Final Polishing Suspensions Specifications |
---|
MasterPrep Alumina |
Sol-gel alumina suspension |
0.05µm |
~8.5pH |
Excellent for minerals, ferrous metals, low melting point alloys, carbides, PWB"s, precious metals and electronics. |
MasterMet Colloidal Silica |
Amorphous colloidal silica suspension |
0.06µm |
~10pH |
Chemo-mechanical polishing action |
Excellent for metals, minerals, ceramics, and polymers |
MasterMet 2 Colloidal Silica |
Non-crystallizing amorphous colloidal silica suspension suitable for automatic dispensing |
0.02µm |
~10.5pH |
Chemo-mechanical polishing action |
Excellent for metals, minerals, ceramics, and polymers |
MasterPolish Final Polish |
Blend of high purity alumina and colloidal silica |
0.05µm |
~9pH |
Contains minimal water and is optimal for water sensitive materials |
Excellent for most magnesium alloys, cobalt alloys, most iron alloys, nickel, and metal matrix composites |
MasterPolish 2 FInal Polish |
Iron oxide suspension |
0.06µm |
~10pH |
Chemo-mechanical polishing action |
Excellent for sapphire, glass, alumina, silicon nitride, and metal/ceramic composites |
MicroPolish Alumina Suspension |
Agglomerated alumina offering higher removal rates compared to other aluminas of the same size |
Available in Suspension or Powder form |
Available in 0.05µm, 0.3µm, and 1µm |
Good for use on magnesium, lead, and their alloys |
MicroPolish Alumina Powder |
Agglomerated alumina powders offering high removal rates |
Available in 0.05µm and 1µm |
Suitable for use on pure and alloyed lead and magnesium |
MicroPolish II Alumina Powder |
High quality deagglomerated alumina powders offering good surface finish |
Available in 0.3µm and 1µm |
Suitable for most minerals and metals |
MicroPolish II Alumina Suspension |
High quality deagglomerated alumina powders offering good surface finish |
Available in 0.3µm |
Suitable for most minerals and metals |
Final Polishing Suspensions | |||||
---|---|---|---|---|---|
Product | Micron Size | 6oz[0.18L] | 32oz[0.95L] | 64oz[1.9L] | |
MasterPrep Alumina | 0.05µm | 63-6377-006 | 40-6377-032 | 40-6377-064 | |
MasterMet Colloidal Silica | 0.06µm | 40-6370-006 | 40-6370-064 | ||
MasterMet 2 Non-Crystalizing Colloidal Silica | 0.02µm | 40-6380-006 | 40-6380-064 | ||
MasterPolish Final Polish | 0.05µm | 40-10084 | |||
MasterPolish 2 Final Polish | 0.06µm | 40-6376-032 |
Powder | Suspension | ||||
---|---|---|---|---|---|
Product | Micron Size | 1lb[0.45kg] | 5lb[2.3kg] | 6oz[0.18L] | 128oz[3.8L] |
MicroPolish Alumina | 0.05µm | 40-10075 | 40-10076 | 40-10083 | |
MicroPolish Alumina | 0.3µm | 40-10077 | 40-10078 | 40-10082 | |
MicroPolish Alumina | 1µm | 40-10079 | 40-10080 | 40-10081 | |
MicroPolish II Alumina | 0.3µm | 40-6323-016 | 40-6323-080 | 40-6363-006 | 40-6363-128 |
MicroPolish II Alumina | 1µm | 40-6322-016 |