# AbrasiMet® XL Pro Automatic Abrasive Cutter

[![AbrasiMet XL Pro Automatic Abrasive Cutter](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/07/AbrasiMet-XL-Pro-Front.png)AbrasiMet® XL Pro Automatic Abrasive Cutter](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/07/AbrasiMet-XL-Pro-Front.png)

[![AbrasiMet XL Pro Automatic Abrasive Cutter](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/07/AbrasiMet-XL-Pro-3qtrs.png)AbrasiMet® XL Pro](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/07/AbrasiMet-XL-Pro-3qtrs.png)

[![AbrasiMet XL Pro Automatic Abrasive Cutter Cutting Gear](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/07/abrasimet-xl-cutting-gear.jpg)AbrasiMet® XL Pro](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/07/abrasimet-xl-cutting-gear.jpg)

[![AbrasiMet XL Pro Automatic Abrasive Cutter User Interface](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/07/abrasimet-xl-user-interface.jpg)AbrasiMet® XL Pro](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/07/abrasimet-xl-user-interface.jpg)

## AbrasiMet XL Pro

### Automatic Abrasive Sectioning Machine

The AbrasiMet XL Pro automatic abrasive saw is ideal for the most demanding environments. This 18″ \[407mm\] cutter gives consistent and repeatable cut quality while featuring intuitive controls and the power you need to cut your largest samples. Combine with Buehler’s abrasive blades for a complete cutting solution providing optimal surface quality and low cycle time.

#### AbrasiMet XL Pro Benefits

Powerful for Difficult Cuts

- 13.4hp \[10kW\] motor for the largest samples
- Variable SmartCut to control sample quality even on aggressive cuts
- Planar Cutting mode to combine Z and Y axis cutting for the largest and hardest cut pieces

Fast Setup

- Easy to use touchscreen
- 4 cutting types: Chop (Z cut), Y-feed (linear), Planar (sawing motion), and Manual
- Aligning laser, bright chamber lights, and large viewing windows
- Serial cutting for programming multiple cuts at once
- Oversized chamber and door for the largest parts and easy placement

Reliable and Easy to Clean

- Enclosed Motor to keep coolant and debris out
- Filtering recirculation system to increase ease of cleaning
- Overhead washdown to clean the walls, doors, and cutting arm

Ordering

| AbrasiMet XL Pro - Ordering |  |  |
| --- | --- | --- |
| Part Number | Voltage | Request a Quote |
| 10-2320-400 | 380-480VAC, 50/60Hz | [Request a Quote](https://www.buehler.com/ca/buehler-request-a-quote-canada.php?pn=10-2320-400) |

Specifications

| AbrasiMet XL Pro |  |
| --- | --- |
| Operation | Automatic, Manual |
| Motor Power | 13.4Hp \[10Kw\] |
| Main Power | 380-480VAC, 3 Phase, 50/60Hz |
| Main Current | 25amp @ 460VAC |
| Blade Movement Axis | Horizontal, Linear, Vertical(X,Y,Z) |
| Blade Sizes | 14in\[356mm\], 16in\[406mm\], 18in\[457mm\] |
| Blade Table Clearance | 9.71in\[247mm\], 8.71in\[221mm\], 7.71in\[196mm\] |
| Cut Capacity | 5in\[127mm\], 6in\[152mm\], 7in\[178mm\] |
| Blade Speed | 2100rpm, 1900rpm, 1860rpm |
| Cut Type | Chop, Y-Feed, Planar |
| Lighting | 4 LEDs |
| Laser | Green Laser(520nm, Class2) |
| Max Sample Width | Up to 49in\[1245m\] |
| Machine Dimensions | Width: 54in\[1372mm\] Depth: 50.7in\[1288mm\] Height: 75in\[1905mm\] |
| Recirculation/Filtration Tank Capacity | 45gal\[170L\] |
| Safety Features | Interlock Hood Switch, Emergency Stop, 2 Hand Operation for Blade Movement(Open Door), Smart Cut™ |
| Compliance | CE Directives |

##### Consumables and Accessories

[![Abrasive Vises for Sectioning](https://www.buehler.com/ca/wp-content/uploads/sites/3/2023/08/vising-main-image.png)](https://www.buehler.com/ca/products/sectioning/accessories-consumables/abrasive-vises-for-sectioning/)

[Abrasive Vising](https://www.buehler.com/ca/products/sectioning/accessories-consumables/abrasive-vises-for-sectioning/)

Vising for Abrasive Saws and Cutters

[![Abrasive Blades for Sectioning](https://www.buehler.com/ca/wp-content/uploads/sites/3/2023/08/Premium-Abrasive-Blade_16in.png)](https://www.buehler.com/ca/products/sectioning/accessories-consumables/abrasive-blades-for-sectioning/)

[Abrasive Blades](https://www.buehler.com/ca/products/sectioning/accessories-consumables/abrasive-blades-for-sectioning/)

Abrasive Blades for Abrasive Saws

[![Cool 3 Coolants](https://www.buehler.com/ca/wp-content/uploads/sites/3/2023/08/Cool-3-Group-Photo.png)](https://www.buehler.com/ca/products/sectioning/accessories-consumables/coolants-for-sectioning/)

[Cool 3](https://www.buehler.com/ca/products/sectioning/accessories-consumables/coolants-for-sectioning/)

Coolants for Sectioning Machines

[![AbrasiMet L Pro Mist Extractor](https://www.buehler.com/ca/wp-content/uploads/sites/3/2023/08/AbrasiMet-L-Pro-Mist-Extractor.png)](https://shop.buehler.com/mist-extractor-for-abrasimet-xl-pro)

[Mist Extractor](https://shop.buehler.com/mist-extractor-for-abrasimet-xl-pro)

For AbrasiMet XL Pro

###### Related Products

[![AbrasiMet L Pro Automatic Abrasive Cutter](https://www.buehler.com/ca/wp-content/uploads/sites/3/2023/08/AbrasiMet-L-Pro-3qtrs.png)](https://www.buehler.com/ca/products/sectioning/abrasive-cutters/abrasimet-l-pro-automatic-abrasive-sectioning-saw/)

[AbrasiMet® L Pro](https://www.buehler.com/ca/products/sectioning/abrasive-cutters/abrasimet-l-pro-automatic-abrasive-sectioning-saw/)

14in \[356mm\] Automatic Abrasive Saw

[![AbrasiMatic 300 Abrasive Cutter](https://www.buehler.com/ca/wp-content/uploads/sites/3/2023/08/AbrasiMatic-300_600x600.jpg)](https://www.buehler.com/ca/products/sectioning/abrasive-cutters/abrasimatic-300-automatic-and-manual-abrasive-cutter/)

[AbrasiMatic® 300](https://www.buehler.com/ca/products/sectioning/abrasive-cutters/abrasimatic-300-automatic-and-manual-abrasive-cutter/)

12in \[305mm\] Automatic Abrasive Saw

[![AbrasiMet M Manual Abrasive Cutter](https://www.buehler.com/ca/wp-content/uploads/sites/3/2023/08/AbrasiMet-M-3qtrs-open.png)](https://www.buehler.com/ca/products/sectioning/abrasive-cutters/abrasimet-m-manual-abrasive-cutter/)

[AbrasiMet® M](https://www.buehler.com/ca/products/sectioning/abrasive-cutters/abrasimet-m-manual-abrasive-cutter/)

12in \[305mm\] Manual Abrasive Saw

[![IsoMet High Speed Pro](https://www.buehler.com/ca/wp-content/uploads/sites/3/2025/05/IsoMet-High-Speed-Pro_112800.jpg)](https://www.buehler.com/ca/products/sectioning/precision-cutters/isomet-high-speed-high-speed-pro/)

[IsoMet® High Speed Pro](https://www.buehler.com/ca/products/sectioning/precision-cutters/isomet-high-speed-high-speed-pro/)

8in \[203mm\] Automatic Precision Saw

Product Literature

[![AbrasiMet XL Pro Sell Sheet](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/07/English-AbrasiMet-XL-Pro-Sellsheet_06-28-2021.jpg)](https://www.buehler.com/assets/Brochures/English/Sectioning/AbrasiMet-XL_Sell_Sheet_EN.pdf)

[AbrasiMet XL Pro Sell Sheet](https://www.buehler.com/assets/Brochures/English/Sectioning/AbrasiMet-XL_Sell_Sheet_EN.pdf)

[![AbrasiMet XL Pro Brochure](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/06/AbrasiMet-XL-Pro-Brochure.jpg)](https://www.buehler.com/assets/Brochures/English/Sectioning/AbrasiMet-XL_Brochure-2-Small.pdf)

[AbrasiMet XL Pro Brochure](https://www.buehler.com/assets/Brochures/English/Sectioning/AbrasiMet-XL_Brochure-2-Small.pdf)

[![Buehler Product Catalog](https://www.buehler.com/ca/wp-content/uploads/sites/3/2023/08/Buehler-Product-Catalog_default_600x782.jpg)](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

[Buehler Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

Videos

![Full Lab Metallography Solutions](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Dr-Mike-Keeble.jpg)

Find Your Solutions

###### Full Lab Metallography Solutions

Looking for more information from us? Browse through our Solutions section to view technical articles, find recommended processing methods, look at industry solutions, and more.

[Solutions by Industry](https://www.buehler.com/ca/solutions/buehler-solutions/solutions-by-industry/)

[Solutions by Material](https://www.buehler.com/ca/solutions/buehler-solutions/methods-by-material/)

Need Additional Help?

Do you want to improve your process? Reach out for one-on-one help from our applications experts.

![Contact Buehler Lab Team](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Lab-Icon.png)

Contact Lab Team

[Contact Lab](https://www.buehler.com/ca/contact-lab-canada.php)

![Contact Buehler Customer Care](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Contact-Buehler.png)

Contact Customer Care

[Contact Us](https://www.buehler.com/ca/contact-us-canada.php)

###### Quick Links

Quickly access important info or visit our [E-Shop](https://shop.opti-tech.com/). Buehler is represented in Canada by Opti-tech Scientific

![Buehler Product Catalog](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Literature-Icon.png)

Product Catalog

View all Products in the Buehler Product Catalog

[Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

![Methods by Material](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/methods-by-material.png)

Methods by Material

Select a method by material

[Buehler Methods](https://www.buehler.com/ca/solutions/buehler-solutions/solutions-by-material/)

![Safety Data Sheets](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/SDS-Search.png)

SDS

Search Buehler's Safety Data Sheets

[Safety Data Sheets](https://www.buehler.com/ca/solutions/buehler-literature/safety-data-sheets/)

![Buehler Product Literature](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Buehler-Literature-Icon.png)

Product Literature

Browse and search Buehler's product literature

[Product Literature](https://www.buehler.com/ca/solutions/buehler-literature/product-literature/)