title: Hardness Testing Legacy Testers
url: https://www.buehler.com/ca/products/hardness-testing/hardness-testing-legacy-testers/
date: 2021-10-21T16:55:17+00:00
modified: 2024-11-20T17:37:14+00:00
lang: en_CA
---

# Hardness Legacy Testers

![Wilson Rockwell 4JR Legacy Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Wilson-Rockwell-4JR.png)

*Wilson Rockwell Legacy Hardness Tester*

![Wolpert Digitester UH930 Hardness Legacy Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Wolpert-UH930.png)

*Wolpert Hardness Legacy Tester*

![Wilson Legacy UH250](https://www.buehler.com/ca/wp-content/uploads/sites/3/2022/03/Legacy_UH-250.png)

*Reicherter Legacy Hardness Tester*

![Precidur Legacy Hardness Testing Software](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Precidur.png)

*Precidur Legacy Hardness Testing Software*

## Legacy Hardness Testers

Since 1936, Buehler has been at the forefront of materials preparation and hardness testing, building on a foundation of legacy machines trusted by industries worldwide. For over a century, Reicherter, Wolpert, and Wilson have pioneered groundbreaking hardness testers, setting the benchmark for quality and precision. Today, Buehler honors their legacy, continuing to innovate and meet the growing demands of modern manufacturing. For service inquiries, please contact our [service team](https://www.buehler.com/ca/service-request_ca.php).

![Wilson Hardness Legacy Logo](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Wilson-Logo.png)

[Wilson](#wilson)

![Wolpert Hardness Legacy Testers](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Wolpert-logo_blue.png)

[Wolpert](#wolpert)

![Reicherter Hardness Legacy Testers](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Reicherter_1912-logo_black.png)

[Reicherter](#reicherter)

![Precidur Legacy Hardness Testers](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Precidur-logo.png)

[Precidur](#precidur)

#### Wilson Hardness Legacy Testers

The Wilson® hardness brand of hardness testers was originally known as the Wilson Mechanical Instrument Company. Here Stanley Rockwell and founder Charles H. Wilson introduced the Rockwell hardness tester, an industry standard. Later, Wilson became the home of the legendary Tukon line of micro-indentation testers – renowned for Knoop and Vickers testing. These early inventions revolutionized industry and paved the way for Wilson today, with innovations that improve usability and allow for full connectivity and automation like the DiaMet software. [Contact our service team](https://www.buehler.com/ca/service-request_ca.php) for any questions about legacy testers, or you can view our [Legacy Tester program](https://www.buehler.com/assets/Brochures/English/Hardness/Legacy_Tester_Sell_Sheet.pdf) flyer.

##### Rockwell 4JR (+/- 1945 - 1960)

![Wilson Rockwell 4JR Legacy Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Wilson-Rockwell-4JR.png)

- Analog Rockwell Hardness Tester
- Scales: HRA, HRB, HRC, etc
- Rockwell: 60, 100 and 150 kgf
- Today’s Tester: Rockwell® 574 & 2150

##### Rockwell 504R (+/- 1960 - 2000)

![Wilson Rockwell 504R Hardness Legacy Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Wilson-Rockwell-504R.png)

- Analog Rockwell Hardness Tester
- Regular Scales: HRA, HRB, HRC
- Superficial Scales: HR15N, HR30T
- Rockwell: 10, 30, 45, 60, 100 and 150 kgf
- Today’s Tester: Rockwell 574 & 2150

##### Rockwell 524T (+/- 1970 - 2005)

![Wilson Rockwell 524T Hardness Legacy Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Wilson-Rockwell-524T.png)

- Digital read-out Rockwell Hardness Tester
- Regular Scales: HRA, HRB, HRC, etc
- Superficial Scales: HR15N, HR30T, etc
- Rockwell: 10, 30, 45, 60, 100 and 150 kgf
- Today’s Tester: Rockwell 574 & 2150

#### Wolpert Hardness Legacy Testers

Wolpert, a well-known name in the hardness testing industry, is known for the practical designs which meet the needs of every hardness testing application. Wolpert has been manufacturing hardness testers since 1927.

##### DigiTestor UH930 (+/-1990 - 2015)

![Wolpert Digitester UH930 Hardness Legacy Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Wolpert-UH930.png)

- First closed-loop universal tester on the market
- Universal Hardness Tester 1-250 kgf
- With Integrated optics
- For Vickers, Brinell and (Super-) Rockwell

##### DiaTronic (+/- 1980 - 1990)

![Wolpert DiaTronic Hardness Legacy Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Wolpert-DiaTronic.png)

- Universal Hardness Tester 1-250 kgf
- With Integrated optics
- Vickers: (1-2-3) 5-10-20-30-40-50
- Brinell: 15.625-31.25-62.5-125-187.5-250
- Rockwell: 60, 100 and 150 kgf

##### HT 8004 (+/- 1975 - 1985)

![Wolpert HT 8004 Legacy Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Wolpert-HT-8004.png)

- Rockwell Hardness Tester
- Digital or Analog Display
- Scales: HRA, HRB, HRC, etc
- Rockwell: 15, 20, 45, 80, 100, 187.5 and 250 kg
- Today’s Testers: R574 & R2150

##### DiaTestor 3a & 3b (+/- 1965 - 1958)

![Wolpert DiaTestor 3a & 3b Legacy Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Wolpert-DiaTestor-3a-y-3b.png)

- Brinell Hardness Tester
- Scales: HB10/3000, HB10/1000, HB5/750
- Brinell: 120, 187.5, 250, 500, 750, 1000, 1500 and 3000 kgf
- Integrated optics
- For heavy castings and forgings
- Optional motorized spindle
- Today’s Tester: BH3000

##### DiaTestor 2RC (+/- 1949 - 1975)

![Wolpert DiaTestor 2RC Hardness Legacy Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Wolpert-DiaTestor-2RC.png)

- Universal Hardness Tester 1-250 kgf
- Vickers: (1-2-3) 5-10-20-30-40-50
- Brinell: 15.625-31.25-62,5-125-187.5-250
- Rockwell: 60, 100 and 150 kgf
- Integrated optics

##### V-Testor 2 (+/- 1985 - 1991)

![Wolpert V Testor 2 Legacy Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Wolpert-V-Testor-2.png)

- Vickers Hardness Tester
- Vickers & Knoop
- Eyepiece
- Objective
- Manual Spindle
- Oildamper for load control
- Today’s Tester: VH1202, VH1150, VH3100 & VH3300

#### Reicherter Hardness Legacy Testers

Reicherter produced Vickers, Rockwell, Brinell and Universal hardness testers that were known globally and manufactured in Germany with sturdy machine construction, maximized testing accuracy and ease of use and maintenance. They were used to test crankshafts, camshafts, engine blocks and other large workpieces. They were some of the earliest testers to be integrated into high throughput production lines of larger and heavier test pieces.

##### UH250 Universal Hardness Tester (+/- 2005)

![Wilson Legacy UH250](https://www.buehler.com/ca/wp-content/uploads/sites/3/2022/03/Legacy_UH-250.png)

- Universal Hardness Tester 1-250 kgf
- Vickers: (1-2-3) 5-10-20-30-40-50
- Brinell: 15.625-31.25-62.5-125-187.5-250
- Rockwell: 60, 100 and 150 kgf

##### BRIRO Automat HE1

![BRIRO Automat HE1 Legacy Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/BRIRO-Automat-HE1.png)

- Rockwell, Rockwell Superficial and Brinell HBT Hardness Tester
- Low-mass spring load
- Automatic test sequence

##### Briro BEV

![BRIRO BEV Legacy Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/BRIRO-BEV.png)

- Universal Hardness Testers, depth measurement
- BRIVISKOP: Vickers and Brinell
- BRIRO: Rockwell

##### BRIRO VA

![BRIRO VA Legacy Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/BRIRO-VA.png)

- Rockwell Hardness Tester
- Original Reicherter Clamping
- 50 – 100 kgf, 62.5 – 187.5 kgf, 100 – 250 kgf
- Today’s Tester: Rockwell® 574 & 2150

##### BRIVISOR KL2 - KL3

![BRIVISOR KL2 KL3 Legacy Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/BRIVISOR_KL2-KL3.png)

- Vickers & Knoop Hardness Tester
- Microscope with interchangeable lenses
- Low-mass spring load
- Today’s Tester: VH1202 & VH3100

##### BRIRO BEH & BRIVISKOP 3000

![BRIRO BEH Legacy Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/BRIRO-BEH.png)

- Universal Hardness Tester, depth measurement
- BRIVISKOP: Vickers & Brinell
- BRIRO: Rockwell

##### BRIRO E

![BRIRO E Legacy Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/BRIRO-E.png)

- Rockwell Hardness Tester
- Simple test procedures
- Today’s Tester: VH3100

##### BRIRO VA AUTOMAT

![BRIRO VA Automat Legacy Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/BRIRO-VA-Automat.png)

- Automatic Rockwell Hardness Tester
- Original Reicherter Clamping
- 50-100 kgf, 62.5-187.5 kgf, 100-250 kgf

##### BRIRO VA

![BRIRO VA Legacy Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/BRIRO-VA.png)

- Universal Hardness Tester
- Brinell and Vickers
- Spring Loaded

##### KL4

![Reicherter KL4 Legacy Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Reicherter-KL4.jpg)

- Fullautomatic Vickers Tester
- Loadrange 0.05 – 10kgf
- WinControl Software
- Can be upgraded with DiaMet software (only digital KL4)
- Current tester: VH3100

##### BRIRO R

![Reicherter Briro R Legacy Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Reicherter-Briro-R.jpg)

- Heavy duty Rockwell tester
- Springload force application
- Original Reicherter clamping
- Current tester: R574

##### Wilson UH250 Universal Hardness Tester (2010-2018)

![Wilson UH250 Legacy Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/UH250.png)

- Closed loop Universal Hardness Tester 1-250kgf
- Vickers, Brinell, Rockwell
- Operated with WinControl and DiaMet software
- Reicherter Clamping Device

#### PRECIDUR Hardness Testing Software

![Precidur Legacy Hardness Testing Software](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/11/Precidur.png)

In 2008, Buehler’s product portfolio was expanded to include PRECIDUR, a state of the art hardness testing software system complementing the Wilson Hardness product line with its renowned flexibility and automatic Vickers/Knoop measurement capabilities. PRECIDUR was developed in Germany by Fritz Müller GmbH in the early 1990s and was used on many micro-hardness testers from various manufacturers. It allowed users to control micro-hardness testers via computer and used a camera for automatic indent measurements. Its programming features enabled full-automatic patterning. For service inquiries or support, please contact our service department.

![Full Lab Metallography Solutions](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Dr-Mike-Keeble.jpg)

Find Your Solutions

###### Full Lab Metallography Solutions

Looking for more information from us? Browse through our Solutions section to view technical articles, find recommended processing methods, look at industry solutions, and more.

[Solutions by Industry](https://www.buehler.com/ca/solutions/buehler-solutions/solutions-by-industry/)

[Solutions by Material](https://www.buehler.com/ca/solutions/buehler-solutions/methods-by-material/)

Need Additional Help?

Do you want to improve your process? Reach out for one-on-one help from our applications experts.

![Contact Buehler Lab Team](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Lab-Icon.png)

Contact Lab Team

[Contact Lab](https://www.buehler.com/ca/contact-lab-canada.php)

![Contact Buehler Customer Care](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Contact-Buehler.png)

Contact Customer Care

[Contact Us](https://www.buehler.com/ca/contact-us-canada.php)

###### Quick Links

Quickly access important info or visit our [E-Shop](https://shop.opti-tech.com/). Buehler is represented in Canada by Opti-tech Scientific

![Buehler Product Catalog](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Literature-Icon.png)

Product Catalog

View all Products in the Buehler Product Catalog

[Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

![Methods by Material](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/methods-by-material.png)

Methods by Material

Select a method by material

[Buehler Methods](https://www.buehler.com/ca/solutions/buehler-solutions/solutions-by-material/)

![Safety Data Sheets](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/SDS-Search.png)

SDS

Search Buehler's Safety Data Sheets

[Safety Data Sheets](https://www.buehler.com/ca/solutions/buehler-literature/safety-data-sheets/)

![Buehler Product Literature](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Buehler-Literature-Icon.png)

Product Literature

Browse and search Buehler's product literature