.biz/product-information.php?pid=423412) | Medium hard, synthetic silk | 9 - 1μm | Diamond | Ferrous and nonferrous metals, microelectronics, coatings |  |
| VelTex® | PSA Magnetic | 10 5 | [40-8218](https://www.metallography.biz/product-information.php?pid=408218) [42-3508](https://www.metallography.biz/product-information.php?pid=423508) | [40-8220](https://www.metallography.biz/product-information.php?pid=408220) [42-3510](https://www.metallography.biz/product-information.php?pid=423510) | [40-8222](https://www.metallography.biz/product-information.php?pid=408222) [42-3512](https://www.metallography.biz/product-information.php?pid=423512) | Short nap, synthetic velvet | 9 - 1μm | Diamond | Soft metals |  |
| WhiteFelt® | PSA | 5 | [16-2002](https://www.metallography.biz/product-information.php?pid=162002) | [16-2502](https://www.metallography.biz/product-information.php?pid=162502) | [16-3002](https://www.metallography.biz/product-information.php?pid=163002) | Soft, durable, matted wool | 6 - 0.02μm | Diamond, AI2O3, SiO2 | Ferrous and nonferrous metals |  |
| PoliCloth® | PSA Magnetic | 10 5 | [40-8418](https://www.metallography.biz/product-information.php?pid=408418) [42-3608](https://www.metallography.biz/product-information.php?pid=423608) | [40-8420](https://www.metallography.biz/product-information.php?pid=408420) [42-3610](https://www.metallography.biz/product-information.php?pid=423610) | [40-8422](https://www.metallography.biz/product-information.php?pid=408422) [42-3612](https://www.metallography.biz/product-information.php?pid=423612) | Medium hard, woven wool | 9 - 1μm | Diamond | Soft metals |  |
| Fine | MicroCloth® | PSA Magnetic | 10 5 | [40-7218](https://www.metallography.biz/product-information.php?pid=407218) [42-3708](https://www.metallography.biz/product-information.php?pid=423708) | [40-7220](https://www.metallography.biz/product-information.php?pid=407220) [42-3710](https://www.metallography.biz/product-information.php?pid=423710) | [40-7222](https://www.metallography.biz/product-information.php?pid=407222) [42-3712](https://www.metallography.biz/product-information.php?pid=423712) | Soft synthetic rayon, long nap | 5 - 0.02μm | Diamond, AI2O3, SiO2 | Ferrous and nonferrous metals, ceramics, composites, PCBs, cast irons, cements, plastics, electronics |
| MicroFloc® | PSA Magnetic | 10 5 | [40-8318](https://www.metallography.biz/product-information.php?pid=408318) [42-3808](https://www.metallography.biz/product-information.php?pid=423808) | [40-8320](https://www.metallography.biz/product-information.php?pid=408320) [42-3810](https://www.metallography.biz/product-information.php?pid=423810) | [40-8322](https://www.metallography.biz/product-information.php?pid=408322) [42-3812](https://www.metallography.biz/product-information.php?pid=423812) | Soft, long nap | 3 - 0.02μm | Diamond, AI2O3, SiO2 | Ferrous and nonferrous materials |  |
| MasterTex® | PSA Magnetic | 10 5 | [40-7738](https://www.metallography.biz/product-information.php?pid=407738) [42-3908](https://www.metallography.biz/product-information.php?pid=423908) | [40-7740](https://www.metallography.biz/product-information.php?pid=407740) [42-3910](https://www.metallography.biz/product-information.php?pid=423910) | [40-7742](https://www.metallography.biz/product-information.php?pid=407742) [42-3912](https://www.metallography.biz/product-information.php?pid=423912) | Soft synthetic velvet, low nap | 1 - 0.05μm | AI2O3, SiO2 | Soft nonferrous and microelectronics |  |
| ChemoMet® | PSA Magnetic | 10 5 | [40-7918](https://www.metallography.biz/product-information.php?pid=407918) [42-4008](https://www.metallography.biz/product-information.php?pid=424008) | [40-7920](https://www.metallography.biz/product-information.php?pid=407920) [42-4010](https://www.metallography.biz/product-information.php?pid=424010) | [40-7922](https://www.metallography.biz/product-information.php?pid=407922) [42-4012](https://www.metallography.biz/product-information.php?pid=424012) | Soft synthetic, porous, chemically resistant | 1 - 0.02μm | AI2O3, SiO2 | Titanium, stainless steel, lead/tin, solders, electronics, soft nonferrous metals, plastics |  |

### Apex® Hercules

Apex Hercules is a unique offering from Buehler. Magnetic backed resin surface provides long life and excellent flatness. It’s ideal to use it with diamond suspensions and pastes such as our MetaDi® Supreme products.

#### Apex Hercules H

![Apex Hercules H](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Apex-Hercules-H.png)

Fine grinding disc ideal for grinding hard ferrous and non-ferrous materials (>HRC 20/HV 236).

[Shop Apex Hercules H](https://www.metallography.biz/grinding-polishing.php)

#### Apex Hercules S

![Apex Hercules S](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Apex-Hercules-S.png)

Fine grinding disc ideal for griding soft ferrous and non-ferrous materials (>HRC 20/HV 236).

[Shop Apex Hercules S](https://www.metallography.biz/grinding-polishing.php)

### Polishing Cloth Selection Guide

Magnetic backed resin surface that provides excellent flatness and edge retention. Use with MetaDi® Diamond Suspension.

| Apex Hercules |  |  |  |
| --- | --- | --- | --- |
| Type | 8in \[203mm\] | 10in \[254mm\] | 12in \[305mm\] |
| Apex Hercules H Fine grinding disc for hard ferrous and non-ferrous material (> HRC 20/HV 236) | [41-2740-308-001](https://www.buehler.com/uk/buehler-request-a-quote-uk.php) | [41-2740-310-001](https://www.buehler.com/uk/buehler-request-a-quote-uk.php) | [41-2740-312-001](https://www.buehler.com/uk/buehler-request-a-quote-uk.php) |
| Apex Hercules S Fine Grinding Disc for soft ferrous and non-ferrous material (\< HRC 20/HV 236) | [41-2740-408-001](https://www.buehler.com/uk/buehler-request-a-quote-uk.php) | [41-2740-410-001](https://www.buehler.com/uk/buehler-request-a-quote-uk.php) | [41-2740-412-001](https://www.buehler.com/uk/buehler-request-a-quote-uk.php) |

###### Frequently Asked Questions

#### How long will my cloths last?

Often, a cloth may get contaminated from improper care or gouged before showing significant signs of wear. End of life for a cloth is typically indicated by unusually high polish time or a drastically different texture than when new.

#### How can I extend the life of polishing cloths?

Proper storage and maintenance will enhance cloth life. Rinsing will also extend cloth life, but requires extra abrasive to recharge. Chamfering the edges of your mount will reduce the likelihood of damaging your cloth with a sharp edge.

#### Do I have to use a different cloth for each polishing step?

To avoid cross contamination, each polishing cloth should only be used with one abrasive size. Applying multiple abrasive sizes to a single cloth can create scratches on the specimen during polishing.

#### My PSA backed cloths are hard to remove. How can I get them off more easily?

Use magnetic back cloths, which eliminate cloth removal time, or MagnoPad, a Teflon coated carrier plate.

##### Product Literature

[![Magnetic Backed Polishing Cloth English](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/10/Magnetic-Backed-Polishing-Cloths_English.jpg)](https://www.buehler.com/assets/Brochures/English/Consumables/Magnetic-Polishing-Cloth-Sell-sheet.pdf)

[Magnetic Backed Polishing Cloths](https://www.buehler.com/assets/Brochures/English/Consumables/Magnetic-Polishing-Cloth-Sell-sheet.pdf)

[![Polishing Guide English](https://www.buehler.com/uk/wp-content/uploads/sites/4/2021/10/Polishing-Guide_English.jpg)](https://www.buehler.com/assets/Brochures/English/Consumables/FN01465_0216_Polishing_Application_Guide_WEB.pdf)

[Polishing Guide](https://www.buehler.com/assets/Brochures/English/Consumables/FN01465_0216_Polishing_Application_Guide_WEB.pdf)

[![Buehler Product Catalog](https://www.buehler.com/uk/wp-content/uploads/sites/4/2023/08/Buehler-Product-Catalog_default_600x782.jpg)](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

[Buehler Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

##### Accessories

[![Aluminum Platen System](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Platen-System.png)](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/platen-systems/)

[Platen System](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/platen-systems/)

##### Related Consumables

[![CarbiMet Silicon Carbide Papers](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/CarbiMet.png)](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/silicon-carbide-grinding-papers/)

[Silicon Carbide Grinding Papers](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/silicon-carbide-grinding-papers/)

[![0011394_apex-dgd-green-240-u-8_600.png](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/0011394_apex-dgd-green-240-u-8_600.png)](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/diamond-grinding-discs/)

[Diamond Grinding Discs](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/diamond-grinding-discs/)

[![MetaDi Diamond Suspension and Paste](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/MetaDi-Diamond-Suspension-and-Paste.png)](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/diamond-suspensions-and-paste/)

[Diamond Suspensions and Paste](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/diamond-suspensions-and-paste/)

[![Final Polishing Suspension and Powders](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Final-Polishing-Suspension.png)](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/final-polishing-suspensions/)

[Final Polishing Suspension](https://www.buehler.com/uk/products/grinding-and-polishing/accessories-and-consumables/final-polishing-suspensions/)

![Full Lab Metallography Solutions](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Dr-Mike-Keeble.jpg)

Find Your Solutions

###### Full Lab Metallography Solutions

Looking for more information from us? Browse through our Solutions section to view technical articles, find recommended processing methods, look at industry solutions, and more.

[Solutions by Industry](https://www.buehler.com/uk/solutions/buehler-solutions/solutions-by-industry/)

[Solutions by Material](https://www.buehler.com/uk/solutions/buehler-solutions/methods-by-material/)

Need Additional Help?

Do you want to improve your process? Reach out for one-on-one help from our applications experts.

![Contact Buehler Lab Team](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Lab-Icon.png)

Contact Lab Team

[Contact Lab](https://www.buehler.com/uk/contact-lab-uk.php)

![Contact Buehler](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Contact-Buehler.png)

Contact Customer Care

[Contact Us](https://www.buehler.com/uk/contact-us-uk.php)

###### Quick Links

Quickly access important info or visit our [E-Shop](https://www.metallography.biz/)

![Product Catalog](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Literature-Icon.png)

Product Catalog

View all Products in the Buehler Product Catalog

[Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

![Methods by Material](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/methods-by-material.png)

Methods by Material

Select a method by material

[Buehler Methods](https://www.buehler.com/uk/solutions/buehler-solutions/solutions-by-material/)

![Safety Data Sheets](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/SDS-Search.png)

SDS

Search Buehler's Safety Data Sheets

[Safety Data Sheets](https://www.buehler.com/uk/solutions/buehler-literature/safety-data-sheets/)

![Buehler Product Literature](https://www.buehler.com/uk/wp-content/uploads/sites/4/2024/02/Buehler-Literature-Icon.png)

Product Literature

Browse and search Buehler's product literature

[Product Literature](https://www.buehler.com/uk/solutions/buehler-literature/product-literature/)
