title: IsoMet Low Speed Precision Cutter
url: https://www.buehler.com/ca/products/sectioning/precision-cutters/isomet-low-speed-precision-cutter/
date: 2021-09-02T16:44:40+00:00
modified: 2025-07-10T13:47:33+00:00
lang: en_CA
---

# IsoMet® Low Speed Precision Cutter

[![IsoMet® Low Speed Precision Cutter](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/09/IsoMet-Low-Speed-Saw.png)IsoMet® Low Speed Precision Cutter](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/09/IsoMet-Low-Speed-Saw.png)

[![IsoMet® Low Speed Precision Cutter](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/09/Iso-Met-Lo-Speed-side-open.png)IsoMet® Low Speed](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/09/Iso-Met-Lo-Speed-side-open.png)

[![Splash Guard Kit IsoMet Low Speed](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/09/111199_Splash-Guard-Kit.png)Splash Guard Kit IsoMet Low Speed](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/09/111199_Splash-Guard-Kit.png)

## IsoMet Low Speed

### Gravity-fed Precision Sectioning Machine

The IsoMet Low Speed precision cutter is a compact gravity-fed precision saw, 5in \[127mm\] tabletop machine that delivers the gentlest cut for your sample. Its precision micrometer and user-friendly controls give total control to the user. Pair with Buehler’s diamond / CBN blades and IsoCut coolant for a comprehensive solution with the highest level of quality.

#### IsoMet Low Speed Benefits

Exceptional Precision and Quality

- Gravity-fed arm minimizes sample stress ensuring a delicate cut
- Precision micrometer guarantees accurate sample width
- Specialized sample chucks for the smallest and most delicate samples

Easy to Use

- Easily adjustable cutting arm allows users to change vises quickly
- Adjustable motor speed up to 300rpm for various applications
- Removable catch tray for easy retrieval of cut sample

Ordering

| IsoMet Low Speed - Ordering |  |  |  |
| --- | --- | --- | --- |
| Part Number | Voltage | Units | Request a Quote |
| 11-1280-160 | 115VAC, 50/60Hz | Inches | [Request a Quote](https://www.buehler.com/ca/buehler-request-a-quote-canada.php?pn=11-1280-160) |
| 11-1280-170 | 115VAC, 50/60Hz | Millimeters | [Request a Quote](https://www.buehler.com/ca/buehler-request-a-quote-canada.php?pn=11-1280-170) |
| 11-1280-250 | 230VAC, 50/60Hz | Millimeters | [Request a Quote](https://www.buehler.com/ca/buehler-request-a-quote-canada.php?pn=11-1280-250) |

Specifications

| IsoMet Low Speed |  |
| --- | --- |
| Frequency | universal |
| Voltage | 115, 220 |
| Phase | 1 |
| Cutting Capacity | 1.50\[in\], 38.00\[mm\] |
| Wheel Diameter | 5.00\[in\] |
| Controls | Push Button |
| Cut Action | Gravity Fed Chop |
| Programmability | No |
| Serial Capabilities | No |
| Wheel Diameter | 127\[mm\] |
| RPM @60 | Hz: 300 |

##### Consumables and Accessories

[![Precision Blades](https://www.buehler.com/ca/wp-content/uploads/sites/3/2023/10/Precision-Blades.jpg)](https://www.buehler.com/ca/products/sectioning/accessories-consumables/diamond-and-cbn-blades-for-sectioning/)

[Precision Blades](https://www.buehler.com/ca/products/sectioning/accessories-consumables/diamond-and-cbn-blades-for-sectioning/)

Blades for Precision Saws and Cutters

[![Precision Vises for Sectioning](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/08/111187-Single-Saddle-Chuck.jpg)](https://www.buehler.com/ca/products/sectioning/accessories-consumables/precision-vises-for-sectioning/)

[Precision Vising](https://www.buehler.com/ca/products/sectioning/accessories-consumables/precision-vises-for-sectioning/)

Vising for Precision Saws and Cutters

[![Cool 3 Coolants](https://www.buehler.com/ca/wp-content/uploads/sites/3/2023/08/Cool-3-Group-Photo.png)](https://www.buehler.com/ca/products/sectioning/accessories-consumables/coolants-for-sectioning/)

[Cool 3](https://www.buehler.com/ca/products/sectioning/accessories-consumables/coolants-for-sectioning/)

Coolants for Sectioning Machines

[![Flange Sets for Sectioning](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/08/11-2283_IsoMet-4in-Flange-Set.png)](https://www.buehler.com/ca/products/sectioning/accessories-consumables/flange-sets/)

[Flange Sets](https://www.buehler.com/ca/products/sectioning/accessories-consumables/flange-sets/)

Flanges for Precision Machines

###### Related Products

[![IsoMet® 1000 Precision Cutter](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/08/IsoMet-1000_600x600.jpg)](https://www.buehler.com/ca/products/sectioning/precision-cutters/isomet-1000-precision-cutter/)

[IsoMet® 1000](https://www.buehler.com/ca/products/sectioning/precision-cutters/isomet-1000-precision-cutter/)

7in \[178mm\]
Gravity-fed Precision Saw

[![IsoMet High Speed Pro](https://www.buehler.com/ca/wp-content/uploads/sites/3/2025/05/IsoMet-High-Speed-Pro_112800.jpg)](https://www.buehler.com/ca/products/sectioning/precision-cutters/isomet-high-speed-pro/)

[IsoMet® High Speed Pro](https://www.buehler.com/ca/products/sectioning/precision-cutters/isomet-high-speed-pro/)

8in \[203mm\]
Automatic Precision Saw

[![PetroThin® Thin Sectioning Machine](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/08/Petro-Thin-Face.png)](https://www.buehler.com/ca/products/sectioning/precision-cutters/petrothin-thin-section-machine/)

[PetroThin®](https://www.buehler.com/ca/products/sectioning/precision-cutters/petrothin-thin-section-machine/)

8in \[203mm\]
Thin Section Saw/Cup Grinder

[![AbrasiMet® M Manual Abrasive Cutter](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/08/AbrasiMet-M-3qtrs-open.png)](https://www.buehler.com/ca/products/sectioning/abrasive-cutters/abrasimet-m-manual-abrasive-cutter/)

[AbrasiMet® M](https://www.buehler.com/ca/products/sectioning/abrasive-cutters/abrasimet-m-manual-abrasive-cutter/)

12in \[305mm\]
Manual Abrasive Saw

Product Literature

[![IsoMet Low Speed Brochure](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/09/English-IsoMet-Low-Speed-Saw_06-28-2021.jpg)](https://www.buehler.com/assets/Brochures/English/Sectioning/IsoMet-Low-Speed-Saw-Brochure-Update-0621-Web.pdf)

[IsoMet Low Speed Brochure](https://www.buehler.com/assets/Brochures/English/Sectioning/IsoMet-Low-Speed-Saw-Brochure-Update-0621-Web.pdf)

[![Buehler Product Catalog](https://www.buehler.com/ca/wp-content/uploads/sites/3/2023/08/Buehler-Product-Catalog_default_600x782.jpg)](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

[Buehler Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

![Full Lab Metallography Solutions](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Dr-Mike-Keeble.jpg)

Find Your Solutions

###### Full Lab Metallography Solutions

Looking for more information from us? Browse through our Solutions section to view technical articles, find recommended processing methods, look at industry solutions, and more.

[Solutions by Industry](https://www.buehler.com/ca/solutions/buehler-solutions/solutions-by-industry/)

[Solutions by Material](https://www.buehler.com/ca/solutions/buehler-solutions/methods-by-material/)

Need Additional Help?

Do you want to improve your process? Reach out for one-on-one help from our applications experts.

![Contact Buehler Lab Team](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Lab-Icon.png)

Contact Lab Team

[Contact Lab](https://www.buehler.com/ca/contact-lab-canada.php)

![Contact Buehler Customer Care](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Contact-Buehler.png)

Contact Customer Care

[Contact Us](https://www.buehler.com/ca/contact-us-canada.php)

###### Quick Links

Quickly access important info or visit our [E-Shop](https://shop.opti-tech.com/). Buehler is represented in Canada by Opti-tech Scientific

![Buehler Product Catalog](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Literature-Icon.png)

Product Catalog

View all Products in the Buehler Product Catalog

[Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

![Methods by Material](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/methods-by-material.png)

Methods by Material

Select a method by material

[Buehler Methods](https://www.buehler.com/ca/solutions/buehler-solutions/solutions-by-material/)

![Safety Data Sheets](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/SDS-Search.png)

SDS

Search Buehler's Safety Data Sheets

[Safety Data Sheets](https://www.buehler.com/ca/solutions/buehler-literature/safety-data-sheets/)

![Buehler Product Literature](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Buehler-Literature-Icon.png)

Product Literature

Browse and search Buehler's product literature

[Product Literature](https://www.buehler.com/ca/solutions/buehler-literature/product-literature/)