Diamond Suspensions and Paste Specifications | ||||
---|---|---|---|---|
Product | Diamond Type | Material Removal | Surface Deformation | Application |
MetaDi Supreme Suspension | Polycrystalline | Best | Minimal | Fastest material removal and minimal subsurface deformation |
Dye-Free MetaDi Supreme Suspension | Polycrystalline | Best | Minimal | For materials that may absorb dye and affect image analysis |
MetaDi Monocrystalline Suspension | Monocrystalline | Better | Minor | Good material removal for most materials |
Oil-Based MetaDi Monocrystalline Suspension | Monocrystalline | Better | Minor | For materials that are water-sensitive |
MetaDi Combo Suspension | Monocrystalline | Better | Minor | Suspension and extender fluid combination to maintain consistency when used with automated systems |
MetaDi Ultra Paste | Polycrystalline | Better | Minimal | Efficient material removal for soft materials that may be prone to diamond embedding |
MetaDi Heavy Concentration Paste | Monocrystalline | Good | Minor | High concentration paste for materials that are prone to diamond embedding |
MetaDi II Medium Concentration Paste | Monocrystalline | Good | Minor | Reduced diamond content for materials that are very prone to diamond embedding |
MetaDi™ Supreme Polycrystalline Suspension | ||||
---|---|---|---|---|
Color | Diamond Size | 8oz[0.24L] | 32oz[0.95L] | 1gal[3.8L] |
0.05 µm | 40-6627 | |||
0.25 µm | 40-6629 | 40-6629-128 | ||
1 µm | 40-6630 | 40-6630-032 | 40-6630-128 | |
1 µm Fine | 40-6630F | 40-6630F-032 | 40-6630F-128 | |
3 µm | 40-6631 | 40-6631-032 | 40-6631-128 | |
3 µm Fine | 40-6631F | 40-6631F-032 | 40-6631F-128 | |
6 µm | 40-6632 | 40-6632-032 | 40-6632-128 | |
9 µm | 40-6633 | 40-6633-032 | 40-6633-128 | |
15 µm | 40-6634 | 40-6634-032 | 40-6634-128 | |
30 µm | 40-6635 | 40-6635-032 | 40-6635-128 | |
45 µm | 40-6636 |
MetaDi Monocrystalline Suspension | ||||
---|---|---|---|---|
Color | Diamond Size | 16oz[0.47L] | 32oz[0.95L] | 1gal[3.8L] |
1 µm | 40-6530 | 40-6530-032 | 40-6530-128 | |
3 µm | 40-6531 | 40-6531-032 | 40-6531-128 | |
6 µm | 40-6532 | 40-6532-032 | 40-6532-128 | |
9 µm | 40-6533 | 40-6533-032 | 40-6533-128 | |
15 µm | 40-6534 | 40-6534-032 | 40-6534-128 |
Dye-Free MetaDi Supreme Polycrystalline Suspension | ||
---|---|---|
Diamond Size | 8oz[0.24L] | 32oz[0.95L] |
1 µm | 40-6730 | 40-6730-032 |
3 µm | 40-6731 | 40-6731-032 |
6 µm | 40-6732 | 40-6732-032 |
9 µm | 40-6733 | 40-6733-032 |
Oil-Based MetaDi Monocrystalline Suspension | ||
---|---|---|
Color | Diamond Size | 16oz[0.47L] |
1 µm | 40-6540 | |
3 µm | 40-6541 | |
6 µm | 40-6542 | |
9 µm | 40-6543 | |
15 µm | 40-6544 |
MetaDi Combo, Diamond Suspension + Extender | ||
---|---|---|
Color | Diamond Size | 32oz[0.95L] |
1 µm | 40-5530-032 | |
3 µm | 40-5531-032 | |
6 µm | 40-5532-032 | |
9 µm | 40-5534-032 |
MetaDi Ultra Polycrystalline Paste | ||
---|---|---|
Color | Diamond Size | 20g |
1 µm | 40-1-6301 | |
3 µm | 40-1-6303 | |
6 µm | 40-1-6305 | |
9 µm | 40-1-6307 | |
15 µm | 40-1-6309 |
MetaDi & MetaDi II Monocrystalline Paste | |||||
---|---|---|---|---|---|
MetaDi Heavy Concentration | MetaDi II Medium Concentration | ||||
Color | Diamond Size | 5g | 20g | 5g | 20g |
0.25µm | 40-6112 | 40-6102 | 40-6241 | 40-6240 | |
1µm | 40-6138 | 40-6128 | 40-6244 | 40-6243 | |
3µm | 40-6152 | 40-6142 | 40-6247 | 40-6246 | |
6µm | 40-6172 | 40-6162 | 40-6250 | 40-6249 | |
9µm | 40-6192 | 40-6182 | 40-6253 | 40-6252 | |
15µm | 40-6212 | 40-6202 | 40-6256 | 40-6255 |