Silicon Carbide Grinding Papers


Buehler’s CarbiMet & MicroCut Silicon Carbide grinding papers are the premier line of SiC grinding discs offering efficient material removal and minimal surface damage. Our discs come in various grit sizes, micron sizes and diameters.

CarbiMet Silicon Carbide grinding discs offers quick grinding times with minimal surface damage during the grinding process. Since there is less damage to remove, the amount of subsequent processing may possibly be reduced, saving valuable time the preparation process.

Apex S Backing allows for fast changeovers between CarbiMet steps. Simply remove the previous SiC grinding paper and apply the next one without needing to remove any backings or liners.

MicroCut abrasive papers provide gentle material removal and superior surface finish when processing delicate or sensitive materials.

High Material Removal with Superior Surface Finish:

 
  • CarbiMet offers quick grinding times with minimal surface damage during the grinding process. Since there is less damage to remove,  the amount of subsequent processing may possibly be reduced, saving valuable time the preparation process.
  • Tightly controlled particle sizes ensures consistent scratch depths and patterns to prevent sample damage and rework.

Quick Change-Overs:

  • Apex S Backing allows for fast changeovers between CarbiMet steps. Simply remove the previous paper and apply the next one without needing to remove any backings or liners.

Delicate Preparation:

  • MicroCut papers provide gentle material removal and superior surface finish when processing delicate or sensitive materials.

No specifications to show at the moment.

CarbiMet S
Grit Size Approx. Micron Size 8"[203mm] 10"[254mm] 12"[305mm]
60 [P60] 260 16-08-0060 16-10-0060 16-12-0060
80 [P80] 188 16-08-0080 16-10-0080 16-12-0080
120 [P120] 127 16-08-0120 16-10-0120 16-12-0120
180 [P180] 78 16-08-0180 16-10-0180 16-12-0180
220 [P240] 58 16-08-0220 16-10-0220 16-12-0220
240 [P280] 52 16-08-0240 16-10-0240 16-12-0240
280 [P320] 46 16-08-0280 16-10-0280 16-12-0280
320 [P400] 35 16-08-0320 16-10-0320 16-12-0320
360 [P600] 26 16-08-0360 16-10-0360 16-12-0360
400 [P800] 22 16-08-0400 16-10-0400 16-12-0400
500 [P1000] 18 16-08-0500 16-10-0500 16-12-0500
600 [P1200] 15 16-08-0600 16-10-0600 16-12-0600
1000 [P2500] 8.4 16-08-1000 16-10-1000 16-12-1000
MicroCut S
800 [P1500] 13 16-08-0800 16-10-0800 16-12-0800
1200 [P2500] 8 16-08-1200 16-10-1200 16-12-1200
P4000 5 16-08-4000 16-10-4000 16-12-4000
PSA Backed
Grit Size Approx. Micron Size 8"[203mm] 10"[254mm] 12"[305mm]
60 [P60] 260 36-08-0060 36-10-0060 36-12-0060
80 [P80] 188 36-08-0080 36-10-0080 36-12-0080
120 [P120] 127 36-08-0120 36-10-0120 36-12-0120
180 [P180] 78 36-08-0180 36-10-0180 36-12-0180
220 [P240] 58 36-08-0220 36-10-0220 36-12-0220
240 [P280] 52 36-08-0240 36-10-0240 36-12-0240
280 [P320] 46 36-08-0280 36-10-0280 36-12-0280
320 [P400] 35 36-08-0320 36-10-0320 36-12-0320
360 [P600] 26 36-08-0360 36-10-0360 36-12-0360
400 [P800] 22 36-08-0400 36-10-0400 36-12-0400
500 [P1000] 18 36-08-0500 36-10-0500 36-12-0500
600 [P1200] 15 36-08-0600 36-10-0600 36-12-0600
1000 [P2500] 8.4 36-08-1000 36-10-1000 36-12-1000
MicroCut
800 [P1500] 13 36-08-0800 36-10-0800 36-12-0800
1200 [P2500] 8 36-08-1200 36-10-1200 36-12-1200
P4000 5 36-08-4000 36-10-4000 36-12-4000
Plain Backed
Grit Size Approx. Micron Size 8"[203mm] 10"[254mm] 12"[305mm]
60 [P60] 260 30-08-0060 30-10-0060 30-12-0060
80 [P80] 188 30-08-0080 30-10-0080 30-12-0080
120 [P120] 127 30-08-0120 30-10-0120 30-12-0120
180 [P180] 78 30-08-0180 30-10-0180 30-12-0180
220 [P240] 58 30-08-0220 30-10-0220 30-12-0220
240 [P280] 52 30-08-0240 30-10-0240 30-12-0240
280 [P320] 46 30-08-0280 30-10-0280 30-12-0280
320 [P400] 35 30-08-0320 30-10-0320 30-12-0320
360 [P600] 26 30-08-0360 30-10-0360 30-12-0360
400 [P800] 22 30-08-0400 30-10-0400 30-12-0400
500 [P1000] 18 30-08-0500 30-10-0500 30-12-0500
600 [P1200] 15 30-08-0600 30-10-0600 30-12-0600
1000 [P2500] 8.4 30-08-1000 30-10-1000 30-12-1000
MicroCut
800 [P1500] 13 30-08-0800 30-10-0800 30-12-0800
1200 [P2500] 8 30-08-1200 30-10-1200 30-12-1200
P4000 5 30-08-4000 30-10-4000 30-12-4000
PSA Backed for Use on MiniMet 1000 CarbiMet
Grit Size 2.875"[73mm]
120 [P120] 36-02-0120
180 [P180] 36-02-0180
240 [P280] 36-02-0240
320 [P400] 36-02-0320
400 [P800] 36-02-0400
600 [P1200] 36-02-0600
MicroCut
800 [P1500] 36-02-0800
1200 [P2500] 36-02-1200


Silicon Carbide Grinding Papers
Sorry no videos at the moment.