# 研磨ディスク

# 特殊研削と研磨

[![FibrMet®研磨ディスク](https://buehler.com/jp/wp-content/uploads/sites/11/2024/04/69-3100_fibrmet-discs-4-in-psa-12-mic.jpg)FibrMet®研磨ディスク](https://buehler.com/jp/wp-content/uploads/sites/11/2024/04/69-3100_fibrmet-discs-4-in-psa-12-mic.jpg)[![UltraPrep® ダイヤモンドラッピングフィルム](https://buehler.com/jp/wp-content/uploads/sites/11/2024/04/0011495_ultra-prep8-1-mic-plain.png)UltraPrep® ダイヤモンドラッピングフィルム](https://buehler.com/jp/wp-content/uploads/sites/11/2024/04/0011495_ultra-prep8-1-mic-plain.png)

## SPECIALTY SOLUTIONS

### 特殊ソリューション

アプリケーションによっては、特殊な製品やソリューションが有効な場合があります。様々なダイヤモンドラッピングフィルム、研磨ディスク、パウダーが、用途に応じたニーズにお応えします。

#### UltraPrep® ダイヤモンドラッピングフィルム

![UltraPrep® ダイヤモンドラッピングフィルム](https://buehler.com/jp/wp-content/uploads/sites/11/2024/04/0011495_ultra-prep8-1-mic-plain.png) UltraPrepダイヤモンドラッピングフィルムは、表面の平坦性と最小限の変形が重要な用途向けに設計されています。これらのラッピングフィルムは、0.1µmから30µmまでの幅広いサイズを取り揃えています。用途には、マイクロエレクトロニクス機器、ウェハー、セラミック、光ファイバー、石油化学などが含まれます。

#### FibrMet®研磨ディスク

![](https://buehler.com/jp/wp-content/uploads/sites/11/2024/04/0011174_fibrmet-discs-4-in-psa-12-mic.png) FibrMet研磨ディスクは、酸化アルミニウム研磨材でコーティングされています。湿式でも乾式でも使用でき、表面の平坦性が重要な光ファイバーやマイクロエレクトロニクスなどの精密研削や研磨用途に最適です。これらの研磨ディスクは、0.3µmから12µmまでの幅広いサイズを取り揃えています。

#### アブレッシブ®パウダー

![](https://buehler.com/jp/wp-content/uploads/sites/11/2024/04/0013738_aluminum-oxide-powder-3m-5lb.png) Abrasive®(アブレッシブ®)パウダーは、鋳鉄や錫材料の微粉砕用です。目的の粘度にするためには、蒸留水との混合が必要です。

##### 品番

| UltraPrep ダイヤモンドラッピングフィルム (5枚) |  |  |
| --- | --- | --- |
| UltraPrep Diamond Lapping Films are designed for various material applications including microelectronic devices, wafers, ceramics, optical fibers, petrographic, and other metallographic materials. Ideal for preparation applica- tions where surface flatness and minimal deformation are critical. |  |  |
| 砥粒径 | 8インチ 裏のり付 | 8インチ 裏のりなし |
| 0.1µm | [15-6791](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [15-6792](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 0.5µm | [15-6795](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [15-6796](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 1µm | [15-6801](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [15-6802](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 3µm | [15-6803](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [15-6804](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 6µm | [15-6806](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [15-6807](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 9µm | [15-6809](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [15-6810](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 15µm | [15-6815](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [15-6816](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 30µm | [15-6830](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [15-6831](https://buehler.com/jp/buehler-request-a-quote-japan.php) |

| FibrMet研磨ディスク (50枚) |  |  |  |
| --- | --- | --- | --- |
| FibrMet Abrasive Disc are PSA (polyester backed) films, approx. 0.1 mm thick, coated with an aluminum oxide abrasive. These discs can be used wet or dry and are most suitable for fine grinding and polishing application, such as optical fiber and microelectronics where resultant surface flatness is essential. |  |  |  |
| 砥粒径 | 4インチ | 8インチ | 12インチ |
| 0.3μm | [69-3104](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3174](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3124](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 1μm | [69-3103](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3173](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3123](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 3μm | [69-3102](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3172](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3122](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 9μm | [69-3101](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3171](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3121](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 12μm | [69-3100](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3170](https://buehler.com/jp/buehler-request-a-quote-japan.php) |  |

| アブレッシブパウダー |  |
| --- | --- |
| Aluminum Oxide Powder is used for fine grinding on cast iron, tin, or cloth-covered platens. They are mixed with distilled water to the desired consistency. |  |
| 品番 | 説明 |
| [406603030080](https://buehler.com/jp/buehler-request-a-quote-japan.php) | 3µm 5lb \[2.3kg\] |
| [406605050080](https://buehler.com/jp/buehler-request-a-quote-japan.php) | 5µm 5lb \[2.3kg\] |

| UltraPrep ダイヤモンドラッピングフィルム (5枚) |  |  |
| --- | --- | --- |
| UltraPrep Diamond Lapping Films are designed for various material applications including microelectronic devices, wafers, ceramics, optical fibers, petrographic, and other metallographic materials. Ideal for preparation applica- tions where surface flatness and minimal deformation are critical. |  |  |
| 砥粒径 | 8インチ 裏のり付 | 8インチ 裏のりなし |
| 0.1µm | [15-6791](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [15-6792](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 0.5µm | [15-6795](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [15-6796](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 1µm | [15-6801](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [15-6802](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 3µm | [15-6803](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [15-6804](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 6µm | [15-6806](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [15-6807](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 9µm | [15-6809](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [15-6810](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 15µm | [15-6815](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [15-6816](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 30µm | [15-6830](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [15-6831](https://buehler.com/jp/buehler-request-a-quote-japan.php) |

| FibrMet研磨ディスク (50枚) |  |  |  |
| --- | --- | --- | --- |
| FibrMet Abrasive Disc are PSA (polyester backed) films, approx. 0.1 mm thick, coated with an aluminum oxide abrasive. These discs can be used wet or dry and are most suitable for fine grinding and polishing application, such as optical fiber and microelectronics where resultant surface flatness is essential. |  |  |  |
| 砥粒径 | 4インチ | 8インチ | 12インチ |
| 0.3μm | [69-3104](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3174](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3124](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 1μm | [69-3103](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3173](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3123](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 3μm | [69-3102](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3172](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3122](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 9μm | [69-3101](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3171](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3121](https://buehler.com/jp/buehler-request-a-quote-japan.php) |
| 12μm | [69-3100](https://buehler.com/jp/buehler-request-a-quote-japan.php) | [69-3170](https://buehler.com/jp/buehler-request-a-quote-japan.php) |  |

| アブレッシブパウダー |  |
| --- | --- |
| Aluminum Oxide Powder is used for fine grinding on cast iron, tin, or cloth-covered platens. They are mixed with distilled water to the desired consistency. |  |
| 品番 | 説明 |
| [406603030080](https://buehler.com/jp/buehler-request-a-quote-japan.php) | 3µm 5lb \[2.3kg\] |
| [406605050080](https://buehler.com/jp/buehler-request-a-quote-japan.php) | 5µm 5lb \[2.3kg\] |

##### 関連製品

[![炭化ケイ素耐水研磨紙](https://buehler.com/jp/wp-content/uploads/sites/11/2024/04/CarbiMet.png)](https://buehler.com/jp/%e8%a3%bd%e5%93%81%e6%83%85%e5%a0%b1/%e7%a0%94%e7%a3%a8/%e3%82%a2%e3%82%af%e3%82%bb%e3%82%b5%e3%83%aa%e6%b6%88%e8%80%97%e5%93%81/%e8%80%90%e6%b0%b4%e7%a0%94%e7%a3%a8%e7%b4%99/)

[炭化ケイ素耐水研磨紙](https://buehler.com/jp/%e8%a3%bd%e5%93%81%e6%83%85%e5%a0%b1/%e7%a0%94%e7%a3%a8/%e3%82%a2%e3%82%af%e3%82%bb%e3%82%b5%e3%83%aa%e6%b6%88%e8%80%97%e5%93%81/%e8%80%90%e6%b0%b4%e7%a0%94%e7%a3%a8%e7%b4%99/)

[![ダイヤモンド研磨ディスク](https://buehler.com/jp/wp-content/uploads/sites/11/2024/04/DGD-Color.png)](https://buehler.com/jp/%e8%a3%bd%e5%93%81%e6%83%85%e5%a0%b1/%e7%a0%94%e7%a3%a8/%e3%82%a2%e3%82%af%e3%82%bb%e3%82%b5%e3%83%aa%e6%b6%88%e8%80%97%e5%93%81/%e3%83%80%e3%82%a4%e3%82%a2%e3%83%a2%e3%83%b3%e3%83%89%e3%82%b0%e3%83%a9%e3%82%a4%e3%83%b3%e3%83%87%e3%82%a3%e3%83%b3%e3%82%b0-%e3%83%87%e3%82%a3%e3%82%b9%e3%82%af/)

[ダイヤモンドディスク](https://buehler.com/jp/%e8%a3%bd%e5%93%81%e6%83%85%e5%a0%b1/%e7%a0%94%e7%a3%a8/%e3%82%a2%e3%82%af%e3%82%bb%e3%82%b5%e3%83%aa%e6%b6%88%e8%80%97%e5%93%81/%e3%83%80%e3%82%a4%e3%82%a2%e3%83%a2%e3%83%b3%e3%83%89%e3%82%b0%e3%83%a9%e3%82%a4%e3%83%b3%e3%83%87%e3%82%a3%e3%83%b3%e3%82%b0-%e3%83%87%e3%82%a3%e3%82%b9%e3%82%af/)

[![ダイヤモンドサスペンションとペースト](https://buehler.com/jp/wp-content/uploads/sites/11/2024/04/MetaDi-Diamond-Suspension-and-Paste.png)](https://buehler.com/jp/%e8%a3%bd%e5%93%81%e6%83%85%e5%a0%b1/%e7%a0%94%e7%a3%a8/%e3%82%a2%e3%82%af%e3%82%bb%e3%82%b5%e3%83%aa%e6%b6%88%e8%80%97%e5%93%81/%e3%83%80%e3%82%a4%e3%82%a2%e3%83%a2%e3%83%b3%e3%83%89%e3%82%b5%e3%82%b9%e3%83%9a%e3%83%b3%e3%82%b7%e3%83%a7%e3%83%b3-%e3%83%9a%e3%83%bc%e3%82%b9%e3%83%88/)

[ダイヤモンドサスペンションとペースト](https://buehler.com/jp/%e8%a3%bd%e5%93%81%e6%83%85%e5%a0%b1/%e7%a0%94%e7%a3%a8/%e3%82%a2%e3%82%af%e3%82%bb%e3%82%b5%e3%83%aa%e6%b6%88%e8%80%97%e5%93%81/%e3%83%80%e3%82%a4%e3%82%a2%e3%83%a2%e3%83%b3%e3%83%89%e3%82%b5%e3%82%b9%e3%83%9a%e3%83%b3%e3%82%b7%e3%83%a7%e3%83%b3-%e3%83%9a%e3%83%bc%e3%82%b9%e3%83%88/)

[![研磨バフ](https://buehler.com/jp/wp-content/uploads/sites/11/2024/04/Premium-Polishing-Cloths_updated.png)](https://buehler.com/jp/%e8%a3%bd%e5%93%81%e6%83%85%e5%a0%b1/%e7%a0%94%e7%a3%a8/%e3%82%a2%e3%82%af%e3%82%bb%e3%82%b5%e3%83%aa%e6%b6%88%e8%80%97%e5%93%81/%e7%a0%94%e7%a3%a8%e7%94%a8%e3%83%90%e3%83%95/)

[研磨バフ](https://buehler.com/jp/%e8%a3%bd%e5%93%81%e6%83%85%e5%a0%b1/%e7%a0%94%e7%a3%a8/%e3%82%a2%e3%82%af%e3%82%bb%e3%82%b5%e3%83%aa%e6%b6%88%e8%80%97%e5%93%81/%e7%a0%94%e7%a3%a8%e7%94%a8%e3%83%90%e3%83%95/)

[![最終研磨用サスペンションとパウダー](https://buehler.com/jp/wp-content/uploads/sites/11/2024/04/Final-Polishing-Suspension.png)](https://buehler.com/jp/%e8%a3%bd%e5%93%81%e6%83%85%e5%a0%b1/%e7%a0%94%e7%a3%a8/%e3%82%a2%e3%82%af%e3%82%bb%e3%82%b5%e3%83%aa%e6%b6%88%e8%80%97%e5%93%81/%e4%bb%95%e4%b8%8a%e3%81%92%e7%94%a8%e7%a0%94%e7%a3%a8%e5%89%a4/)

[最終研磨用サスペンションとパウダー](https://buehler.com/jp/%e8%a3%bd%e5%93%81%e6%83%85%e5%a0%b1/%e7%a0%94%e7%a3%a8/%e3%82%a2%e3%82%af%e3%82%bb%e3%82%b5%e3%83%aa%e6%b6%88%e8%80%97%e5%93%81/%e4%bb%95%e4%b8%8a%e3%81%92%e7%94%a8%e7%a0%94%e7%a3%a8%e5%89%a4/)

##### 製品カタログ

[![アプリケーションガイド研磨](https://buehler.com/jp/wp-content/uploads/sites/11/2021/10/grinding-and-polishing-guide-Japanese.jpg)](https://buehler.com/assets/Brochures/Japan/Consumables/FN01465JP_Polishing-Application-Guide_021016_WEB.pdf) [研磨ガイド](https://buehler.com/assets/Brochures/Japan/Consumables/FN01465JP_Polishing-Application-Guide_021016_WEB.pdf) [![](https://buehler.com/jp/wp-content/uploads/sites/11/2024/04/Buehler-Product-Catalog_default_600x782.jpg)](https://www.calameo.com/buehler/read/00639329184b15ac80c23) [Buehler 製品カタログ](https://www.calameo.com/buehler/read/00639329184b15ac80c23)