Recommended Books
 

Currently In Print:
Metallography: Principles and Practice by George F. VanderVoort
1999 ASM International Materials Park, OH, 44073
(tel 1-800-262-4729)

Surface Preparation and Microscopy of Materials by Brian Bousfield
1992 John Wiley & Sons Ltd. Baffins Lane Chichester West Sussex PO19 1UD, England

Hardness Testing edited by Howard E. Boyer
1987 ASM International Materials Park, OH, 44073

ASM Handbook Volume 9: Metallography and Microstructures
1985 ASM International Materials Park, OH, 44073

ASM Handbook Volume 10: Materials Characterization
1985 ASM International Materials Park, OH, 44073

Light Microscopy of Carbon Steels (new and update edition of Optical Microscopy of Carbon Steels)
by Leonard E. Samuels 1998 ASM International Materials Park, OH, 44073

The Quantitative Description of Microstructure of Materials by Krzysztof Jan Kurzydlowski and
Brian Ralph 1995 CRC Press Inc. 2000 Corporate Blvd., N.W. Boca Raton, Florida, 33431

Quantitative Image Analysis of Microstructures edited by Habns Eckart Exner and Hans Paul Hougardy 1998 DGM Metallurgy Information Adenauerallee 21, D-6370 Oberursel 1 Germany

Video Microscopy: The Fundamentals (second edition) by Shinya Inoue and Kenneth Spring,
1997 Plenum Publishing Corp., 233 Spring Street, NY, NY 10013

Metallographic Atlas of Powder Metallurgy by W.J. Huppman and K. Dalal
1996 Verlag Schmid, order from Powder Metallurgy Publications c/o Metal Powder Industries
Federation 105 College Road East, Princeton, NJ 18540

Polymer Microscopy by Linda C. Sawyer and David T. Grubb
1987 Chapman and Hall Ltd 11 New Fetter Lane, London EC4P 4EE

Understanding How Components Fail by Donal J. Wulpi
1985 ASM International Materials Park, OH, 44073

Metallurgical Failure Analysis by C. Brooks and A. Choudhury
1993 McGraw Hill Co. 1221 Avenue of Americas, NY, NY 10020 (tel 1-800-262-4729)

ASM Handbook Volume 11: Failure Analysis and Prevention
1986 ASM International Materials Park, OH, 44073

ASM Handbook Volume 12: Fractography
1987 ASM International Materials Park, OH, 44073

Ceramography by R.E. Chinn
Published by ASM International and the American Ceramic Society, 2002

Currently Out of Print:
Metallographic Polishing by Mechanical Methods by Leonard E. Samuels
1982 America Society for Metals (ASM International) Metals (Materials) Park, OH, 44073

A History of Metallography by Cyril Stanley Smith
1960 The University of Chicago Press, Chicago, IL