# PC Met® and PWB Met® Electronic Solutions

[![PC-Met Kit](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/10/605090_PC-Met-Ki.png)PC-Met Kit](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/10/605090_PC-Met-Ki.png)

[![PC-Met Coupon Pins](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/10/605053_PC-Met-Coupon-Pins-1000-pcs.png)PC-Met Coupon Pins](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/10/605053_PC-Met-Coupon-Pins-1000-pcs.png)

[![PWB Met Kit](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/10/605175_PWB-Met-Kit.png)PWB Met Kit](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/10/605175_PWB-Met-Kit.png)

[![PWB Met Pins](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/10/605084_PWB-Met-Pins.png)PWB Met Pins](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/10/605084_PWB-Met-Pins.png)

[![PWB Met Short Pin Loader](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/10/605186_PWB-Met-Short-Pin-Loader.png)PWB Met Short Pin Loader](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/10/605186_PWB-Met-Short-Pin-Loader.png)

## PCB-Met and PWB Met

### For Grinding and Polishing Machines

Beyond the conventional sample holder options, the PC Met and PWB Met cater specifically to the electronics sector as high-volume solutions. Compatible with the Automet 300 and EcoMet 30, these specialized systems empower users to grind and polish multiple samples automatically using central force mode. This proves exceptionally beneficial for batch processing, as the sample loading accessories of these systems ensure uniformity across all samples. With a focus on user-friendliness and ease of learning, our dedicated electronics solutions not only expedite processing but also enhance overall efficiency, allowing you to significantly reduce processing time.

#### PC-Met Precision Wiring Board Accessory

- High volume, printed wiring board preparation system for use with AutoMet 300 and a 12″” \[305mm\] platen
- Simultaneously prepare up to 36 coupons for significantly faster batch processing
- Prepares reproducible cross-sections of through-holes down to 0.008″ \[0.2mm\]

#### PWB-Met Small Hole Accessory

- Highest precision, printed wiring board preparation system for use with EcoMet 30 and AutoMet 300 and a 12″ \[305mm\] platen
- Simultaneously prepare up to 18 coupons
- Attain reproducible cross-sections of through-holes down to 0.004″ \[0.1mm\]

Each system is equipped with all necessary accessories to properly process your samples. For fast processing, we highly recommend our SamplKwick, among other acrylic solutions, for rapid curing. For those in need of a higher quaility cure and willing to accept a longer curing time, choose our epoxy solutions. For description and ordering information on these accessories and consumables, refer to the ordering table provided below.

Ordering

| PC-Met |  |
| --- | --- |
| Precision High Volume Printed Wiring Board Accessory |  |
| Part Number | Description |
| [60-5090](https://www.buehler.com/buehler-request-a-quote.php?pn=60-5090) | Indexing pins, carbide and diamond stops, pin loader, dial indicator, gauge blocks and wooden case |
| PC-Met Accessories |  |
| Part Number | Description |
| [60-5053](https://www.buehler.com/buehler-request-a-quote.php?pn=60-5053) | Coupon Pins 1.0625in \[27mm\] long (Qty 1000) |
| [60-5067](https://www.buehler.com/buehler-request-a-quote.php?pn=60-5067) | Cup, Extended Upper Mold Plate, 0.8in (Qty 6) |
| [60-9000](https://www.buehler.com/buehler-request-a-quote.php?pn=60-9000) | Central Force Drive Adapter for AutoMet® 250/300 |
| [60-5061](https://www.buehler.com/buehler-request-a-quote.php?pn=60-5061) | Upper cup |
| [60-5062](https://www.buehler.com/buehler-request-a-quote.php?pn=60-5062) | Lower cup |
| [60-5055](https://www.buehler.com/buehler-request-a-quote.php?pn=60-5055) | Dial Indicator |
| [60-5095](https://www.buehler.com/buehler-request-a-quote.php?pn=60-5095) | Holder with diamond and carbide |
| [60-5091](https://www.buehler.com/buehler-request-a-quote.php?pn=60-5091) | Carbide stops (Qty 3) |
| [60-5092](https://www.buehler.com/buehler-request-a-quote.php?pn=60-5092) | Diamond stops (Qty 3) |

| PWB-Met |  |
| --- | --- |
| Small Hole Accessory |  |
| Part Number | Description |
| [60-5175](https://www.buehler.com/buehler-request-a-quote.php?pn=60-5175) | Indexing pins, polycrystalline diamond stops, Pin loader, dial indicator calibration gauge, silicone mold release spray, gauge blocks, sample extractor and wooden case |
| PC-Met Accessories |  |
| Part Number | Description |
| [60-5186](https://www.buehler.com/buehler-request-a-quote.php?pn=60-5186) | PWB Met Short Pin Loader 0.375in \[10mm\] long |
| [60-5084](https://www.buehler.com/buehler-request-a-quote.php?pn=60-5084) | PWB Met Pins 0.375in \[10mm\] long (Qty 3000) |
| [60-5091](https://www.buehler.com/buehler-request-a-quote.php?pn=60-5091) | Long stop assembly |
| [60-5094](https://www.buehler.com/buehler-request-a-quote.php?pn=60-5094) | Short stop assembly with polycrystalline diamond |
| [60-5097](https://www.buehler.com/buehler-request-a-quote.php?pn=60-5097) | Holder with polycrystalline stops |

| Epoxy Mounting System |  |  |  |  |
| --- | --- | --- | --- | --- |
|  | Small Resin & Hardener | Large Resin & Hardener |  |  |
| Material | Resin | Hardener† | Resin | Hardener† |
| EpoKwick® FC mix ratio 4:1 by volume |  |  | [20-3453-128](https://shop.buehler.com/epokwick-fc-resin-128-oz-38l) 128oz \[3.8L\] | [20-3453-032](https://shop.buehler.com/epokwick-fc-hardener-32oz095l) 32oz \[0.95L\] |
| EpoThin® 2 mix ratio 2:1 by volume | [20-3440-032](https://shop.buehler.com/epothin-2-resin-32oz095l) 32oz \[0.95L\] | [20-3442-016](https://shop.buehler.com/epothin-2-hardener-16oz05l) 16oz \[0.48L\] | [20-3440-128](https://shop.buehler.com/epothin-2-resin-128oz38l) 128oz \[3.8L\] | [20-3442-064](https://shop.buehler.com/epothin-2-hardener-64oz19l) 64oz \[1.9L\] |
| EpoxiCure® 2 mix ratio 4:1 by volume | [20-3430-064](https://shop.buehler.com/epoxicure-2-resin-64oz19l) 64oz \[1.9L\] | [20-3432-016](https://shop.buehler.com/epoxicure-2-hardener-16oz05l) 16oz \[0.48L\] | [20-3430-128](https://shop.buehler.com/epoxicure-2-resin-128oz38l) 128oz \[3.8L\] | [20-3432-032\</a. 32oz \[0.95L\]](https://shop.buehler.com/epoxicure-2-hardener-32oz09l) |
| EpoHeat® CLR mix ratio 4:1 by volume | [20-3423-064](https://shop.buehler.com/epoheat-clr-resin-64oz-19l) 64oz \[1.9L\] | [20-3424-016](https://shop.buehler.com/epoheat-clr-hardener-16oz-048l) 16oz \[0.48L\] |  |  |
| † Restricted article, requires special packaging |  |  |  |  |

| Acrylic Mounting System |  |  |  |  |
| --- | --- | --- | --- | --- |
|  | Powder | Liquid† |  |  |
| Material | Part Number | Size | Part Number | Size |
| SamplKwick® | [20-3562](https://shop.buehler.com/sampl-kwick-powder-1-lb) [20-3566](https://shop.buehler.com/sampl-kwick-powder-5-lbs) [20-3562-025](https://shop.buehler.com/sampl-kwick-powder-25-lbs) [20-3562-100](https://shop.buehler.com/sampl-kwick-powder-100-lbs) | 1 lb \[0.45kg\] 5 lbs \[2.3kg\] 25 lbs \[11.3kg\] 100 lb \[45kg\] | [20-3564](https://shop.buehler.com/sampl-kwick-liquid-12-oz) [20-3568](https://shop.buehler.com/sampl-kwick-liquid-12-gal) [20-3564-320](https://shop.buehler.com/sampl-kwick-liquid-2-12-gal) [20-3564-640](https://shop.buehler.com/sampl-kwick-liquid-5-gal) | 12oz \[0.36L\] 64oz \[1.9L\] 2.5gal \[9.5L\] 5gal \[19L\] |
| VariKleer® | [20-3591](https://shop.buehler.com/varikleer-powder-22lbs-1-kg) 20-3591-002 20-3591-010 | 2.2 lbs \[1kg\] 4.4 lbs \[2kg\] 22 lbs \[10kg\] | [20-3592](https://shop.buehler.com/varikleer-liquid-169oz-500-ml) [20-3592-001](https://shop.buehler.com/varikleer-liquid-338oz-1l) 20-3592-005 | 16.9oz \[500mL\] 33.8oz \[1L\] 1.3gal \[5L\] |
| VariDur™ 10 | [11-1027](https://shop.buehler.com/varidur-10-powder-22lbs-1kg) [11-1031](https://shop.buehler.com/varidur-10-powder-22lbs-10kg) | 2.2 lbs \[1kg\] 22 lbs \[10kg\] | [11-1029](https://shop.buehler.com/varidur10200-liquid-169-oz-05l) [11-1033](https://shop.buehler.com/varidur10200-liquid-13gal-5l) | 16.9oz \[500mL\] 1.3gal \[5L\] |
| VariDur™ 200 | [11-1030](https://shop.buehler.com/varidur-200-powder-22lbs-1kg) [11-1034](https://shop.buehler.com/varidur-200-powder-22lbs-10kg) | 2.2 lbs \[1kg\] 22 lbs \[10kg\] | [11-1029](https://shop.buehler.com/varidur10200-liquid-169-oz-05l) [11-1033](https://shop.buehler.com/varidur10200-liquid-13gal-5l) | 16.9oz \[500mL\] 1.3gal \[5L\] |
| VariDur™ 3003 3-part system | [20-3531](https://shop.buehler.com/varidur-3003-powder-1500g) 20-3534 | 3.3 lbs \[1.5kg\] 16.5 lbs \[7.5kg\] | 20-3535 20-3536 [20-3532](https://shop.buehler.com/varidur-3003-500ml-liquid-1-1000ml-liquid-2) | .65gal \[2.5L\] Liquid 1 1.3gal \[5L\] Liquid 2 Liquid Kit Contains: 16.9oz \[500mL\] Liquid 1 33.8oz \[1L\] Liquid 2 |
| † Restricted article, requires special packaging |  |  |  |  |

##### Related Products

[![AutoMet 300 Pro Grinder Polisher](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/08/AutoMet-300-Pro_Front-600x600-1.png)](https://www.buehler.com/ca/products/grinding-and-polishing/grinder-polishers/automet-300-pro-grinder-polisher-touch-screen-programmable-pcb/)

[AutoMet® Pro 300](https://www.buehler.com/ca/products/grinding-and-polishing/grinder-polishers/automet-300-pro-grinder-polisher-touch-screen-programmable-pcb/)

8-12in \[203-305mm\]
Semi-Automatic Grinder-Polisher

[![AutoMet® 250 Pro Grinder-Polisher](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/10/AutoMet-250_Front_Black-600x600-1.png)](https://www.buehler.com/ca/products/grinding-and-polishing/grinder-polishers/automet-250-pro-grinder-polisher-touch-screen-programmable/)

[AutoMet® 250 Pro](https://www.buehler.com/ca/products/grinding-and-polishing/grinder-polishers/automet-250-pro-grinder-polisher-touch-screen-programmable/)

8-10in \[203-254mm\]
Semi-Automatic Grinder-Polisher

[![EcoMet® 30 Semi-Automatic Grinder Polisher](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/10/EcoMet-30-with-head-front_OL.jpg)](https://www.buehler.com/ca/products/grinding-and-polishing/grinder-polishers/ecomet-30-semi-automatic-grinder-polisher/)

[EcoMet® 30](https://www.buehler.com/ca/products/grinding-and-polishing/grinder-polishers/ecomet-30-semi-automatic-grinder-polisher/)

8-12in \[203-305mm\]
Semi-Automatic Grinder-Polisher

[![Specimen Holder Round](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/10/602482_1_SpecimenHolder6Round.png)](https://www.buehler.com/ca/products/grinding-and-polishing/accessories-and-consumables/specimen-holders/)

[Specimen Holder](https://www.buehler.com/ca/products/grinding-and-polishing/accessories-and-consumables/specimen-holders/)

For Grinding and Polishing Machines

###### Related Consumables

[![Acrylic Mounting System](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Acrylic-Mounting-System.png)](https://www.buehler.com/ca/products/mounting/accessories-consumables/acrylic-mounting-systems/)

[Acrylic Mounting System](https://www.buehler.com/ca/products/mounting/accessories-consumables/acrylic-mounting-systems/)

[![Epoxy Mounting Systems](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Epoxy-Mounting-Systems.png)](https://www.buehler.com/ca/products/mounting/accessories-consumables/epoxy-mounting-systems/)

[Epoxy Mounting Systems](https://www.buehler.com/ca/products/mounting/accessories-consumables/epoxy-mounting-systems/)

[![Silicone Carbide Papers](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/CarbiMet.png)](https://www.buehler.com/ca/products/grinding-and-polishing/accessories-and-consumables/silicon-carbide-grinding-papers/)

[Silicon Carbide Grinding Paper](https://www.buehler.com/ca/products/grinding-and-polishing/accessories-and-consumables/silicon-carbide-grinding-papers/)

[![MetaDi Diamond Suspension and Paste](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/MetaDi-Diamond-Suspension-and-Paste.png)](https://www.buehler.com/ca/products/grinding-and-polishing/accessories-and-consumables/diamond-suspensions-and-paste/)

[Diamond Suspensions and Paste](https://www.buehler.com/ca/products/grinding-and-polishing/accessories-and-consumables/diamond-suspensions-and-paste/)

Product Literature

[![Polishing Guide English](https://www.buehler.com/ca/wp-content/uploads/sites/3/2021/10/Polishing-Guide_English.jpg)](https://www.buehler.com/assets/Brochures/English/Consumables/FN01465_0216_Polishing_Application_Guide_WEB.pdf)

[Polishing Guide](https://www.buehler.com/assets/Brochures/English/Consumables/FN01465_0216_Polishing_Application_Guide_WEB.pdf)

[![Buehler Product Catalog](https://www.buehler.com/ca/wp-content/uploads/sites/3/2023/08/Buehler-Product-Catalog_default_600x782.jpg)](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

[Buehler Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

![Full Lab Metallography Solutions](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Dr-Mike-Keeble.jpg)

Find Your Solutions

###### Full Lab Metallography Solutions

Looking for more information from us? Browse through our Solutions section to view technical articles, find recommended processing methods, look at industry solutions, and more.

[Solutions by Industry](https://www.buehler.com/ca/solutions/buehler-solutions/solutions-by-industry/)

[Solutions by Material](https://www.buehler.com/ca/solutions/buehler-solutions/methods-by-material/)

Need Additional Help?

Do you want to improve your process? Reach out for one-on-one help from our applications experts.

![Contact Buehler Lab Team](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Lab-Icon.png)

Contact Lab Team

[Contact Lab](https://www.buehler.com/ca/contact-lab-canada.php)

![Contact Buehler Customer Care](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Contact-Buehler.png)

Contact Customer Care

[Contact Us](https://www.buehler.com/ca/contact-us-canada.php)

###### Quick Links

Quickly access important info or visit our [E-Shop](https://shop.opti-tech.com/). Buehler is represented in Canada by Opti-tech Scientific

![Buehler Product Catalog](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Literature-Icon.png)

Product Catalog

View all Products in the Buehler Product Catalog

[Product Catalog](https://en.calameo.com/buehler/read/00639329103cfc405df2c)

![Methods by Material](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/methods-by-material.png)

Methods by Material

Select a method by material

[Buehler Methods](https://www.buehler.com/ca/solutions/buehler-solutions/solutions-by-material/)

![Safety Data Sheets](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/SDS-Search.png)

SDS

Search Buehler's Safety Data Sheets

[Safety Data Sheets](https://www.buehler.com/ca/solutions/buehler-literature/safety-data-sheets/)

![Buehler Product Literature](https://www.buehler.com/ca/wp-content/uploads/sites/3/2024/02/Buehler-Literature-Icon.png)

Product Literature

Browse and search Buehler's product literature

[Product Literature](https://www.buehler.com/ca/solutions/buehler-literature/product-literature/)