The IsoMet® Low Speed Saw is a precision sectioning saw designed for cutting various types of materials with minimal deformation. Its low kerf loss capability and great versatility in holding all types of sample shapes and configurations, gives today's laboratory a precision sectioning tool capable of cutting viturally any mateiral including brittle or ductile metals, composites, cements, laminates, plastics, electronic devices and biomaterials.

  • Compact saw uses gravity feed system to provide constant feed rate
  • Produces minimum deformation
  • ±5μm or ±0.001in positioning via manual micrometer
  • 0.02 Hp motor

(includes 4in [102mm] IsoMet Blade for general sectioning, assorted weights, dressing stick, IsoCut Fluid, flanges and the following chucks: single saddle, irregular specimen and wafer).