title: Wilson Rockwell Test Blocks
url: https://www.buehler.com/ca/products/hardness-testing/hardness-testing-blocks/wilson-rockwell-test-blocks/
date: 2021-10-18T21:00:54+00:00
modified: 2022-05-12T14:00:46+00:00
lang: en_CA
---

# Wilson Rockwell Test Blocks

Wilson Rockwell Test Blocks

Wilson Rockwell hardness test blocks set the standard for the industry and are made from the highest quality material to insure the most uniform and repeatable Rockwell test blocks available. A comprehensive variety of scales and hardness test blocks are available to meet the wide ranges and hardness scales associated with Rockwell®, Brinell, Knoop and Vickers testing. All Wilson Rockwell hardness test blocks are calibrated in the Wilson Hardness Calibration Laboratory in Binghamton, NY. The Wilson lab is accredited to ISO/IEC 17025 by A2LA and the testers used in the calibration process undergo a stringent monitoring process using NIST traceable devices.

For the ultimate accuracy and performance in tester verification, calibration sets are available for most Rockwell scales.

100% inspection to ensure that every single Rockwell test block meets the physical requirements of ASTM (thickness, flatness, parallelism, surface roughness)

Benefits

Specifications

Ordering

Benefits

- We work directly with the steel and brass mills to specify the chemical composition.
- Our machining processes (grinding, lapping, polishing) are all done in house, at the site of calibration.
- 100% inspection to ensure that every single test block meets the physical requirements of ASTM (thickness, flatness, parallelism, surface roughness).
- Rockwell test blocks support NADCAP compliance

Specifications

| Wilson Rockwell Hardness Test Blocks Specifications |  |
| --- | --- |
| Block size: | Ø 2.4 in x 0.35 in (Ø 60mm x 9mm) |
| Block weight: | ±0.66 lbs (± 0.3kg) |
| Certification: | According to ISO 6508-3 & ASTM E18 |
| The Buehler-Wilson Hardness Calibration Laboratory is accredited to ISO / IEC 17025 by A2LA |  |

Ordering

| HRA Scale |  |  |  |  |  |
| --- | --- | --- | --- | --- | --- |
| Certified with Diamond Brale Indenter |  |  |  |  |  |
| Part Number | Hardness Value | Scale | Min | Max | Quick Ship |
| [9201-050](https://shop.buehler.com/31hra-rockwell-test-block) | 31 | HRA | 28 | 32 |  |
| [9201-060](https://shop.buehler.com/35hra-rockwell-test-block) | 35 | HRA | 33 | 37 |  |
| [9201-080](https://shop.buehler.com/44hra-rockwell-test-block) | 44 | HRA | 42 | 46 |  |
| [9201-090](https://shop.buehler.com/50hra-rockwell-test-block) | 50 | HRA | 47 | 51 |  |
| [9201-100](https://shop.buehler.com/58hra-rockwell-test-block) | 58 | HRA | 56 | 61 |  |
| [9201-110](https://shop.buehler.com/tst-bk-hra-63-wilson-cert) | 63 | HRA | 61 | 65 |  |
| [9201-120](https://shop.buehler.com/65hra-rockwell-test-block) | 65 | HRA | 63 | 67 |  |
| [9201-130](https://shop.buehler.com/68hra-rockwell-test-block) | 68 | HRA | 66 | 70 |  |
| [9201-140](https://shop.buehler.com/70hra-rockwell-test-block) | 70 | HRA | 68 | 72 |  |
| [9201-150](https://shop.buehler.com/tst-bk-hra-73-wilson-cert) | 73 | HRA | 71 | 75 |  |
| [9201-160](https://shop.buehler.com/76hra-rockwell-test-block) | 76 | HRA | 74 | 78 |  |
| [9201-180](https://shop.buehler.com/81hra-rockwell-test-block) | 81 | HRA | 79 | 83 |  |
| [9201-190](https://shop.buehler.com/tst-bk-hra-83-wilson-cert) | 83 | HRA | 81 | 85 |  |
| [9201-200](https://shop.buehler.com/84hra-rockwell-test-block) | 84 | HRA | 82 | 86 |  |
| [9201-210](https://shop.buehler.com/87hra-rockwell-test-block) | 87 | HRA | 85 | 89 |  |

| HRA Scale |  |  |  |  |  |
| --- | --- | --- | --- | --- | --- |
| Certified with Diamond Brale Indenter (for Carbide testing) |  |  |  |  |  |
| Part Number | Hardness Value | Scale | Min | Max | Quick Ship |
| [900990185](https://shop.buehler.com/85hra-rockwell-test-block-carbide) | 85 | HRA | 84 | 86 |  |
| [900990187](https://shop.buehler.com/87hra-rockwell-test-block-carbide) | 87 | HRA | 86 | 88 |  |
| [900990189](https://shop.buehler.com/89hra-rockwell-test-block-carbide) | 89 | HRA | 88 | 90 |  |
| [900990191](https://shop.buehler.com/91hra-rockwell-test-block-carbide) | 91 | HRA | 90 | 91 |  |
| [900990192](https://shop.buehler.com/92hra-rockwell-test-block-carbide) | 92 | HRA | 91 | 92 |  |
| [900990193](https://www.buehler.com/buehler-request-a-quote.php) | 93 | HRA | 92 | 93 |  |

| HRB Scale |  |  |  |  |  |
| --- | --- | --- | --- | --- | --- |
| Certified with Tungsten Carbide Ball Indenter |  |  |  |  |  |
| Part Number | Hardness Value | Scale | Min | Max | Quick Ship |
| [9202-030W](https://shop.buehler.com/20hrb-rockwell-test-block-carbide) | 20 | HRB(W) | 15 | 25 |  |
| [9202-040W](https://shop.buehler.com/30hrb-rockwell-test-block-carbide) | 30 | HRB(W) | 25 | 35 |  |
| [9202-050W](https://shop.buehler.com/tst-bk-40-hrb-crbd-ball-cal-w) | 40 | HRB(W) | 35 | 45 |  |
| [9202-060W](https://shop.buehler.com/tst-bk-50-hrbcrbd-ball-cal-w) | 50 | HRB(W) | 45 | 55 |  |
| [9202-070W](https://shop.buehler.com/tst-bk-60-hrb-crbd-ball-cal-w) | 60 | HRB(W) | 55 | 65 |  |
| [9202-080W](https://shop.buehler.com/tst-bk-70hrb-crbd-ball-cal-w) | 70 | HRB(W) | 65 | 75 |  |
| [9202-090W](https://shop.buehler.com/tst-bk-80hrb-crbd-ball-cal-w) | 80 | HRB(W) | 75 | 85 |  |
| [9202-100W](https://shop.buehler.com/tst-bk-95-hrb-crbd-ball-cal-w) | 95 | HRB(W) | 85 | 99 |  |

| HRB Scale |  |  |  |  |  |
| --- | --- | --- | --- | --- | --- |
| Certified with Steel Ball Indenter |  |  |  |  |  |
| Part Number | Hardness Value | Scale | Min | Max | Quick Ship |
| [9202-060](https://shop.buehler.com/tst-bk-50-hrbcrbd-ball-cal-w) | 50 | HRB(S) | 45 | 55 |  |
| [9202-070](https://shop.buehler.com/tst-bk-60-hrb-crbd-ball-cal-w) | 60 | HRB(S) | 55 | 65 |  |
| [9202-080](https://shop.buehler.com/tst-bk-70hrb-crbd-ball-cal-w) | 70 | HRB(S) | 65 | 75 |  |
| [9202-090](https://shop.buehler.com/tst-bk-80hrb-crbd-ball-cal-w) | 80 | HRB(S) | 75 | 85 |  |
| [9202-100](https://shop.buehler.com/tst-bk-95-hrb-crbd-ball-cal-w) | 90 | HRB(S) | 85 | 95 |  |

| HRC Scale |  |  |  |  |  |
| --- | --- | --- | --- | --- | --- |
| Certified with Diamond Brale Indenter |  |  |  |  |  |
| Part Number | Hardness Value | Scale | Min | Max | Quick Ship |
| [9203-111](https://shop.buehler.com/tst-bk-hrc-25-nist-scale) | 25 | HRC | 22.5 | 27.5 |  |
| [9203-121](https://shop.buehler.com/tst-bk-hrc-30-nist-scale) | 30 | HRC | 27.5 | 32.5 |  |
| [9203-131](https://shop.buehler.com/tst-bk-hrc-35-nist-scale) | 35 | HRC | 32.5 | 37.5 |  |
| [9203-141](https://shop.buehler.com/tst-bk-hrc-40-nist-scale) | 40 | HRC | 37.5 | 42.5 |  |
| [9203-151](https://shop.buehler.com/tst-bk-hrc-45-nist-scale) | 45 | HRC | 42.5 | 47.5 |  |
| [9203-161](https://shop.buehler.com/tst-bk-hrc-50-nist-scale) | 50 | HRC | 47.5 | 52.5 |  |
| [9203-171](https://shop.buehler.com/tst-bk-hrc-55-nist-scale) | 55 | HRC | 52.5 | 57.5 |  |
| [9203-181](https://shop.buehler.com/tst-bk-hrc-60-nist-scale) | 60 | HRC | 57.5 | 62 |  |
| [9203-191](https://shop.buehler.com/tst-bk-hrc-63nist-scale) | 63 | HRC | 62.1 | 64.6 |  |
| [9203-201](https://shop.buehler.com/65hrc-rockwell-test-block-steel) | 65 | HRC | 64.6 | 68 |  |
| [9203-211](https://shop.buehler.com/70hrc-rockwell-test-block) | 70 | HRC | 68 | 80 |  |

| HRE Scale |  |  |  |  |  |
| --- | --- | --- | --- | --- | --- |
| Certified with Tungsten Carbide Ball Indenter |  |  |  |  |  |
| Part Number | Hardness Value | Scale | Min | Max | Quick Ship |
| [9205-010W](https://shop.buehler.com/57hre-rockwell-test-block-carbide) | 57 | HRE | 54 | 61 |  |
| [9205-020W](https://shop.buehler.com/63hre-rockwell-test-block-carbide) | 63 | HRE | 59 | 65 |  |
| [9205-030W](https://shop.buehler.com/69hre-rockwell-test-block-carbide) | 69 | HRE | 65 | 71 |  |
| [9205-040W](https://shop.buehler.com/75hre-rockwell-test-block-carbide) | 75 | HRE | 72 | 78 |  |
| [9205-050W](https://shop.buehler.com/tst-bk-81-hre-crbd-ball-cal-w) | 81 | HRE | 78 | 84 |  |
| [9205-060W](https://shop.buehler.com/tst-bk-87hre-crbd-ball-cal-w) | 87 | HRE | 84 | 90 |  |
| [9205-070W](https://shop.buehler.com/tst-bk-93-hre-crbd-ball-cal-w) | 93 | HRE | 90 | 96 |  |
| [9205-080W](https://shop.buehler.com/99hre-rockwell-test-block-carbide) | 99 | HRE | 96 | 102 |  |

| HRF Scale |  |  |  |  |  |
| --- | --- | --- | --- | --- | --- |
| Certified with Tungsten Carbide Ball Indenter |  |  |  |  |  |
| Part Number | Hardness Value | Scale | Min | Max | Quick Ship |
| [9206-010W](https://shop.buehler.com/57hrf-rockwell-test-block-carbide) | 57 | HRF | 54 | 60 |  |
| [9206-020W](https://shop.buehler.com/tst-bk-63-hrf-crbd-ball-cal-w) | 63 | HRF | 60 | 66 |  |
| [9206-030W](https://shop.buehler.com/69hrf-rockwell-test-block-carbide) | 69 | HRF | 65 | 71 |  |
| [9206-040W](https://shop.buehler.com/74hrf-rockwell-test-block-carbide) | 74 | HRF | 71 | 77 |  |
| [9206-050W](https://shop.buehler.com/tst-bk-795hrf-crbd-ball-cal-w) | 80 | HRF | 76 | 82 |  |
| [9206-060W](https://shop.buehler.com/86hrf-rockwell-test-block-carbide) | 86 | HRF | 82 | 88 |  |
| [9206-070W](https://shop.buehler.com/tst-bk-91hrf-crbd-ball-cal-w) | 91 | HRF | 88 | 94 |  |
| [9206-080W](https://shop.buehler.com/97hrf-rockwell-test-block-carbide) | 97 | HRF | 94 | 100 |  |

| HRR Scale |  |  |  |  |  |
| --- | --- | --- | --- | --- | --- |
| Certified with Tungsten Carbide Ball Indenter |  |  |  |  |  |
| Part Number | Hardness Value | Scale | Min | Max | Quick Ship |
| [9216-020W](https://shop.buehler.com/114hrr-rockwell-test-block-carbide) | 114 | HRR | 104 | 124 |  |

| HR15N Scale |  |  |  |  |  |
| --- | --- | --- | --- | --- | --- |
| Certified with Diamond Brale Indenter |  |  |  |  |  |
| Part Number | Hardness Value | Scale | Min | Max | Quick Ship |
| [9212-110](https://shop.buehler.com/tst-bk-72-hr15n-astm) | 72 | HR15N | 70 | 74 |  |
| [9212-120](https://shop.buehler.com/75hr15n-superficial-rockwell-test-block) | 75 | HR15N | 73 | 77 |  |
| [9212-130](https://shop.buehler.com/tst-bk-78-hr15n-astm) | 78 | HR15N | 76 | 80 |  |
| [9212-140](https://shop.buehler.com/80hr15n-superficial-rockwell-test-block) | 80 | HR15N | 78 | 82 |  |
| [9212-150](https://shop.buehler.com/tst-bk-83-hr15n-astm) | 83 | HR15N | 81 | 85 |  |
| [9212-160](https://shop.buehler.com/86hr15n-superficial-rockwell-test-block) | 86 | HR15N | 84 | 88 |  |
| [9212-170](https://shop.buehler.com/88hr15n-superficial-rockwell-test-block) | 88 | HR15N | 86 | 90 |  |
| [9212-180](https://shop.buehler.com/90hr15n-superficial-rockwell-test-block) | 90 | HR15N | 88 | 92 |  |
| [9212-190](https://shop.buehler.com/tst-bk-91-hr15n-astm) | 91 | HR15N | 89 | 93 |  |
| [9212-200](https://shop.buehler.com/92hr15n-superficial-rockwell-test-block) | 92 | HR15N | 90 | 94 |  |
| [9212-210](https://shop.buehler.com/94hr15n-superficial-rockwell-test-block) | 94 | HR15N | 92 | 96 |  |

| HR45N Scale |  |  |  |  |  |
| --- | --- | --- | --- | --- | --- |
| Certified with Diamond Brale Indenter |  |  |  |  |  |
| Part Number | Hardness Value | Scale | Min | Max | Quick Ship |
| [9214-110](https://shop.buehler.com/25hr45n-superficial-rockwell-test-block) | 25 | HR45N | 22 | 28 |  |
| [9214-120](https://shop.buehler.com/31hr45n-superficial-rockwell-test-block) | 31 | HR45N | 28 | 34 |  |
| [9214-130](https://shop.buehler.com/37hr45n-superficial-rockwell-test-block) | 37 | HR45N | 34 | 40 |  |
| [9214-140](https://shop.buehler.com/43hr45n-superficial-rockwell-test-block) | 43 | HR45N | 40 | 46 |  |
| [9214-150](https://shop.buehler.com/49hr45n-superficial-rockwell-test-block) | 49 | HR45N | 46 | 52 |  |
| [9214-160](https://shop.buehler.com/55hr45n-superficial-rockwell-test-block) | 55 | HR45N | 52 | 58 |  |
| [9214-170](https://shop.buehler.com/61hr45n-superficial-rockwell-test-block) | 61 | HR45N | 58 | 64 |  |
| [9214-180](https://shop.buehler.com/67hr45n-superficial-rockwell-test-block) | 67 | HR45N | 64 | 70 |  |
| [9214-190](https://shop.buehler.com/70hr45n-superficial-rockwell-test-block) | 70 | HR45N | 68 | 72 |  |
| [9214-210](https://shop.buehler.com/78hr45n-superficial-rockwell-test-block) | 78 | HR45N | 73 | 78 |  |

| HR15T Scale |  |  |  |  |  |
| --- | --- | --- | --- | --- | --- |
| Certified with Tungsten Carbide Ball Indenter |  |  |  |  |  |
| Part Number | Hardness Value | Scale | Min | Max | Quick Ship |
| [9218-020W](https://shop.buehler.com/tst-bk-64hr15t-crbd-ball-cal-w) | 64 | HR15T | 62 | 66 |  |
| [9218-030W](https://shop.buehler.com/67hr15t-superficial-rockwell-test-block) | 67 | HR15T | 65 | 69 |  |
| [9218-040W](https://shop.buehler.com/71hr15t-superficial-rockwell-test-block) | 71 | HR15T | 68 | 72 |  |
| [9218-050W](https://shop.buehler.com/tst-bk-735-hr15t-crbd) | 74 | HR15T | 71 | 75 |  |
| [9218-060W](https://shop.buehler.com/77hr15t-superficial-rockwell-test-block) | 77 | HR15T | 75 | 79 |  |
| [9218-070W](https://shop.buehler.com/tst-bk-80hr15t-crbd-ball-cal-w) | 80 | HR15T | 78 | 82 |  |
| [9218-080W](https://shop.buehler.com/hr15t-superficial-rockwell-test-block) | 84 | HR15T | 81 | 85 |  |
| [9218-090W](https://shop.buehler.com/87hr15t-superficial-rockwell-test-block) | 87 | HR15T | 84 | 88 |  |
| [9218-100W](https://shop.buehler.com/92hr15t-superficial-rockwell-test-block) | 92 | HR15T | 89 | 93 |  |

| HR30T Scale |  |  |  |  |  |
| --- | --- | --- | --- | --- | --- |
| Certified with Tungsten Carbide Ball Indenter |  |  |  |  |  |
| Part Number | Hardness Value | Scale | Min | Max | Quick Ship |
| [9219-030W](https://shop.buehler.com/29hr30t-superficial-rockwell-test-block-carbide) | 29 | HR30T | 25 | 31 |  |
| [9219-040W](https://shop.buehler.com/36hr30t-superficial-rockwell-test-block-carbide) | 36 | HR30T | 33 | 39 |  |
| [9219-050W](https://shop.buehler.com/tst-bk-43hr30t-crbd-ball-cal-w) | 43 | HR30T | 40 | 46 |  |
| [9219-060W](https://shop.buehler.com/50hr30t-superficial-rockwell-test-block-carbide) | 50 | HR30T | 46 | 52 |  |
| [9219-070W](https://shop.buehler.com/tst-bk-56hr30t-crbd-ball-cal-w) | 56 | HR30T | 53 | 59 |  |
| [9219-080W](https://shop.buehler.com/63hr30t-superficial-rockwell-test-block-carbide) | 63 | HR30T | 59 | 65 |  |
| [9219-090W](https://shop.buehler.com/tst-bk-70hr30t-crbd-ball-cal-w) | 70 | HR30T | 67 | 73 |  |
| [9219-100W](https://shop.buehler.com/80hr30t-superficial-rockwell-test-block-carbide) | 80 | HR30T | 77 | 83 |  |

| HR45T Scale |  |  |  |  |  |
| --- | --- | --- | --- | --- | --- |
| Certified with Tungsten Carbide Ball Indenter |  |  |  |  |  |
| Part Number | Hardness Value | Scale | Min | Max | Quick Ship |
| [9220-060W](https://shop.buehler.com/23hr45t-superficial-rockwell-test-block-carbide) | 23 | HR45T | 18 | 28 |  |
| [9220-070W](https://shop.buehler.com/34hr45t-superficial-rockwell-test-block-carbide) | 34 | HR45T | 28 | 38 |  |
| [9220-080W](https://shop.buehler.com/43hr45t-superficial-rockwell-test-block-carbide) | 43 | HR45T | 37 | 47 |  |
| [9220-090W](https://shop.buehler.com/53hr45t-superficial-rockwell-test-block-carbide) | 53 | HR45T | 48 | 58 |  |
| [9220-100W](https://shop.buehler.com/67hr45t-superficial-rockwell-test-block-carbide) | 67 | HR45T | 57 | 77 |  |

| HR15Y Scale |  |  |  |  |  |
| --- | --- | --- | --- | --- | --- |
| Certified with Steel Ball Indenter |  |  |  |  |  |
| Part Number | Hardness Value | Scale | Min | Max | Quick Ship |
| [9228-020](https://shop.buehler.com/90hr15y-superficial-rockwell-test-block-steel) | 90 | HR15Y | 87 | 93 |  |
| [9228-060](https://shop.buehler.com/96hr15y-superficial-rockwell-test-block-steel) | 96 | HR15Y | 93 | 99 |  |

| HR15Y Scale |  |  |  |  |  |
| --- | --- | --- | --- | --- | --- |
| Certified with Tungsten Carbide Ball Indenter |  |  |  |  |  |
| Part Number | Hardness Value | Scale | Min | Max | Quick Ship |
| [9228-020W](https://shop.buehler.com/90hr15y-superficial-rockwell-test-block-carbide) | 90 | HR15Y | 87 | 93 |  |
| [9228-060W](https://shop.buehler.com/96hr15y-superficial-rockwell-test-block-carbide) | 96 | HR15Y | 93 | 99 |  |

| Special Order Test Blocks |  |  |
| --- | --- | --- |
| The Wilson Hardness Calibration Laboratory is capable of special orders outside the standard product offering. The following item numbers should be used for special orders including specific hardness values, hardness ranges, engraving or other compliances. Only available in the US and China |  |  |
| Part Number | Description | Quick Ship |
| 9201-002 | Special Hardness or Range Request |  |
| 9201-003 | NADCAP Engraved Grid |  |
| 9201-006 | API Compliant Test Block |  |

## Related Products

Wilson® Rockwell® 574

[![Wilson Rockwell R574 Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/10/R574.png)](https://www.buehler.com/ca/products/hardness-testing/rockwell-hardness-testers/wilson-rockwell-574/)

Wilson® Rockwell® RH2150

[![Wilson Rockwell RH2150 Hardness Tester](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/10/RH2150_Front.png)](https://www.buehler.com/ca/products/hardness-testing/rockwell-hardness-testers/wilson-rh2150-hardness-tester/)

### Downloads

\[wp_books_gallery category="Product Catalog"\]

\[wp_books_gallery category="Hardness Testing Catalog"\]

\[wp_books_gallery category="Test Block Application Guide"\]

\[wp_books_gallery category="Diamet Brochure"\]

\[wp_books_gallery category="Wilson Hardness Legacy Brochure"\]

\[wp_books_gallery category="Wilson Hardness Testing Catalog"\]

\[wp_books_gallery category="The Evolution of Hardness Testing"\]

\[wp_books_gallery category="50 Years of Quality: History of Hardness Testing"\]

\[wp_books_gallery category="Wilson Legacy Tester Program"\]

\[wp_books_gallery category="Proper Indent Spacing"\]

##### Quick Links

- [Quick Quote](https://www.buehler.com/buehler-request-a-quote.php)
- [Shop Now](https://shop.opti-tech.ca)
- [Quick Solutions](https://www.buehler.com/ca/solutions/buehler-solutions/methods-by-material/)
- [Contact Us](https://www.buehler.com/contact-us.php)
- [Safety Data Sheets](https://www.buehler.com/ca/solutions/buehler-literature/safety-data-sheets/)

[![Buehler Sustainable Resources](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/10/Buehler-Green-Logo-02-1024x346.png)](https://www.buehler.com/ca/solutions/buehler-solutions/sustainable-supplies/)