Buehler’s Planar grinding stones are multi-use abrasive discs designed for the PlanarMet 300 planar grinding machine. They provide high material removal rates and consistent scratch patterns.

Aluminum Oxide Grinding Stone

Versatile abrasive recommended for both hard and soft materials and for extended wheel life. For grinding or cutting carbon steel, high speed steel, tool and die steel and other high alloy, high tensile strength materials.

Silicon Carbide Grinding Stone

A very hard, sharp abrasive grain. Used in grinding of cast iron, aluminum, copper, bronze and non-metallic materials such as plastic and glass. Find all planar grinding stone options in the Ordering tab below.