# Wilson VH1102 and 1202 Micro Hardness Testers

# Wilson® VH1102 and 1202 Micro Hardness Testers

![Wilson® VH1102 and 1202 Micro Hardness Testers](https://www.buehler.com/wp-content/uploads/2021/10/N9A0184_frontal_S_Touched.png)

*Wilson VH1102 and 1202 Micro Hardness Testers*

## Wilson VH1102 and 1202

### Micro Hardness Testers

The Wilson VH1102 and 1202 Micro Hardness testers provide dependable solutions for precise microhardness testing in quality control and metallurgical research. With testing capabilities ranging from 0.01-2kgf, the VH1102 features a four-position turret for single-scale testing, while the VH1202 offers greater versatility with a six-position turret. Both units support measurements using the digital eyepiece or an optional integrated, high-resolution camera with DiaMet software.

#### Wilson VH1102 and 1202 Benifits

Best in Class Optics

- Precise indenting system paired with a high-quality optical system for unparalleled images
- Optional digital camera housed internally for reliability, protected from dust and misalignment

Automatic Load Selection

- Menu-controlled automatic load selection eliminates the need for a load selector knob
- Wide load range (10gf to 2kgf) with 9 individual load steps, streamlining testing without changing internal mechanics

Dynamic Software Solutions

- Complete your system with optional DiaMet automation software

### Diamet® Hardness Testing Software

Enhance sample throughput while ensuring consistency with minimal complexity through our DiaMet 2.0 software system.

![DiaMet Computer Monitor](https://www.buehler.com/wp-content/uploads/2024/03/DiaMet-Computer-Monitor-1024x442.png)

![DiaMet - Automated](https://www.buehler.com/wp-content/uploads/2024/03/DiaMet-Automated.png)

Automated

By prioritizing swift and simple operation for all users, DiaMet software can utilize high automation, ensuring flexibility for the future.

![DiaMet - Fast](https://www.buehler.com/wp-content/uploads/2024/03/DiaMet-Fast.png)

Fast

Achieving auto-focus and auto-measurement in 5 seconds or less, deliver the fastest test cycle for precise and efficient results.

![DiaMet - Safe](https://www.buehler.com/wp-content/uploads/2024/03/DiaMet-Safe.png)

Safe

Emphasize machine safety with collision-resistant indenters and objectives, ensuring safety meets flexibility.

![DiaMet - Versatile](https://www.buehler.com/wp-content/uploads/2024/03/DiaMet-Versatile.png)

Versatile

Optimized for Vickers, Knoop, Rockwell, Superficial Rockwell, Brinell, and K1c fracture as per ISO and ASTM standards.

[Learn More About DiaMet](https://www.buehler.com/products/hardness-testing/automation-software/diamet-hardness-testing-software/)

#### Ordering

| Wilson VH1102 and 1202 Ordering |  |
| --- | --- |
| [Request a Quote](https://www.buehler.com/buehler-request-a-quote.php) |  |
| Features | Description |
| VH1102 Stand Alone Tester - W1102D03 |  |
| Hardness scales | HV |
| Main-load | 0.01 – 0.025 – 0.05 – 0.1 – 0.2 – 0.3 – 0.5 – 1 - 2kgf |
| Objectives | 10x and 50x Long Working Distance |
| Sample Support | Flat anvil (19mm pin) & Digital XY Stage |
| VH1202 Stand Alone Tester - W1202D03 |  |
| Hardness scales | HV & HK |
| Main-load | 0.01 – 0.025 – 0.05 – 0.1 – 0.2 – 0.3 – 0.5 – 1 - 2kgf |
| Objectives | 5x, 10x and 50x Long Working Distance |
| Sample Support | Flat anvil (19mm pin) & Digital XY Stage |

| VH1102 and 1202 with DiaMet® Automation Software |  |
| --- | --- |
| Part # | Description |
| VH1102 Vickers |  |
| W1102D33 | DiaMet Basic: Manual (Digital) |
| W1102D35 | DiaMet Semi Auto |
| W1102D37 | DiaMet Full Auto |
| W1102D45 | DiaMet Enterprise |
| Part # | Description |
| VH1102 Vickers and Knoop |  |
| W1202D33 | DiaMet Basic: Manual (Digital) |
| W1202D35 | DiaMet Semi Auto |
| W1202D37 | DiaMet Full Auto |
| W1202D45 | DiaMet Enterprise |
| Features | Description |
| Automation included |  |
| DiaMet Basic: Manual (Digital) | Camera, Digital Stage Readout |
| DiaMet Semi Auto | Camera, Motorized 100 x 100mm Stage |
| DiaMet Full Auto | Camera, Motorized 100 x 100mm Stage, Auto-Focus |
| DiaMet Enterprise | Camera, Motorized 100 x 100mm Stage, Auto-Focus |

#### Specifications

|  | Wilson VH1102 | Wilson VH1202 |
| --- | --- | --- |
| Hardness Scales | HV (Vickers), HK (Knoop) |  |
| Turret | Motorized |  |
| Indentors | 1 indenter position Select Vickers or Knoop | 2 indenter position Select Vickers and/or Knoop |
| Standard Objectives | 10x & 50x Regular | 5x, 10x & 50x Long Working Distance |
| Total Magnification | 100x, 500x | 50x, 100x, 500x |
| Test Loads | 0.01 - 0.025 - 0.05 - 0.1 - 0.2 - 0.3 - 0.5 - 1 - 2kgf |  |
| Test Load Accuracy | ±1.5% \< 200g, ±1% > 200g |  |
| Test Cycle Type | Motorized Dead Weight |  |
| Standard Compliance | ASTM E384 & E92;ISO 6507, 9385, 4546 |  |
| Light Source | LED |  |
| XY-Stage Options | Manual 100 x 100mm stage, 25 x 25mm travel Motorized stage 100 x 100mm travel (with PC software only) |  |
| Data-out | USB abd RS232 |  |
| Software Options | Options from basic camera kit to full automatic system available |  |
| Operating Temperature | 50 - 100°F \[10 - 38°C\] |  |
| Humidity | 10 - 90% non-condensing |  |
| Power | 100 - 240VAC, 50/60Hz |  |

#### Consumables and Accessories

[![Hardness Test Blocks](https://www.buehler.com/wp-content/uploads/2024/03/Hardness-Test-Blocks.png)](https://www.buehler.com/products/hardness-testing/hardness-testing-blocks/)

[Test Blocks](https://www.buehler.com/products/hardness-testing/hardness-testing-blocks/)

Available in a wide range that set the standard for industry

[![Carbide Ball](https://www.buehler.com/wp-content/uploads/2024/03/0012356_carbide-ball-116in-for-uh250-iso.png)](https://www.buehler.com/products/hardness-testing/hardness-testing-indenters/)

[Indenters](https://www.buehler.com/products/hardness-testing/hardness-testing-indenters/)

Browse our selection of ISO & ASTM Certified Indenters

[![Self Leveling Vise](https://www.buehler.com/wp-content/uploads/2024/03/0013215_6x-self-leveling-vise-for-round-samples-wo-insert.png)](https://www.buehler.com/products/hardness-testing/hardness-testing-sample-holders-and-anvils/)

[Sample Holders](https://www.buehler.com/products/hardness-testing/hardness-testing-sample-holders-and-anvils/)

Find sample support that’s right for your application

[![Anti Vibration Table](https://www.buehler.com/wp-content/uploads/2024/03/anti-vibration-table.png)](https://shop.buehler.com/active-anti-vibration-table)

[Vickers-Knoop Vibration Isolation Systems](https://shop.buehler.com/active-anti-vibration-table)

Limit outside vibrations and ensure your specimen remains motionless during testing

#### Related Products

[![Wilson VH3100 and VH3300 All in One Hardness Testers](https://www.buehler.com/wp-content/uploads/2024/03/VH3000-All-in-one.png)](https://www.buehler.com/products/hardness-testing/vickers-knoop-hardness-testers/wilson-vh3100-and-vh3300-all-in-one-hardness-tester/)

[Wilson® VH3000 Series All-in-One Hardness Testers](https://www.buehler.com/products/hardness-testing/vickers-knoop-hardness-testers/wilson-vh3100-and-vh3300-all-in-one-hardness-tester/)

Remove complexity with pre-configured machine setups and effortlessly conduct Vickers and Knoop hardness tests.

[![Wilson® VH3100 Vickers & Knoop Hardness Testers](https://www.buehler.com/wp-content/uploads/2021/10/VH3100.png)](https://www.buehler.com/products/hardness-testing/vickers-knoop-hardness-testers/wilson-vh3100-vickers-and-knoop-hardness-testers/)

[Wilson® VH3100 Hardness Tester](https://www.buehler.com/products/hardness-testing/vickers-knoop-hardness-testers/wilson-vh3100-vickers-and-knoop-hardness-testers/)

The workhorse of the VH3000 series. Featuring a 3-position virtual turret with one indenter and two measurement objectives.

[![Wilson® VH3300 Automatic Hardness Tester](https://www.buehler.com/wp-content/uploads/2021/10/VH3300_front-view_no-monitor.png)](https://www.buehler.com/products/hardness-testing/vickers-knoop-hardness-testers/wilson-vh3300-vickers-and-knoop-hardness-tester/)

[Wilson® VH3300 Hardness Tester](https://www.buehler.com/products/hardness-testing/vickers-knoop-hardness-testers/wilson-vh3300-vickers-and-knoop-hardness-tester/)

A completely integrated system for a full range of Vickers & Knoop applications with its fast, six position turret.

#### Product Literature

[![Wilson VH1102 and VH1202 Vickers Knoop Micro-Hardness Tester English](https://www.buehler.com/wp-content/uploads/2021/10/Wilson-VH1102-and-VH1202-Vickers-Knoop-Micro-Hardness-Tester_English.jpg)](https://www.buehler.com/assets/Brochures/English/Hardness/FN01515_VH1102-1202_Brochure_EN_WEB.pdf)

[VH1102 & 1202 Series Brochure](https://www.buehler.com/assets/Brochures/English/Hardness/FN01515_VH1102-1202_Brochure_EN_WEB.pdf)

[![DiaMet Software Brochure English](https://www.buehler.com/wp-content/uploads/2021/10/DiaMet-Brochure_English.jpg)](https://www.buehler.com/assets/Brochures/English/Hardness/DiaMet-Brochure-Update-09-12-2023.pdf)

[DiaMet Brochure](https://www.buehler.com/assets/Brochures/English/Hardness/DiaMet-Brochure-Update-09-12-2023.pdf)

[![Test Block Application Guide](https://www.buehler.com/wp-content/uploads/2024/10/Test-Block-Application-Guide_10-31-2024.png)](https://www.buehler.com/assets/Brochures/English/Hardness/FN01526_Test_Block_Guide_EN_Web.pdf)

[Test Block Application Guide](https://www.buehler.com/assets/Brochures/English/Hardness/FN01526_Test_Block_Guide_EN_Web.pdf)

##### Videos

![Dr. Mike Keeble](https://www.buehler.com/wp-content/uploads/2023/12/Dr-Mike-Keeble.jpg)

Find Your Solutions

###### Full Lab Metallography Solutions

Looking for more information from us? Browse through our Solutions section to view technical articles, find recommended processing methods, look at industry solutions, and more.

[Solutions by Industry](https://www.buehler.com/solutions/buehler-solutions/solutions-by-industry/)

[Solutions by Material](https://www.buehler.com/solutions/buehler-solutions/solutions-by-material/)

Need Additional Help?

Do you want to improve your process? Reach out for one-on-one help from our applications experts.

![Contact Buehler Lab](https://www.buehler.com/wp-content/uploads/2023/12/Lab-Icon.png)

Contact Lab Team

[Contact Lab](https://www.buehler.com/contact-lab.php)

![Contact Buehler](https://www.buehler.com/wp-content/uploads/2023/12/Contact-Buehler.png)

Contact Customer Care

[Contact Us](https://www.buehler.com/contact-us.php)

###### Quick Links

Quickly access important info or visit our [E-Shop](https://shop.buehler.com/)

![Buehler Literature](https://www.buehler.com/wp-content/uploads/2023/05/Literature-Icon.png)

Product Catalog

View all Products in the Buehler Product Catalog

[Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

![](https://www.buehler.com/wp-content/uploads/2023/12/methods-by-material.png)

Methods by Material

Select a method by material

[Buehler Methods](https://www.buehler.com/solutions/buehler-solutions/solutions-by-material/)

![](https://www.buehler.com/wp-content/uploads/2023/12/SDS-Search.png)

SDS

Search Buehler's Safety Data Sheets

[Safety Data Sheets](https://www.buehler.com/solutions/buehler-literature/safety-data-sheets/)

![Buehler Literature Search](https://www.buehler.com/wp-content/uploads/2023/12/Buehler-Literature-Icon.png)

Product Literature

Browse and search Buehler's product literature

[Product Literature](https://www.buehler.com/solutions/buehler-literature/product-literature/)