title: Epoxy Mounting Systems
url: https://www.buehler.com/ca/products/mounting/accessories-consumables/epoxy-mounting-systems/
date: 2021-09-29T18:24:11+00:00
modified: 2024-03-04T19:57:49+00:00
lang: en_CA
---

# Epoxy Mounting Systems

# Epoxy Mounting Systems

[![Epoxy Mounting Systems](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Epoxy-Mounting-Systems.png)Epoxy Mounting Systems](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Epoxy-Mounting-Systems.png)

[![Epoxy Mounting Systems](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/09/203432032-EpoxiCure2mounts.jpg)Epoxy Mounting](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/09/203432032-EpoxiCure2mounts.jpg)

## High Performance Choices

### Epoxy Mounting

The ideal solution for mounting specimens that are sensitive to high pressures and temperatures and require excellent pore infiltration. Choose our best-in-class epoxy solutions to improve the overall quality while reducing the curing time of your mounts. Combine with our SimpliVac™, vacuum mounting machine, to amplify pore penetration.

##### Excellent Pore Penetration and Infiltration

Choose Buehler’s epoxy media when pore penetration and sample quality are your top priorities. Easy-to-mix precise ratios make it a great choice in the lab.

##### Highest Quality Mounts with Fast Cure

Achieve the best mounting performance in your labs with Buehler’s EpoKwick® FC and EpoHeat® CLR. EpoHeat CLR cures in as little as 60 minutes with a curing oven, and EpoKwick FC cures only in 120 minutes at room temperature.

[Shop Now](https://shop.buehler.com/epoxy-systems)

#### EpoKwick® FC

![0012445_epokwick-fc-hardener-32oz095l](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/0012445_epokwick-fc-hardener-32oz095l.png)

EpoKwick FC is the fastest epoxy at room temperature while delivering the highest quality mounts. EpoKwick FC has only 2 hour cure time at room temperature, making it ideal for the technician.

[Shop Epoxy FC](https://shop.buehler.com/epoxy-systems#/specFilters=15m!#-!545)

#### EpoHeat® CLR

![0011650_epoheat-clr-resin-64oz-19l](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/0011650_epoheat-clr-resin-64oz-19l.png)

A game changer in delivering high quality mounts in fastest time. EpoHeat CLR helps you achieve maximum pore penetration within an hour in the oven.

[Shop EpoHeat CLR](https://shop.buehler.com/epoxy-systems#/specFilters=15m!#-!239)

#### EpoThin™ 2

![0011172_epothin-2-hardener-16oz-05l](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/0011172_epothin-2-hardener-16oz-05l.png)

EpoThin 2 protects your samples with its low cure temperature while providing good quality mounts.

[Shop EpoThin 2](https://shop.buehler.com/epoxy-systems#/specFilters=15m!#-!244)

#### EpoxiCure® 2

![0011184_epoxicure-2-hardener-16oz05l](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/0011184_epoxicure-2-hardener-16oz05l.png)

EpoxiCure 2 is a general purpose epoxy system that balances good hardness and low shrinkage.

[Shop EpoxiCure 2](https://shop.buehler.com/epoxy-systems#/specFilters=15m!#-!243)

### Epoxy Systems Selection Guide

Epoxy media is the preferred castable system when you need excellent infiltration in the most feasible cure time possible. Buehler offers a variety of products to meet your needs for speed, pore penetration, low curing temperature, and more.

|  | Material | Properties | Cure Time | Peak Exotherm | Shore D |
| --- | --- | --- | --- | --- | --- |
| General Purpose | EpoxiCure® 2 | General-purpose mount media with an excellent balance of good hardness and low shrinkage. | 6 hrs @ room temp | 104°F \[40°C\] | 80 |
| Specialty | EpoKwick® FC | Combines very low viscocity and extremely low shrinkage with good hardness and a fast cure. EpoKwick FC is the fastest Buehler epoxy without use of an oven. | 2 hrs @ room temp | 250°F \[121°C\] | 82 |
| EpoThin® 2 | Combines low viscosity and low cure temperature with strong adherence and good pore penetration | 9 hrs @ room temp | 149°F \[65°C\] | 78 |  |
| EpoHeat® CLR | When peak exotherm is not of concern, EpoHeat saves time when used in conjunction with an oven, providing strong sample infiltration for porous materials and materials with fine features | 1 hrs @ 149°F \[65°C\] | 324°F \[162°C\] | 82 |  |

| Selection Guide Notes |  |  |  |
| --- | --- | --- | --- |
| Values are compared to other Buehler medias and based on a one to three scale. Best values are ranked as a value of three. |  |  |  |
| Edge Retention | Viscocity / Infiltration | Shrinking | Recommended Use |
|  |  |  | For general applications, particularly when low viscosity isn’t required. Also ideal when using heat sensitive samples. |
|  |  |  | Aerospace coatings and other porous samples insensitive to heat. |
|  |  |  | For vacuum impregnation of intricate parts including heat sensitive materials such as electronic boards. |
|  |  |  | When processing large quantities of samples, large volume mounting, vacuum impregnation or applications which require a long pot life. |

##### Ordering

| Epoxy Mounting Systems |  |  |
| --- | --- | --- |
| EpoKwick FC |  |  |
| Component | Part Number | Size |
| Resin | [20-3453-128](https://shop.buehler.com/epokwick-fc-resin-128-oz-38l) | 128oz \[3.8L\] |
| Hardener | [20-3453-032](https://shop.buehler.com/epokwick-fc-hardener-32oz095l) | 32oz \[0.95L\] |

| EpoHeat CLR |  |  |
| --- | --- | --- |
| Component | Part Number | Size |
| Resin | [20-3423-064](https://shop.buehler.com/epoheat-clr-resin-64oz-19l) | 64oz \[1.9L\] |
| Hardener | [20-3424-016](https://shop.buehler.com/epoheat-clr-hardener-16oz-048l) | 16oz \[0.48L\] |

| EpoThin 2 |  |  |
| --- | --- | --- |
| Component | Part Number | Size |
| Resin | [20-3440-032](https://shop.buehler.com/epothin-2-resin-32oz095l) | 32oz \[0.95L\] |
| Resin | [20-3440-128](https://shop.buehler.com/epothin-2-resin-128oz38l) | 128oz \[3.8L\] |
| Hardener | [20-3442-016](https://shop.buehler.com/epothin-2-hardener-16oz05l) | 16oz \[0.48L\] |
| Hardener | [20-3442-064](https://shop.buehler.com/epothin-2-hardener-64oz19l) | 64oz \[1.9L\] |

| EpoxiCure 2 |  |  |
| --- | --- | --- |
| Component | Part Number | Size |
| Resin | [20-3430-064](https://shop.buehler.com/epoxicure-2-resin-64oz19l) | 64oz \[1.9L\] |
| Resin | [20-3430-128](https://shop.buehler.com/epoxicure-2-resin-128oz38l) | 128oz \[3.8L\] |
| Hardener | [20-3432-016](https://shop.buehler.com/epoxicure-2-hardener-16oz05l) | 16oz \[0.48L\] |
| Hardener | [20-3432-032](https://shop.buehler.com/epoxicure-2-hardener-32oz09l) | 32oz \[0.95L\] |

###### Epoxy Mounting Tips and Tricks

- Some epoxies can be cured more quickly by gently heating, which accelerates exothermic reactions. Use caution using excessive heat.
- When mixing, tilt the cup containing the resin and hardener slightly and gently work the resin and hardener together using a lift and stir motion.
- To get the best results, use a vacuum system to evacuate air from samples and pour under vacuum. This best fills gaps and pores in the specimen with epoxy. Cycling the vacuum greatly improves penetration of the sample.
- Epoxies are sensitive to the ratio of resin and hardener. Be sure to follow the recommended mixing ratio for each product. Measuring by mass is recommended, especially when mixing small quantities.
- Epoxy systems are sensitive to shelf life, which depends on proper storage. Keep out of excessive high or low temps and extreme humidity. It is good practice to date your containers when received.

##### Accessories

[![Mounting Accessories](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Castable-Molds.png)](https://www.buehler.com/ca/products/mounting/accessories-consumables/ring-forms-and-castable-molds-for-mounting/)

[Ring Forms & Castable Molds](https://www.buehler.com/ca/products/mounting/accessories-consumables/ring-forms-and-castable-molds-for-mounting/)

[![Support Clips Additives and Mixing Cups](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Cups-and-Additives.png)](https://www.buehler.com/ca/products/mounting/accessories-consumables/support-clips-additives-and-mixing-cups-for-mounting/)

[Support Clips, Additives, and Mixing Cups](https://www.buehler.com/ca/products/mounting/accessories-consumables/support-clips-additives-and-mixing-cups-for-mounting/)

[![Release Agents and Powders](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Release-Agent.png)](https://www.buehler.com/ca/products/mounting/accessories-consumables/mount-and-mold-release-agents/)

[Release Agents and Powders](https://www.buehler.com/ca/products/mounting/accessories-consumables/mount-and-mold-release-agents/)

##### Related Consumables

[![Acrylic Mounting System](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Acrylic-Mounting-System.png)](https://www.buehler.com/ca/products/mounting/accessories-consumables/acrylic-mounting-systems/)

[Acrylic Mounting Systems](https://www.buehler.com/ca/products/mounting/accessories-consumables/acrylic-mounting-systems/)

[![Hot Compression Mounting](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Hot-Compression-Mounting-Image.png)](https://www.buehler.com/ca/products/mounting/accessories-consumables/compression-mounting-powder-and-pre-molds/)

[Compression Mounting System](https://www.buehler.com/ca/products/mounting/accessories-consumables/compression-mounting-powder-and-pre-molds/)

##### Product Literature

[![Epoxy Mounting Guide](https://www.buehler.com/ca/wp-content/uploads/sites/3/2023/02/Epoxy-Mounting-Guide.jpg)](https://www.buehler.com/assets/Brochures/English/Mounting/Epoxy_Mounting_Guide_Web.pdf)

[Epoxy Mounting Guide](https://www.buehler.com/assets/Brochures/English/Mounting/Epoxy_Mounting_Guide_Web.pdf)

[![Buehler Product Catalog](https://www.buehler.com/ca/wp-content/uploads/sites/3/2023/08/Buehler-Product-Catalog_default_600x782.jpg)](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

[Buehler Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

###### Frequently Asked Questions

#### When do you recommend castable mounting systems over compression mounting systems?

Castable mounting systems are recommended for mounting specimens that are sensitive to heat and/or pressure. Learn more about how to choose the right [mounting media](https://www.buehler.com/ca/choose-the-right-mounting-media/) for your needs.

#### When would someone prefer Epoxy Mounting Systems over Acrylics Systems?

Epoxy media is preferred when you need excellent infiltration and minimal shrinkage gaps, and when pore penetration is critical. Please visit our [acrylic](https://www.buehler.com/assets/Brochures/English/Mounting/Acrylic_Mounting_Guide_Web.pdf) and [epoxy](https://www.buehler.com/assets/Brochures/English/Mounting/Epoxy_Mounting_Guide_Web.pdf) mounting guides for more information.

#### Do I need to use a vacuum system with Epoxy Systems?

You can use our [SimpliVac®](https://www.buehler.com/ca/products/mounting/castable-mounting/simplivac-vacuum-mounting-system/) to enhance edge retention and epoxy penetration in your process. Explore more here.

![Full Lab Metallography Solutions](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Dr-Mike-Keeble.jpg)

Find Your Solutions

###### Full Lab Metallography Solutions

Looking for more information from us? Browse through our Solutions section to view technical articles, find recommended processing methods, look at industry solutions, and more.

[Solutions by Industry](https://www.buehler.com/ca/solutions/buehler-solutions/solutions-by-industry/)

[Solutions by Material](https://www.buehler.com/ca/solutions/buehler-solutions/methods-by-material/)

Need Additional Help?

Do you want to improve your process? Reach out for one-on-one help from our applications experts.

![Contact Buehler Lab Team](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Lab-Icon.png)

Contact Lab Team

[Contact Lab](https://www.buehler.com/ca/contact-lab-canada.php)

![Contact Buehler Customer Care](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Contact-Buehler.png)

Contact Customer Care

[Contact Us](https://www.buehler.com/ca/contact-us-canada.php)

###### Quick Links

Quickly access important info or visit our [E-Shop](https://shop.opti-tech.com/). Buehler is represented in Canada by Opti-tech Scientific

![Buehler Product Catalog](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Literature-Icon.png)

Product Catalog

View all Products in the Buehler Product Catalog

[Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

![Methods by Material](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/methods-by-material.png)

Methods by Material

Select a method by material

[Buehler Methods](https://www.buehler.com/ca/solutions/buehler-solutions/solutions-by-material/)

![Safety Data Sheets](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/SDS-Search.png)

SDS

Search Buehler's Safety Data Sheets

[Safety Data Sheets](https://www.buehler.com/ca/solutions/buehler-literature/safety-data-sheets/)

![Buehler Product Literature](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Buehler-Literature-Icon.png)

Product Literature

Browse and search Buehler's product literature

[Product Literature](https://www.buehler.com/ca/solutions/buehler-literature/product-literature/)